    q240z, this 'weld' has problems.

    to much wire feed rate for the amount of weld power (voltage in this case) shown by the overly bulged and not fused toe and top of weld.

    @ 5:00 to 6:00 there is one stretch of 'acceptable' -not decent or good, but acceptable weld that is the toe and top are showing fusion of the puddle to the parent metal (there could be some undercutting?) not clear- but the puddle to puddle definition shows continuity of fusion.

    There is another stretch from 3:20 to nearly 4:00 where a few puddles are correctly formed, although apparently by accident not intent, where the only correctly formed weld is placed. However, even this set of four or five semi-acceptable puddles are marred by cold start and crater cracked ends with some porosity to boot.

    Almost all the rest of the weld shows puddle to puddle (the weld was 'buttered' poorly) cold fusion or 'cold lapping'. Almost all the starts and stops are cold lapped and not done correctly by the 'welder' (not even Jr. High shop student skill level).

    The voids are not really porosity they are actually places where the clean up /contamination of the parent metal gassed off so long the molten edge of the parent metal actually was prevented from flowing into the filler. Porosity is likely to be present if this weld were cut off the surface skin, not sanded or ground, but cut; there will be uniform Swiss cheese like consistency due the lack of joint fit, joint prep, joint design, clean up and welding technique which is totally unsuited for job.

    Now a 30A is the worst torch to try to weld this as the wt is high and therefore the agility of the torch is lowered, but this weld should been done with TIG. However if a MIG torch was the only choice it should have been done with full back up bars, and allowing a single pass down into teh parent metal to fully fuse to the consumable back up. Instead the weld is 'buttered' onto the filler and deck and built up cold with little fusion.

    This weld is an example of a poor welder because a good welder will decline to weld if he cannot do a good job. If you can't do good work: don't do any work. I know we all need to learn but that should be done on the bench not someone's boat.

    a more reliable weld to discuss below.



    some things to look for in this uncleaned MIG weld. There is a boundary of clean zone at the toe and top of weld, that shows the argon was cleaning the entire weld zone -no gas flow problems. 5356 Wire soots as the magnesium alloy component vaporizes outside the argon envelope. The top and toe of the weld 'flow into' the parent metal, they don't ball up- and the flow lines disappear into the parent metal without a big ridge or undercut. So this weld was balanced in terms of weld wattage- to melt the wire at this rate combine with the rate that arc melted wire filler was added to the melted parent in the molten metal. The weld you show above was not adjusted correctly.

    Also the puddle to puddle ridges are present but only ridges not overlapping 'scales' of cold lapped metal, so the puddle movement of the arc/wire filler happened while the puddle was molten; not cold lapping.

    The start was done on a small 'run on strip' to take up the cold part of the beginning more or less an aluminum MIG technique. And the stop was 'doubled back' on itself so the crater (normal to aluminum MIG stops) is only on top of a previous weld puddle already frozen and that is mostly cut out with carbide cutters to leave room to initiate the next or 'tie-in' weld.



    This weld is just a bit 'too cold' that is; the voltage is slightly too low. Why? first the ridges aren't flowing into one another- they're just a bit too pronounced- indicating a small amount of edge cold lapping. In other words with this weld setting movement of the gas cup/wire arc is moving over semi-chilled metal not just providing a movement within the molten puddle.

    Second; the toe and top fusion is just curling back not much- but enough to indicate that we should either; slow the wire; or crank the voltage; or pull up the cup a fraction, all of which will add the adjustment to get a more fused weld. The bottom edge is much better at this than the top so it may have been a matter of torch angle into the joint, where more arc should have been aimed to the upper leg?



    This is the best way to do hull and deck patch repairs. The back up material would be fully consumed in a weld were the root face would be fused into the bottom or back up material. I realize that not all repairs get this level of attention but it is the right way to do the work.

    The edges would be cleaned back inches inside and out, any old weld cut cleanly out back into parent material not just ground off or sanded smooth and the repair weld would go ahead on 'new' parent material not like the weld shown where likely some of the old weld porosity bubbled into the new 'weld'. This works well for 3/16" and thinner repairs but should have top edges beveled back for any materiel thicker than that.

