    I'm about to weld about a 100+ 3/8" SS rods to 1/4" SS plates as shown in the attached image.



    How would you go about it?

    1. What would be the best equipment to use?
    2. What's the best weld type for this application?
    3. Any general advice would be really appreciated. I'm going to be welding so many of these that I wan't to make sure I'm doing it right.

    Thanks, Danny

  2. #2
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,159
    Post Thanks / Like

    Re: How would you weld this?

    All stainless? I'd be tempted to drill the plates, insert the rods and tig them in from behind rather than the way they did them in that pict.


    Small round stock like shown in the picts is a PITA to weld either with mig or tig. It's tough to get the gun or torch around fast enough with something that small. If you weld from the back, then you have a flat surface and can simply weld then in no problem.
    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  3. #3
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,131
    Post Thanks / Like

    Re: How would you weld this?

    What are they used for? What kind of pressures/weight/forces are put on them? What machines do you have access to?

  4. #4
    Join Date
    Jan 2013
    Posts
    6
    Post Thanks / Like

    Re: How would you weld this?

    I'm going to use them as table legs. They'll need to withstand about 500lbs of weight.

    I'm going to buy new equipment for this job, any recommendations would be helpful.

  5. #5
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: How would you weld this?

    stainless stick

  6. #6
    Join Date
    Jan 2006
    Location
    In A Nice Comfy Chair
    Posts
    18,773
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by bittiker View Post
    I'm going to buy new equipment for this job, any recommendations would be helpful.
    I would tig it..be done in no time..


    I don't like this one bit...
    Do you have any idea what you just ate?

    Here we go.

    ...zap!


    I am not completely insane..
    Some parts are missing

    Professional Driver on a closed course....
    Do not attempt.

    Just because I'm a dumbass don't mean that you can be too.
    So DON'T try any of this **** l do at home.

  7. #7
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,569
    Post Thanks / Like

    Re: How would you weld this?

    I would tig them. I did 750 of these, 100 won't take long. Sorry the pics are all sideways
    Attached Images Attached Images    
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller Maxstar 161STH
    Miller AEAD200LE
    Hobart MIG
    Lincoln Idealarc 250

  8. #8
    Join Date
    Jan 2013
    Posts
    6
    Post Thanks / Like

    Re: How would you weld this?

    I'm an amateur welder at best. I'm trying to go with the most fool-proof method. If I drilled a hole, and welded from the back, would I drill a slightly bigger hole? Or use the same dia. drill bit?

    Also, if I were to weld from the back, could I use this MIG welder? Or would I need something more heavy duty?

    http://www.amazon.com/Pro-Series-MMI...1&keywords=kit

  9. #9
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,159
    Post Thanks / Like

    Re: How would you weld this?

    I'd go with the same size hole myself.

    That welder isn't really the right tool for stainless if you want it to stay stainless. For that you will want a mig that uses gas vs a small flux core welder. Understand to mig stainless it will not be cheap. Stainless mig usually uses a trimix gas specifically for stainless. My supplier doesn't usually stock small cylinders of this gas, but can order then is as needed. It is not cheap.
    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  10. #10
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,347
    Post Thanks / Like

    Re: How would you weld this?

    Ditto DSW, I'd punch them out on the ironworker and tig from the back. Update your user cp with your location and you might find somebody willing to help you out.
    100 of them isn't a lot, maybe a days work.

  11. #11
    Join Date
    Mar 2010
    Posts
    360
    Post Thanks / Like

    Re: How would you weld this?

    You'd do way better with the punch and weld from the back method. The welding from the back method is just a flat weld, and you'll be able to do 5 of them in the time it would take to do 1 of the flllet weld around a very small rod method shown in the pics, plus if you're not experienced in doing the small circumference of the fillet weld method, you'll have a substantial learning curve before you get to production....

    SquirmyPig, what is that thing used for?

  12. #12
    Join Date
    Mar 2009
    Location
    MN
    Posts
    5,265
    Post Thanks / Like

    Re: How would you weld this?

    Are they for a restaurant or something? All on one table? Or 25 tables? For your use? Or did you accept a job you weren't ready for?
    My name's not Jim....

  13. #13
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,898
    Post Thanks / Like

    Re: How would you weld this?

    Mr. Moose, Duh, It's a dime holder.

    Bittiker

    Learn to weld first, Seems like a serious project 500 lbs capacity. Not a lot a weld to hide your lack of ability. Might want to pay somebody to do it.

    Good luck

  14. #14
    Join Date
    Jan 2006
    Posts
    1,894
    Post Thanks / Like

    Re: How would you weld this?

    drilling stainless is a chore if you have never done that before. I would second the punch, but many shops will charge more for punching stainless than for punching mild steel. Lastly, I am not sure he knows how to tig. Stick welding from the back would be cheaper in the long run due to needing just a cracker box. if he already had a cracker box and wanted to add a tig stinger to it then he is looking at another 200-300 dollars. on the cheap.

  15. #15
    Join Date
    Jan 2006
    Posts
    1,894
    Post Thanks / Like

    Re: How would you weld this?



