    each leg is two 3/8 rods that form a v and there are 4 legs thus 8 rods. each leg holds up to 125 lbs under compression so I don't see where that is too much weight.

    Just my understanding. I don't see it as spam. I see spam as the likes of sellers or people trying to move traffic to other websites for monetary gain.

  2. #27
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by Scott Young View Post
    each leg is two 3/8 rods that form a v and there are 4 legs thus 8 rods. each leg holds up to 125 lbs under compression so I don't see where that is too much weight.

    Just my understanding. I don't see it as spam. I see spam as the likes of sellers or people trying to move traffic to other websites for monetary gain.
    You are right on the spam..But I'm still not sure.
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

  3. #28
    Join Date
    Jan 2006
    Location
    In A Nice Comfy Chair
    Posts
    18,773
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by Scott Young View Post
    Just my understanding. I don't see it as spam. I see spam as the likes of sellers or people trying to move traffic to other websites for monetary gain.
    That's correct..
    I don't see it as spam either..

    What I DO see is someone either in over their head..
    Or a TROLL.

    Lets see.. 3 posts and no response...
    It's a "Pick'em"...

    ...zap!


    I am not completely insane..
    Some parts are missing

    Professional Driver on a closed course....
    Do not attempt.

    Just because I'm a dumbass don't mean that you can be too.
    So DON'T try any of this **** l do at home.

  4. #29
    Join Date
    Jan 2013
    Posts
    6
    Post Thanks / Like

    Re: How would you weld this?

    Not spam, just an overly optimistic woodworker.

    I got some reasonable quotes from a local san francisco shop, and decided for now I'm just going to purchase the legs. I figured if I only had one type of weld to learn, I could figure it out on my own... but I realized welding is a world of its own. I'll learn eventually.

    Thanks for all your help!

    Here are the tables I'm hoping to build:

    www.stemfurniture.com

  5. #30
    Join Date
    Mar 2010
    Location
    Morton, Washington
    Posts
    5,108
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by bittiker View Post
    just an overly optimistic woodworker.
    Cool... and welcome.

    Stainless is a tough starting point as it's harder to bend, cut, and drill. Add to that the material cost make mistakes painful. I wouldn't let our exercise in reality discourage you from adding some metal fab to your craft.

    Before heading off to buy some equipment I'd recommend taking some basic classes to get your feet wet and gain some skills to get you where you'd like to be. I'd use your project for the class and glean all you can. There are several ways to complete this job... it all comes down to your skills and equipment. You may find your new passion... or you may decide you hate welding and your happier subbing it out.

    I grew up in a wood shop... but was introduced to metal shop in junior high. I think my Dad's ok with it.

  6. #31
    Join Date
    Apr 2007
    Location
    Poco British Columbia
    Posts
    264
    Post Thanks / Like

    Re: How would you weld this?

    I think he might weld photobooths for a hobby.

  7. #32
    Join Date
    Dec 2010
    Location
    Olathe Kansas
    Posts
    665
    Post Thanks / Like

    Re: How would you weld this?

    Id use a welder.
    I forgot how to change this.

  8. #33
    Join Date
    Jan 2013
    Posts
    6
    Post Thanks / Like

    Re: How would you weld this?

    Thanks everyone for your help! I finished 13 tables with this method, check them out here:

    http://www.stemfurniture.com

    -Danny

  9. #34
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: How would you weld this?

    The tables look nice Bittiker.
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

  10. #35
    Join Date
    Apr 2012
    Posts
    222
    Post Thanks / Like

    Re: How would you weld this?

    I would agree they look good.
    Welding is a world of it own. That does not mean you cannot learn though.
    Either taking a class and staying on here, or even just buying a welder and start playing around with some stuff.

  11. #36
    Join Date
    Jul 2011
    Location
    Melbourne, Australia.
    Posts
    863
    Post Thanks / Like

    Re: How would you weld this?

    A wood worker cum welder.....now I've heard it all.

    It is little wonder the USA has lost most of it's ability to produce trade goods against the Chinese "back yarders"......I weep.

    In this situation the wood worker is taking the bread out of the mouth of a person who relies on welding for a living and can guarantee his work.

    If the table leg fails at the weld and the customer ends up with hot soup amongst the family jewels.....expect some expensive court time due to also attempting to be a lawyer.....LOL.
    Ian.

  12. #37
    Join Date
    Jan 2010
    Location
    Northwest Missouri
    Posts
    1,180
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by bittiker View Post
    Thanks everyone for your help! I finished 13 tables with this method, check them out here:

    http://www.stemfurniture.com

    -Danny
    HOLY FIREWOOD, BATMAN!

    I burned a couple of chords of walnut this past winter, cause around here stuff like that is scrap wood. Unless a log is long and straight (veneer tree) nobody wants to buy it anymore.

    Nice looking tables there Danny!

    Did I mention I do my best wood working with Stihl equipment?
    Roger
    Old, Tired, and GRUMPY

    Salesman will call, Batteries not included, Assembly is required, and FREE ADVICE IS WORTH EXACTLY WHAT YOU PAY FOR IT!

    Dial Arc 250HF
    Thunderbolt 225 AC/DC

    Assorted A/O torches

  13. #38
    Join Date
    Feb 2008
    Location
    Indiana
    Posts
    1,469
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by puddytat View Post
    A wood worker cum welder.....now I've heard it all.

    It is little wonder the USA has lost most of it's ability to produce trade goods against the Chinese "back yarders"......I weep.