    Not sure if you wanted this blunt a statement about that weld (?) but if you've gone to the effort to do the nicely done sheer clamp in pretty pieces of dead tropical plants; it seems a shame to allow the other trades to be at lower standards?

    cheers,
    Kevin Morin
    Kenai, AK

  2. #27
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Thanks, Kevin. I appreciate your informative and blunt reply. I've been concerned for a while that the main reason my repower is nine months behind schedule is because this fellow just doesn't have the experience his mouth thinks he's got. I have a day job and don't have time to become as proficient with certain technical skills as I think are necessary. It's one thing to fire up the Millermatic 35 and do sheetmetal work on an old car, and quite another to weld aluminum in mission critical spots. That's why I call in the pros when things need to get done and done right.

    I think I'm at the point of telling this fellow he's off the job.

    Know any aluminum welders in Maryland? My Trailblazer runs fine, and it will power a TIG if the Spoolmatic's the wrong tool for the job. I have no problem saying I don't have the skills to do it.

    It's always something...

    Thx
    Q

  3. #28
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,156
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Yikes.....fired and money refunded for that job.

    Wow.

    Dave J.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  4. #29
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Dave, the last job he did ended with him complaining about the Miller equipment being junk and pointing to one part of the job he'd done (that looked kind of like the 5-6 o'clock area in the pic I just posted) and calling it a "stack of dimes" weld.

    I'd never welded aluminum before but have had a Millermatic 35 for a few decades. I'll tell you what, my aluminum welds after an hour of practice with the same TB280 and Spoolmatic looked far better than his "stack of dimes." I didn't say it at the time, but I felt like telling him dimes don't look like that where I'm from... but used toilet paper does.

    I'm getting tired of firing highly paid American craftsmen for junk work. gad

    Q

  5. #30
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,156
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    You have expensive, critical welds to make - consider giving them a couple of test pieces to weld.

    Many welders have to test on the job - you being the employer is no different in my opinion.

    One job I asked for scrap of the aluminum they wanted welded and gave them sample welds the next day for inspection.

    If I'm willing to offer to make sample welds to get a job, you should feel comfortable requiring them on your equipment with your material.

    Dave J.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  6. #31
    Join Date
    Apr 2010
    Location
    Kenai, Alaska
    Posts
    772
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    q240z, glad I wasn't considered rude, and glad you're considering another welder.

    I'd say we need a touch of perspective here, we have on here (just one of many sites) lots of welders of extraordinary skill whose knowledge allows good work for their clients.

    I'd say perhaps you may want to tighten up your contractor hiring procedures just a bit? First, if the welder doesn't have their own equipment then that alone should say something about their qualifications to join your project? It does to me, that welder is not committed enough to the trade to provide his own machine- fine with me; but I'm not hiring someone with that attitude/practice/policy/work ethic to come work on my boat!

    Next, a work sample/weld test/break bend test run with your own equipment, if that is the only tool for this particular job, is not out of line. So if they can't weld up, down, left, right, butt, outside fillet, inside fillet: why would you consider them an "American craftsman"?

    Let's call them what that group is, wanna-bee's who can't weld- yet. (hopefully) They may develop into fine craftsman but if you can't have an onsite demo - you're being too generous with your terminology and not stringent enough with your hiring standards.

    This guy must not be sought after enough to have fulltime MIG gig for a local aluminum shop? Otherwise why is he lose to work for you?

    If they can't make a decent bend break test in plate, you sure as shootin' don't want them on your boat! I don't care for the 30A, I prefer the push pull MK guns- but I can weld with the Miller "club"- if required. (perhaps being threatened with a beating using that particular MIG gun would induce me to pick one up... but not if I could avoid it.) I'm not saying the 30A won't weld, but I am saying the gun is huge for any kind of close quarters, out of position, or small size circular or rolled welds that require high degree of welder motion to make the weld.