    That looks like the same high dollar gig set I use from time to time.

  16. #16
    Join Date
    Jul 2011
    Location
    Australia
    Posts
    41
    Post Thanks / Like

    Re: How would you weld this?

    Here's another vote for punching the holes and welding from the back.
    • Don't attempt to drill the holes yourself, you'll regret it - just outsource.
    • Make sure you have a jig set up so that everything slots into place nicely at the required angles/heights.
    • Have it so that the rod is recessed slightly from the back of the plate, so the weld bead doesn't protrude above the face of the plate (assuming you want to keep it flat).
    • I'd reach straight for a tig machine - you'll get a quick neat weld with no cleanup required.
    • When you get the holes punched, they'll probably come back with oil and crap on them, so you'd be best advised to dunk them all in a cleaning solution and a wipe down with acetone before welding.

  17. #17
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,569
    Post Thanks / Like

    Re: How would you weld this?

    Mr.Moose, the name is SquirmyPug and the part is an adjustment handle for a tool called a Knucklemate..something I don't think anyone here has used .

    Scott Young..it is high dollar it has made us alot of $$
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller Maxstar 161STH
    Miller AEAD200LE
    Hobart MIG
    Lincoln Idealarc 250

  18. #18
    Join Date
    Mar 2010
    Location
    Morton, Washington
    Posts
    5,136
    Post Thanks / Like

    Re: How would you weld this?

    Can you buy them for less than making them?
    http://hairpinlegs.com/products.php?id=1

    If you decided to have the holes punched or drilled remember that the legs are cambered a few degrees. I'd lay out my fixture and then experiment with the hole size as you likely need to oversize a little. In an ideal world you'd drill the holes at the appropriate angles for the camber but angled holes cost more than flat drilled or punched.

    Do the exposed welds have an aesthetics value?

  19. #19
    Join Date
    Oct 2010
    Location
    The Netherlands
    Posts
    441
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by TimmyTIG View Post
    stainless stick


    Stick would be the fastest and way cheaper then any other process.

    SS stick can be as nice as tig , you have 100 tries

    You have about 6-8 hours hard work (including cleaning) \I would finish faster, go home drink some beer

    Happy new year guys !!!
    --------------------------------------------------------------
    www.becmotors.nl
    yup, I quit welding.. joined welder anonymous

  20. #20
    Join Date
    Nov 2007
    Location
    Kittanning, Pa
    Posts
    41
    Post Thanks / Like

    Re: How would you weld this?

    knucklemate,,, appears to be for loco/ car knuckles.. hmm, learn something new every day .
    L-Tec PCM-VPi II
    Hobart Handler140
    Millermatic 35
    Lincoln Power arc 4000
    Lincoln Ranger 10,000 ( 3 )
    Longevity Tigweld 160SX
    Purox O/A setup
    100lb anvil
    XLO/servosource cnc mill

  21. #21
    Join Date
    Oct 2009
    Posts
    28
    Post Thanks / Like

    Re: How would you weld this?

    drill the hole

    insert the rod half way throught he plate, leave it about 1/8" from flush on the back side, and weld it up with the mig.

    it the wel is beyond flush grinder down!

  22. #22
    Join Date
    Nov 2005
    Posts
    353
    Post Thanks / Like

    Re: How would you weld this?

    Those plates in the sample don't look 1/4 to me, if the rods are 3/8
    Experience is something you get right after you need it

  23. #23
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: How would you weld this?

    you're building a 500 pound table with those little rods for legs?

  24. #24
    Join Date
    Aug 2010
    Location
    NE Ocean County, NJ
    Posts
    178
    Post Thanks / Like

    Re: How would you weld this?

    I apologize if I'm wrong, but is this spam?

    The OP wants to weld up something to withstand 500lb, stresses, seems to have no idea of the equipment or processes or difficulty involved and asks if a 110V flux core machine is up to the task.

    I'm just wondering ......

    If not: I like the punching or option and weld from the back, but would it be reasonable with limited equipment options I am assuming the OP has available to tig the fillet and stop a couple times to turn the piece, since it is difficult to manipulate around the small diameter without a turntable positioner? How about some simple positioner kinda like the old sit n spin kids toy you could spin with your foot?
    Last edited by jtcnj; 01-02-2013 at 09:03 PM.
    Lincoln AC/DC 225/125 and WP17. 75A AC is for pipe thawing!
    HH 140 - new addtion 9/2012.

    I didn't agree, but hoped for Hope and Change.
    I got change for myself and my family: for the worse.
    This is the reality of: Barackalypse Now. Again.

  25. #25
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,569
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by jtcnj View Post
    I apologize if I'm wrong, but is this spam?

    The OP wants to weld up something to withstand 500lb, stresses, seems to have no idea of the equipment or processes or difficulty involved and asks if a 110V flux core machine is up to the task.

    I'm just wondering ......
    I didn't notice that he said they are table legs, but I see now. Maybe it is spam..Don't know
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller Maxstar 161STH
    Miller AEAD200LE
    Hobart MIG
    Lincoln Idealarc 250

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,289,947.65878 seconds with 19 queries