Thread: Sheet-Gauge Thickness Chart

  1. #26
    Join Date
    Jan 2005
    Posts
    38
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    Thanks printed out 2 copies and laminated them to put in my tool box

  2. #27
    Join Date
    Jul 2009
    Location
    Western NC
    Posts
    141
    Post Thanks / Like

    Re: Printable table in Word

    Quote Originally Posted by Bobcatter View Post
    Great information, thanks. I formatted it into Word so I could print and post it. Sheez, allergies, keep me up all night....

    Okay, I made the file smaller, so I could upload it. You can put your own title on it.
    Thanks for the work. I made a few copies for the study, shop, etc...
    Nctox,
    Stickmate LX 235AC/160DC
    HH210

  3. #28
    Join Date
    Jan 2008
    Location
    Arkansas
    Posts
    1,202
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    Charts attached.
    Attached Files Attached Files
    A butterfly without wings,
    is just an ugly bug


  4. #29
    Join Date
    Mar 2008
    Location
    Greater Seattle, WA
    Posts
    592
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    Here is the table from the original post with improved formatting:

    Code:
    Thickness Weight
    Gauge   Frac.   Inch       mm         oz/ft^2 lb/ft^2 kg/ft^2 kg/m^2 lb/m^2
    0000000 1/2     .5         12.7       320     20.00   9.072   97.65  215.28
    000000  15/32   .46875     11.90625   300     18.75   8.505   91.55  201.82
    00000   7/16    .4375      11.1125    280     17.50   7.983   85.44  188.37
    0000    13/32   .40625     10.31875   260     16.25   7.371   79.33  174.91
    000     3/8     .375       9.525      240     15      6.804   73.24  161.46
    00      11/32   .34375     8.73125    220     13.75   6.237   67.13  148.00
    0       5/16    .3125      7.9375     200     12.50   5.67    61.03  134.55
    1       9/32    .28125     7.14375    180     11.25   5.103   54.93  121.09
    2       17/64   .265625    6.746875   170     10.625  4.819   51.88  114.37
    3       1/4     .25        6.35       160     10      4.536   48.82  107.64
    4       15/64   .234375    5.953125   150     9.375   4.252   45.77  100.91
    5       7/32    .21875     5.55625    140     8.75    3.969   42.72  94.18
    6       13/64   .203125    5.159375   130     8.125   3.685   39.67  87.45
    7       3/16    .1875      4.7625     120     7.5     3.402   36.62  80.72
    8       11/64   .171875    4.365625   110     6.875   3.118   33.57  74.00
    9       5/32    .15625     3.96875    100     6.25    2.835   30.52  67.27
    10      9/64    .140625    3.571875   90      5.625   2.552   27.46  60.55
    11      1/8     .125       3.175      80      5       2.268   24.41  53.82
    12      7/64    .109375    2.778125   70      4.375   1.984   21.36  47.09
    13      3/32    .09375     2.38125    60      3.75    1.701   18.31  40.36
    14      5/64    .078125    1.984375   50      3.125   1.417   15.26  33.64
    15      9/128   .0703125   1.7859375  45      2.8125  1.276   13.73  30.27
    16      1/16    .0625      1.5875     40      2.5     1.134   12.21  26.91
    17      9/160   .05625     1.42875    36      2.25    1.021   10.99  24.22
    18      1/20    .05        1.27       32      2       .9072   9.765  21.53
    19      7/160   .04375     1.11125    28      1.75    .7938   8.544  18.84
    20      3/80    .0375      .9525      24      1.50    .6804   7.324  16.15
    21      11/320  .034375    .873125    22      1.375   .6237   6.713  14.80
    22      1/32    .03125     .793750    20      1.25    .567    6.103  13.46
    23      9/320   .028125    .714375    18      1.125   .5103   5.493  12.11
    24      1/40    .025       .635       16      1       .4536   4.882  10.76
    25      7/320   .021875    .555625    14      .875    .3969   4.272  9.42
    26      3/160   .01875     .47625     12      .75     .3402   3.662  8.07
    27      11/640  .0171875   .4365625   11      .6875   .3119   3.357  7.40
    28      1/64    .015625    .396875    10      .625    .2835   3.052  6.73
    29      9/640   .0140625   .3571875   9       .5625   .2551   2.746  6.05
    30      1/80    .0125      .3175      8       .5      .2268   2.441  5.38
    31      7/640   .0109375   .2778125   7       .4375   .1984   2.136  4.71
    32      13/1280 .01015625  .25796875  6 1/2   .40625  .1843   1.983  4.37
    33      3/320   .009375    .238125    6       .375    .1701   1.831  4.04
    34      11/1280 .00859375  .21828125  5 1/2   .34375  .1559   1.678  3.70
    35      5/640   .0078125   .1984375   5       .3125   .1417   1.526  3.36
    36      9/1280  .00703125  .17859375  4 1/2   .28125  .1276   1.373  3.03
    37      17/2560 .006640625 .168671875 4 1/4   .265625 .1205   1.297  2.87
    38      1/160   .00625     .15875     4       .25     .1134   1.221  2.69