    But the measure of the man, in my opinion, was to take on your work, knowing the welds to be done and the equipment to do it... that is #1 dishonest or #2 so lacking in experience that they should not have been considered or #3 so unaware of good work the welded didn't know any better?

    I often tell young aluminum MIG welders " if you aren't between the lines you don't keep driving your car do you?" So if you're clearly in the 'ditch' beside the road instead of on the road, why do you keep putting down a bead: that is worse than driving in the ditch????

    It's not going to get better: stop. Something is wrong so you need to figure that out on scrap before you go ahead.

    Your man needs to be let go, you need to hire more carefully and remember all welders claim to be able to weld " Anything but the Crack of Dawn and a Broken Heart".
    "Why!! if you can jump a stallion over that gap at a full gallop; I can weld that sum'b**ch!"

    So "Trust but Verify" and that's what a weld test is. You need to test any future welder to make sure he/she can do what you need done. If you don't then you're making your own problems.

    If the work is done wrong (done once) you'll have to take it out (done twice) and then do it again (done three times) so it can be said its three times faster to the job right: once.

    Cheers,
    Kevin Morin

  7. #32
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Dave and Kevin, I really do appreciate the responses.

    The deal is, this guy is a Naval Academy-trained marine engineer. Or maybe I should say allegedly, since I haven't seen the actual sheepskin. He's got a very well equipped shop, with a 5" capacity shaft lathe, milling machine, Snap On MIG and TIG machines etc. I've seen both stainless and aluminum work come out of his shop and it's all looked pretty good. I'd say he's a marine mechanic/machinist with good welding machines in the shop as opposed to him being a "welder." I hope that makes sense.

    I got the TB280 and Spoolmatic because it's a big aluminum boat project and I've always been a DIY type. Also, there's lousy power supply out in the boatyard, so it made sense to get a welding power supply that can also output 240vac. I wouldn't think twice about firing it up to weld a non-critical bracket, but we're talking cutlass bearing housings and the hull near the waterline. That's the point where I want a pro to do it right.

    Anyway, I sent him an email with "All stop" in the subject line. He called back and we had words...tried to keep it short and professional. He said there was "good penetration" and that the welds would "grind down nice and flat." I was tempted to quote some observations that were made here, but decided not to. I know he'll talk smack about me no matter what (it's kind of a small town), but I don't want to hurt the guy's feelings any more than necessary. It'll be interesting to see the final bill...

    I've been on the phone to a few local welders and have already nixed two from the possible pool.

    You know...what I need is one of those things from the movie The Matrix where you plug something into your head and next thing you know, you're a kung fu master. I need that, but with advanced MIG/TIG training! lol

    Q
    Last edited by q240z; 07-02-2013 at 03:13 PM.

  8. #33
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,156
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    In the shop is different than spool gun at the dock.

    Make them show you they can dial it in perfect. On site test required.

    If they say they need an hour to experiment with your machine before showing you welds, I'd say let them.

    Dave J.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  9. #34
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    I was looking at his settings on my TB280 today. 3/16" plate and the amps were dialed down to 80. Seems kinda low to me.

    He also cranked the wire tension thumbscrew inside the gun so tight that the tensioner couldn't be pushed "home." This is with .35" wire.

    Last time he welded with it, he had it cranked up to 210 and was burning up tips like crazy (and blaming the machine). I set it at 140 and played with the wire feed until it seemed to be welding better. You guys would have had good cause to rip into my welds, too, but they looked better than his!

    Oh, and I just got the final bill. It includes the hour or so he spent playing with the machine to learn how it works and 4 hours to weld in the plate in the exhaust hole in that pic I posted.

  10. #35
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    8,498
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    [QUOTE=q240z;2826941
    You know...what I need is one of those things from the movie The Matrix where you plug something into your head and next thing you know, you're a kung fu master. I need that, but with advanced MIG/TIG training! lol

    Q[/QUOTE]

    Then you wouldn't need a boat- just plug in and " experience" it all



    Good luck with finding a competent weldor.
    Enjoyed the blog
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  11. #36
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Thanks, Ed!