    In this situation the wood worker is taking the bread out of the mouth of a person who relies on welding for a living and can guarantee his work.

    If the table leg fails at the weld and the customer ends up with hot soup amongst the family jewels.....expect some expensive court time due to also attempting to be a lawyer.....LOL.
    Ian.
    What???
    Tim Beeker.

  14. #39
    Join Date
    Nov 2012
    Posts
    121
    Post Thanks / Like

    Re: How would you weld this?

    $2199 for a table

  15. #40
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by puddytat View Post
    A wood worker cum welder.....now I've heard it all.

    It is little wonder the USA has lost most of it's ability to produce trade goods against the Chinese "back yarders"......I weep.

    In this situation the wood worker is taking the bread out of the mouth of a person who relies on welding for a living and can guarantee his work.

    If the table leg fails at the weld and the customer ends up with hot soup amongst the family jewels.....expect some expensive court time due to also attempting to be a lawyer.....LOL.
    Ian.
    Not sure what you are saying here...
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

  16. #41
    Join Date
    Mar 2010
    Posts
    360
    Post Thanks / Like

    Re: How would you weld this?

    bittiker, I like your tables and the fact that you are using material that would otherwise be discarded to make functional and good looking things. If you are in an area where you can sell your products for enough to make a business out of it, all the better.

    Most of us have a personality trait that causes us to enjoy making things, and learning new skills. You came and asked a reasonable question. You got some good advice on that question, and if you find that welding is a skill that would take you further down the road to where you want to go, I'm sure you'll do well with some practice and focus. Good luck!

  17. #42
    Join Date
    Oct 2010
    Location
    The Netherlands
    Posts
    441
    Post Thanks / Like

    Re: How would you weld this?

    I'd like to see the welds on that 2k $ table
    --------------------------------------------------------------
    www.becmotors.nl
    yup, I quit welding.. joined welder anonymous

  18. #43
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,032
    Post Thanks / Like

    Re: How would you weld this?

    In my area every single person that would want a table like that would make their own. Pretty tough to do something that makes money around here. You have to be good at something that is very hard to do around these parts and then still no one has money. lol

  19. #44
    Join Date
    Feb 2009
    Location
    Calg, AB
    Posts
    719
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by SquirmyPug View Post
    Not sure what you are saying here...
    Quote Originally Posted by puddytat View Post
    A wood worker cum welder.....now I've heard it all.

    It is little wonder the USA has lost most of it's ability to produce trade goods against the Chinese "back yarders"......I weep.

    In this situation the wood worker is taking the bread out of the mouth of a person who relies on welding for a living and can guarantee his work.

    If the table leg fails at the weld and the customer ends up with hot soup amongst the family jewels.....expect some expensive court time due to also attempting to be a lawyer.....LOL.
    Ian.
    Quote Originally Posted by tnjind View Post
    What???



    Was thinking the exact same thing... What an 'Odd' comment.
    Miller Diversion 165
    120 amp Buzz Box
    Victor Oxy/Ace Oxy/LPG
    Smith "Little" Oxy/LPG
    Hypertherm Powermax 30
    Lot's of Misc. tools n' crap....

  20. #45
    Join Date
    Feb 2009
    Location
    Calg, AB
    Posts
    719
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by SquirmyPug View Post
    You are right on the spam..But I'm still not sure.
    Quote Originally Posted by zapster View Post
    That's correct..
    I don't see it as spam either..

    What I DO see is someone either in over their head..
    Or a TROLL.

    Lets see.. 3 posts and no response...
    It's a "Pick'em"...

    ...zap!

    OMFG... seriously? Paranoid or Impatient much? It had only been 26 hours since the OP's initial post! Now 'Moderators' are implying that people might be 'TROLLS' because they don't answer fast enough? Christ, It's a wonder people come here for at all....
    Miller Diversion 165
    120 amp Buzz Box
    Victor Oxy/Ace Oxy/LPG
    Smith "Little" Oxy/LPG
    Hypertherm Powermax 30
    Lot's of Misc. tools n' crap....

  21. #46
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,679
    Post Thanks / Like

    Re: How would you weld this?

    He is based in Los Gatos.... Probably has a hard time keeping them in stock.

  22. #47
    Join Date
    Jan 2013
    Posts
    6
    Post Thanks / Like

    Re: How would you weld this?

    It's crazy on these threads how a simple welding question can get such intense reactions out of people. Thanks everyone for your input, I've got my hands full marketing now, but I'll have more questions once I get back in the shop - Danny
    Last edited by bittiker; 04-23-2013 at 02:57 PM.

  23. #48
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,032
    Post Thanks / Like

    Re: How would you weld this?

    Good stuff! If you have buyers all power to you! They do look nice!

  24. #49
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: How would you weld this?

    Quote Originally Posted by jman View Post
    OMFG... seriously? Paranoid or Impatient much? It had only been 26 hours since the OP's initial post! Now 'Moderators' are implying that people might be 'TROLLS' because they don't answer fast enough? Christ, It's a wonder people come here for at all....
    Jman, when this thread was started and the OP was asking questions some things just didn't seem "right" to me. He even said he was an amateur, asking about what kind of welder to use and things like that. Often when people on here "ask" questions they don't even pay attention to the replys and do whatever it is they wanted to do anyway. (asking about welding on a trailer..Everyone says don't do it..They do it anyway)
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,356,373.78799 seconds with 13 queries