    Maybe a solution . I wrapped some of this fiber tape around the thumb where I had a hole sure felt a lot better.. The link is just to show what I used I got it a the local electrical supply .
    https://www.platt.com/platt-electric...spx?zpid=64133

  2. #2
    Join Date
    Aug 2012
    Location
    AR
    Posts
    2,327
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    Jody on weldingtipsandtricks has some TIG fingers, fiberglass weave material it looks like. Might take a look at those and see if it's what you need.

    http://www.weldingtipsandtricks.com/store.html
    Last edited by shortfuse; 04-25-2013 at 10:53 PM.

  3. #3
    Join Date
    Nov 2009
    Location
    Hellinois
    Posts
    5,893
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    Quote Originally Posted by shortfuse View Post
    Jody on weldingtipsandtricks has some TIG fingers, fiberglass weave material it looks like. Might take a look at those and see if it's what you need.

    http://www.weldingtipsandtricks.com/store.html
    I bought one of those, but haven't used it yet. Unfortunately, when I showed it to my pipe fitter buddy, he laughed and said, "tell me you are not going to put a f'n condom on your finger when you tig weld"!!!
    "Where's Stick man????????" - 7A749
    "SHHHHHH!! I sent him over to snag that MIC-4 while tbone wasn't looking!" - duaneb55
    "I have bought a few of Tbone's things unlike Stick-Man who helps himself" - TozziWelding
    "Stick-man"

  4. #4
    Join Date
    Feb 2013
    Posts
    72
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    I'm not a welder just weld a little here at the house on pipe fence or tractors or implements. So I just tear that left glove up grabbing rough hot material just thought about that tape just to keep in a pinch . I understand they sell only the left glove when I get a new one I believe I'll wrap the thumb and index to start with to save on the glove .

  5. #5
    Join Date
    Apr 2012
    Location
    On a farm, north of Scranton, PA
    Posts
    313
    Post Thanks / Like
    I have a few of those welding finger condoms. I find that 90% of the time, finding a comfortable place to steady is difficult. Sliding along the material with the finger condom is really nice, until they fail. And they can.

    I was moving right along on a bunch of 3/16" aluminum when OH FCK THAT'S HOT the tig finger melted a hole.

    Name:  ImageUploadedByTapatalk 21366996687.000976.jpg
Views: 318
Size:  33.0 KB

    So be careful. They work great until the don't.
    Lincoln Precision Tig 185
    Lincoln Power Mig 256
    Hypertherm PM 45
    Everlast 140ST
    Smith O/A

  6. #6
    Join Date
    Jun 2010
    Location
    Niagara on the lake Canada
    Posts
    1,401
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    So... I dont tig but it occurs to me that you might not want to put your finger on hot steel. so why not make a metal tip ie wire that go onto your finger over your glove and IT runs down the hot metal. Provideing a small insulation layer of distance perhaps 1/2 inch. Just a thought.
    Miller thunderbolt 250
    Decastar 135E
    Recovering tool-o-holic
    ESAB OA
    I have been interested or involved in Electrical, Fire Alarm, Auto, Marine, Welding, Electronics ETC to name a just a few. So YES you can own too many tools.

  7. #7
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    Quote Originally Posted by dumb as a stump View Post
    So... I dont tig but it occurs to me that you might not want to put your finger on hot steel. so why not make a metal tip ie wire that go onto your finger over your glove and IT runs down the hot metal. Provideing a small insulation layer of distance perhaps 1/2 inch. Just a thought.
    Thats a good idea, but the heat radiating off the metal will still cook your fingers. Even with a tig finger sometimes my other fingers will get so hot I've got to stop welding.
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

  8. #8
    Join Date
    Apr 2013
    Location
    Socal/NE Oregon
    Posts
    416
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    Funny.........I seem to kill my right glove all the time. But then I'm a lefty.
    HF 180 amp/240 volt Mig (cap mod)
    1987 Harley FLHTP (project)
    1990 F350 XLT Lariat S/C dually
    1990 S&S 11SC Cabover Camper
    2011 Ford Ranger S/C XLT

  9. #9
    Join Date
    May 2010
    Location
    Andover, MN
    Posts
    327
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    Unless I miss my guess, the TIG fingers are made out of a ceramic fiber. Most likely from by 3M.

  10. #10
    Join Date
    May 2012
    Location
    Australia
    Posts
    249
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    I only buy left handed welding gloves, and use a lighter riggers glove on the right hand, pity I can't buy only right handed riggers gloves.

    Cheers Andrew

  11. #11
    Join Date
    Jul 2012
    Posts
    156
    Post Thanks / Like

    Re: Left welding glove tearing up before the right

    my first thought is you should switch hands every now and then.. but other than that, listen to the professionals. LOL

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,185,898.01909 seconds with 12 queries