    What I want is the instantaneous training program outside of the Matrix, not the "blue pill." ;-)

    Q

  12. #37
    Join Date
    Jun 2013
    Location
    Glen Mills, PA
    Posts
    119
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    "Naval Academy-trained marine engineer" is not a welder, more like a philosopher of floating objects.

  13. #38
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    I suppose, wade23454, but I remember what I learned in Material Science back when I thought I wanted to be a civil engineer, and I could see how understanding metal at the molecular level might help make an even better welder. But apparently not this one...

    I interviewed three potential welders yesterday. Two of the three guessed who the guy was after I described him as a mechanic who said he could weld but the final product shows he couldn't. He had great references from customers I spoke with, but the local pros know his work and gave it a thumbs-down.

  14. #39
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    With the previous mechanic/welder off the scene, I've begun to question some of his ideas for the engine install. For example, the boat has 1/4" 5086 plating on the hull and I'm relocating the exhaust outlet from the transom to just in front of the aft engine room bulkhead. This will avoid station-wagon effect and keep diesel exhaust fumes out of the boat, as well as drastically reducing back pressure and giving an additional foot of width to the aft cabin.

    I thought it might be reasonable to make an exhaust outlet from 6" and 8" aluminum tubing and weld it directly to the hull. The mechanic/welder didn't like that idea because he felt it would not be possible to get clean welds from 45 year-old aluminum. He suggested making the outlet from fiberglass, and bolting it to the hull with 3M 5200. Any thoughts on which would be preferred? Stainless bolts present potential dissimilar metal problems for the FRP approach, but then dissimilar alloy is what I'm looking at going with the welded version.

    Here's what I had in mind for the outlet:









    In other news, today's article is on priming the deck for the last time. I also threw in some CAD sketches of the non-skid.

    1969 Chris Craft Roamer 46 Refit: Final Sanding and Primer on the decks

    Cheers,
    Q


  15. #40
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    993
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    The outlets should be welded to the hull by a pro. You should leave room for proper mufflers and use flexible connections so engine vibration isn't transferred to the hull.

  16. #41
    Join Date
    Apr 2010
    Location
    Kenai, Alaska
    Posts
    772
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    q240z, I'm glad to hear you're getting more control of the personnel and therefore work on your project. I think the idea that someone took more than an hour to put in the patch you showed above to fit, tack, & weld -seems excessive -but I don't know its location or the logistics of your work space either.

    I will remark that you've paying for education and therefore what may seem a high bill was just an expensive lesson- and you got what you paid for; not necessarily in work done but in education of the real level of effort it takes to do your project correctly.

    Regarding the spool gun adjustments, this is probably widely known but here is how to adjust the wire. First loosen the wire drive compression roll tension spring/screw until the wire will not feed. These tests are all done with a gloved hand on the left, and the MIG torch in your right hand.

    Hold the gun and pull the trigger with the gas off, and no 'ground' near you or your MIG gun. The loosened drive roll set, (powered roller and tension/compression roller) should not feed wire, the resistance of coiling the wire into your gloved hand should be too much so the wire stays still and the driven roll turns/"spins out".

    Now tighten the tension screw and repeat. Continue until the drive roll will feed with wire into a tightly coiled 'bird's nest' into the palm of the gloved hand and then release 1/4 turn and see if will still feed?

    The goal is to have the tension 'just' above the spin out, low tension pressure and the 'too tight' place where the gun will STALL the drive roll when you stop the wire.

    Not sure if that made sense when read (? hope so) but this is the first balance of MIG gun wire drive tension adjustment for a 1lb. gun.

    Next the tips, the bore is critical to aluminum a little more critical than steel wire. 0.035" wire tips MAY be, don't know your tip brand/supplier/labels, marked with WIRE SIZE? Some others tips may be labeled with BORE size. This is super-important because the wire to copper tip gap is critical to smooth wire feed.