  5. #30
    Join Date
    Jan 2009
    Posts
    495
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    according to the charts, our modern cars are 1/32" thick skin...(.22ga.) I don't think the older cars were 18 ga. as stated , I was told the 50 ish cars were 20ga... anyway 1/32" sounds scary.....

  6. #31
    Join Date
    Nov 2009
    Location
    lancaster,kentucky
    Posts
    884
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    I was needing this info about 2 weeks ago,I printed 1 out and saved it on my computer for future copies
    Maxus Pro-125 Mig
    Chicago Electric 90 amp DC flux-core
    Lincoln Electric AC 225 tombstone
    O/A torch
    M/O mini-torch
    10 acres of flatland
    15 acres of holler

  7. #32
    Join Date
    May 2009
    Location
    Portland, ME
    Posts
    774
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    anyone else find it interesting that a square foot of 1/2" thick steel is EXACTLY 20.00 lbs?

    Pretty cool!

  8. #33
    Join Date
    Jan 2010
    Posts
    341
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    http://www.google.com/products/catal...&ved=0CBIQrRI#

    i've been using one of these for a long, long time.

    if you can work with fractions and you know that steel is app 40 lbs per ft sq, then it is pretty easy to convert to whatever you are dealing with.

    ie .125/1/8th is equal to 5lbs per ft sq

    .062/1/16th us equal to half of that.

    after a while you can do them in your head. at least you can ball park a weight this way.

  9. #34
    Join Date
    Dec 2011
    Location
    Texas
    Posts
    634
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    Quote Originally Posted by fdcmiami View Post
    http://www.google.com/products/catal...&ved=0CBIQrRI#

    i've been using one of these for a long, long time.

    if you can work with fractions and you know that steel is app 40 lbs per ft sq, then it is pretty easy to convert to whatever you are dealing with.

    ie .125/1/8th is equal to 5lbs per ft sq

    .062/1/16th us equal to half of that.

    after a while you can do them in your head. at least you can ball park a weight this way.
    Thanks FDC. That got me to thinking since I'm making a table base out of 1" square tube.

    A 3 foot length of 11 gauge (1/8") mild steel would also be 5 pounds, because it's 144 in2 (one square foot).

    And since 16 gauge is half as thick, a 3 foot length would be 2.5 pounds.

    And a 22 guage would weight half as much again - 1.25 pounds.

    Very helpful now that I've got it in my head.

  10. #35
    Join Date
    Aug 2011
    Location
    Texas
    Posts
    96
    Post Thanks / Like

    Re: Sheet-Gauge Thickness Chart

    Thanks. This is really good to know, especially the weight per square foot.
    Matthew Morton
    Texas A&M '06

    SA 200 (Code: 6633)
    TB 302
    CP 302 w/22A Wire Feeder
    MillerMatic 141
    MillerMatic 200
    Miller Syncrowave 200
    MillerMatic 252
    MillerMatic 350P
    BurnTables 4x4 CNC Machine
    Hypertherm 65

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,285,754.46517 seconds with 21 queries