    The SIZE of the bore of the MIG contact tip for 0.035" wire should be from 0.040" up to 0.053" actual size depending on high your welding range. (at the upper end it may be time to switch up to 0.045" wire.) So the tips may be labeled 0.040", 0.044", 0.053" OR they may be labeled; 0.035". One set of markings is for the diameter of original bore or the tip and the other is for 'this size wire' and the latter marking may be on any of the three sizes above!!!

    I have seen this 'unknown factor' absolutely frustrate welders who didn't choose the right tip bore because of the labeling.


    Further confusing is: if the tips are labeled by WIRE size then a tip labeled 0.045" may be confused for a TIP BORE of 0.045" when it is bored to 0.055" or 0.060" for use with 0.045" WIRE.

    So, if a 'too large' bore tip is used, (or too small) the there will be 'tip arc' inside the tip and that will stick the wire to tip causing excessive burn back. Many welders with too little experience will diagnosis this as loose drive rolls since the general symptoms are similar: burn back and tip fusion for failure to feed wire.

    However the wire feed is not always the culprit, tip bore and a CLEAN bore is the key to most of these problems once the wire feed drive roll tension is set correctly.

    Last but not least in regard tip burn back in aluminum, many welders don't pay adequate attention to the ground connection tot he work where they have a high resistance connection that only 'grounds' -just after- the initiation of the weld sequence. So, the open circuit voltage used to 'light ' the wire is consumed in an unseen arc because the ground clamp is one used for steel and has not been correctly sanded and clamped.

    Open circuit surges of 70 or 80 volts are common for a part of a second in most MIG power supplies but it should be at the tip of the now feeding wire- not between the rough, pitted, loosely fitted "steel" ground clamp. That arc must be at the tip of the wire, so if the wire won't feed OR if the wire surges unlit- then bounces off the parent metal, the lifting of the contact tip will result in a weld surge and the tip may burn back-....

    Hope this helps with some of your weld gun questions?

    I'd remark more about your exhaust fittings if I could understand if this is a wet overboard? The flange component will not allow you to get the gun into the inboard side to back weld as it is designed. (that includes even experienced and skilled welders- there's just not room for the gas cup to get close enough.)

    I'd use a double layer flange if it will be welded outside the hull only? That is the idea from my previous hull patch example where a weld joint backup plate is provided to fuse the root of the "outboard only" weld.

    I would avoid the vertical 'cut off' of the flange and make it oval to spread the heat, and make the patch's area of contraction uniform instead of 'notched'.

    If this is a wet mixture of exhaust and seawater, I'd design this thru-hull differently if it were mine.

    Also, I'd turn off the 'sketchy' line type so that the images are more machine and less art drawings. There are details of the joints and shapes that would be more easily understood without that line less cluttered type.

    Last, I think I'd put a translucent 'hull topsides' pane and a translucent bulkhead in their relationship to the through hull into the images. Then mock up the MIG gun and show yourself how it could be back welded? Looks tight to me?

    cheers,
    Kevin Morin
    Kenai AK

  17. #42
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Kevin, thank you so much for the detailed post.

    The patch in the pic is about 5' off the ground, with open space all around, and it's inside a shrink wrap tent/scaffolding structure that surrounds the entire boat...basically, it's in a shop-like environment but with a compacted gravel floor.

    I used to own a six-man collision repair shop. Finding good help was always a problem. Everybody talks up their skills, but sometimes the finished product doesn't support the talk. Word has it, virtually every employer in the skilled trades faces the same sort of issues. I admit, though, that my BS detector has been on the fritz lately...either that, or the marine trades have a larger percentage of guys who are full of 5h1t than the automotive sector.

    On the contact tips, the mechanic/welder wanted to use .35 wire, so I bought the FASTIP tips, PN 206187 (.312" OD .035-0.40" AL WIRE 25 PER PKG). I had no idea they were sold with either bore or wire size specs.

    On the exhaust component, this is a wet exhaust application. I'll be using waterlift mufflers with 6" inlets and outlets, and hose connections to isolate vibration. You mentioned you'd do it differently if it was a wet exhaust. If you have time and are so inclined, I'd be very interested to hear what you have in mind. One thing to keep in mind is that the interior hull is coated with 1969-era bitumastic, a hard, tar-like material that's painted over but melts when heated or in the presence of petroleum (including mist from engines). Where the exhaust would go, the bitumastic is in good shape and is very difficult to remove entirely.

    The oval approach for the flange makes sense, but I actually envisioned just cutting a hole in the hull so the exhaust pipe would just fit through, then weld up the gaps around inside and out. The mechanic/welder felt the exterior baffle was unnecessary, but then I'm no longer paying attention to his opinions even with several grains of salt.

    The only other option that's come to mind is to just make the exhaust outlet in FRP and bolt the flange to the hull with 3M 4200 or Sikkaflex to seal the connection. I'd cut the hole, wax the hull, push the FRP pipe through and then make the flange in place so it conforms to the hull. After the epoxy resin cured, I'd remove the component then refit it and drill the mounting holes...probably use delrin spacers and oversized holes to isolate the stainless bolts from the aluminum.

    In other news, I came up with a few alternate designs for the non-skid based on comments I've received. Check them out and vote for your favorite at 1969 Chris Craft Roamer 46 Refit: Cast Your Vote for the Non-skid Layout

    Cheers,
    Q


  18. #43
    Join Date
    Apr 2010
    Location
    Kenai, Alaska
    Posts
    772
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    q240z,
    I agree hiring really top skills are a limit to doing quality work if you're a contractor. And if you create a skill building program in your business; it can end up creating skilled competition if it's not organized in a very clear way from the beginning- not all that easy to do.

    First, hull coating in general then in specific. In general if the inside of a hull will be finished it's good practice to use a coal tar epoxy or other paint system to keep the moisture from the bare metal. And sprayed tars are a good way to do this simply; once the fab is done and you're ready to add the systems on top of the metal.

    But, if you want to repair, replace or modify it's somewhat like automobile undercoating- its a pain in the stern. But it can be removed in a fairly controlled way if you do some planning.

    If you don't plan to remove the inner liner coating: don't plan to weld on the hull. Only plan to weld if you plan to take the time and effort to clean (really Capital C- clean) the hull, inside, and out where your welds will be.

    To remove the tar, (you can) get a set of rags of the diameter of the cutout (round?) plus about 4" so for a four inch hole you'd have round rags 12" in diameter. Wet, but not dripping, with a solvent (Stoddard if its still sold?) or kerosene or white gas, and then lay the rags (two or three layers) over the area to be cleaned.

    Tape a plastic bag over the area too, sealing in the rags even on the vertical. This keeps the volatiles from evaporating into your hull and means the VOC's will work their solvent magic to soften the cooled and dried tar coating. Wait till it's good and soft, then use a putty knife with a wide blade to scrape it off into a bucket or bag.

    Once the worst is gone, then you can use a gloved hand and rags to keep cleaning until you're to what appears to be 'bare' metal. Now you can clean the hull, but I'd make the weld cut out first, and then clean once the cutting lube and saw work is done.

    The remarks I was making about the wet exhaust riser is that exhaust is pretty acidic and mixed with salt water is tough on aluminum pipe. I'd make it of sched. 80 or even 160 to avoid having to do this work more than once- it will pit and corrode inside.

    The question of a spray shield is not as critical with a water lift muffle its mainly to keep the swell from flooding the riser with direct force instead of just level flooding. An opening on the side or stern can be forced pretty hard when the right swell comes along so a covering is not unwise to keep from having any back pressure surges. With the riser the shroud is not critical but it won't hurt, you've shown it as though it were from cut down forged 90 which in 6" is going to cost a house payment. I'd use a scallop of straight pipe section and call it good; I'd skip the compound form as unneeded.

    My idea for this fit is to make sure you (can) clean the hull on both sides adequately to bare metal or don't bother welding. The same goes for gun position and 'reach" meaning; can the gas cup get to within a reasonable distance of the weld zone?

    Last, the turn tight of pipe or tube to the hull is a potential design problem, you need the inboard space clear- but the close area to the hull makes working welding and re-coating a major pain in the stern. I'd usually use a sea chest, a box-like structure, to convey fluids overboard tight to the hull with out welding more than an opening, and it may be a good idea to consider a flanged repair point too? That way the riser/sea chest is a 'bench built' part you can replace without more than wrenches.

    "sketchy" lines setting still seems to put overlap or 'hogs' at the ends of the arc segments in the sheer clamp in the bow too view you show of the decking. I'd sure be worried about side to side visibility with those "blinders" on the forward sides of the trunk windscreen, I guess the helm must be up another level?

    Cheers,
    Kevin Morin

  19. #44
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Thanks for the info, Kevin.

    I think I'm leaning toward a fiberglass exhaust outlet.

    On the windows, the helm station is, indeed, up one level. The fwd windows you see are for the galley/salon. The boat will look something like this when she's all assembled:



    Cheers,
    Q

  20. #45
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    The latest article on my Roamer 46 refit is a bit of a rant about the way one contractor (the mechanic/pseudo-welder) falling off schedule early on can have ripple effects that go on (for what feels like) forever, significantly adding to both the completion time and the cost of a big project like this. The article ends, though, with pix of the decks primed in Awl Grip 545 -- the final prime coat before we start painting the topsides!

    1969 Chris Craft Roamer 46 Refit: The Butterfly Effect


    Cheers,

    Q


  21. #46
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    OK, after interviewing ten guys, I've settled on somebody I have confidence in. He's got lots of marine experience, including DoD work. He's coming out this week to look at what needs to be done. AND, he says he can align the engines. Now I just need to find a machine shop that will do shafts they didn't sell.

    In other news, the weather gods really do need to just stop kickin' me in the nether regions. Then again, I suppose I can't blame the weather gods for a clown mechanic who threw the whole schedule off...

    Anyway, we've got the cabin top final sanded and ready for the shiny Awl Craft 2000. Just two more days of prep work and we'll spray early one morning before it gets too steamy.

    1969 Chris Craft Roamer 46 Refit: Final sanding the cabin top
    Cheers,
    Q


  22. #47
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    It's like Christmas in July!

    A box arrived from Kocian Instruments and a bunch of sparkly stuff was inside.

    1969 Chris Craft Roamer 46 Refit: Shiny Gauges

    Back to the boatyard...

    Q


  23. #48
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    I took a week off to get the topsides all painted only to get sidelined by yet another SMIB-ification. The Southern Maryland "fabricator" who created my aft enclosure (a different guy than the last mechanic/welder) welded it all together with twist in three of the six window frames. gak

    Anyway, my latest article covers my solution to the window problem he created. 1969 Chris Craft Roamer 46 Refit: Aft enclosure windows

    Cheers,
    Q


  24. #49
    Join Date
    Jan 2011
    Location
    Mid-Atlantic, USA
    Posts
    1,039
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Thanks, 7A749!

    I've been trying to figure out if I've just got the worst luck with contractors or what. But it seems that the more people I talk to who have work done by "marine tradesmen," the more it seems I'm not alone by a long stretch.

    Anyway, thanks for the kudos.

    Q

  25. #50
    Join Date
    Jan 2008
    Location
    Lansing, MI
    Posts
    6,117
    Post Thanks / Like

    Re: Aluminum Chris Craft Roamer refit project

    Quote Originally Posted by q240z View Post
    Thanks, 7A749!

    I've been trying to figure out if I've just got the worst luck with contractors or what. But it seems that the more people I talk to who have work done by "marine tradesmen," the more it seems I'm not alone by a long stretch.

    Anyway, thanks for the kudos.

    Q
    I have luck with Syncrowave 250s like you have with "contractors"

    Hard to find qualified ppl who are actually as "qualified" as they say they are.

    Great boat. Great documentation!!!!!!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,830,631.70485 seconds with 11 queries