    How long does Argon last?

    Hello all -- first post here. I am learning to TIG aluminum with a new Diversion 165. I got a 20 cubic foot bottle of Argon and thought it would last a long time for a hobby welder, but after less than a few hours of practice it's empty. Is that normal?!? I set it to 12-15 or so on the gauge it comes with.

    My MIG will last a year or more on a 40 cubic foot tank of gas, so just assumed I'd get months out of a little tank of argon. Did I get a near-empty tank or is it normal to use it up that fast?

  2. #2
    Join Date
    Mar 2009
    Location
    MN
    Posts
    5,157
    Post Thanks / Like

    Re: How long does Argon last?

    A 20 cf bottle is way too small. At 15cfh, you will get a little over an hour of arc time.
    My name's not Jim....

  3. #3
    Join Date
    May 2010
    Location
    laguna niguel, Ca USA
    Posts
    1,183
    Post Thanks / Like

    Re: How long does Argon last?

    that tank is kid sized you will only get about a hours weld time with a 20cf bottle

    i would step up to a 80 to 154 cf bottle
    or bigger
    Last edited by WeldorWes; 08-22-2013 at 01:11 AM.
    Miller Xmt 350
    Lincoln Ln-25
    Ahp 200x
    Smith Gas Mixer AR/H
    Tig is my Kung Fu
    Throwing down dimes and weaving about
    Instagram http://instagram.com/weldor_wes
    WeldorWes@WcWeldingLLC.com

  4. #4
    Join Date
    Feb 2012
    Posts
    4,228
    Post Thanks / Like

    Re: How long does Argon last?

    Non linear dynamics.
    Im thinking because the bigger the tank, the better the economy

  5. #5
    Join Date
    Jul 2011
    Location
    Utah
    Posts
    2,190
    Post Thanks / Like

    Re: How long does Argon last?

    Quote Originally Posted by Boostinjdm View Post
    A 20 cf bottle is way too small. At 15cfh, you will get a little over an hour of arc time.
    or significantly less depending on your post flow time.
    Welding/Fab Pics: www.UtahWeld.com

  6. #6
    Join Date
    Mar 2009
    Location
    MN
    Posts
    5,157
    Post Thanks / Like

    Re: How long does Argon last?

    Quote Originally Posted by MikeGyver View Post
    or significantly less depending on your post flow time.
    True, that's why I didn't say an hour and a half.
    My name's not Jim....

  7. #7
    Join Date
    Aug 2013
    Posts
    76
    Post Thanks / Like

    Re: How long does Argon last?

    Ok, thanks, at least the gas place didn't rip me off with a near-empty bottle.

    My 40 cubic foot tanks for my MIG welder have lasted over a year, and I could swear I've welded 10 times more and they're still going strong. It that a perception thing or do MIGs use less gas (even though the flow rate seems comparable....)?

  8. #8
    Join Date
    Aug 2013
    Posts
    76
    Post Thanks / Like

    Re: How long does Argon last?

    Quote Originally Posted by MikeGyver View Post
    or significantly less depending on your post flow time.
    Post flow time is controlled by the Diversion -- no adjustable as far as I know.

  9. #9
    Join Date
    Mar 2009
    Location
    MN
    Posts
    5,157
    Post Thanks / Like

    Re: How long does Argon last?

    Tig is generally slower than Mig. Especially for a beginner. That means less weld for the same amount of gas
    My name's not Jim....

  10. #10
    Join Date
    Aug 2013
    Posts
    76
    Post Thanks / Like

    Re: How long does Argon last?

    Quote Originally Posted by Boostinjdm View Post
    Tig is generally slower than Mig. Especially for a beginner. That means less weld for the same amount of gas
    Well, that's certainly true in my case... I guess I'm getting a bigger bottle.... Thanks all.

  11. #11
    Join Date
    Jul 2008
    Posts
    2,907
    Post Thanks / Like

    Re: How long does Argon last?

    Cheapest way to buy argon is usually in the biggest bottle they lease. 330 or 300 CF (Airgas) is the way to go if you want to save $, especially since the annual lease on a big bottle is not much more expensive (if at all) than a smaller bottle.

  12. #12
    Join Date
    Aug 2013
    Posts
    1
    Post Thanks / Like

    Re: How long does Argon last?

    Hi tom86951
    Argon in a tank is a gas and it last at the rate you use it in cfh (cubic feet per hour). when it gone it's gone. Carbon dioxide is a liquid in the tank and it changes (vaporizes) to a gas as you use it until all the liquid is gone. Thus a smallish tank of carbon dioxide lasts much longer.

  13. #13
    Join Date
    May 2010
    Location
    Wyoming
    Posts
    70
    Post Thanks / Like

    Re: How long does Argon last?

    Not possible to tig weld with CO2 - You have to use argon or an argon helium mix.

    John

  14. #14
    Join Date
    May 2006
    Location
    Northern California
    Posts
    1,862
    Post Thanks / Like

    Re: How long does Argon last?

    Quote Originally Posted by tmind View Post
    Hi tom86951
    Argon in a tank is a gas and it last at the rate you use it in cfh (cubic feet per hour). when it gone it's gone. Carbon dioxide is a liquid in the tank and it changes (vaporizes) to a gas as you use it until all the liquid is gone. Thus a smallish tank of carbon dioxide lasts much longer.
    A 20 pound C02 cylinder is approximately equivalent to a 160 cu.ft high pressure gas cylinder. This is because one pound of C02 will expand to provide approximately 8 cu. ft. of gas.

    A MIG unit is somewhat more economical on shielding gas since there is no pre or post-flow on a MIG machine.

    I use straight C02 with my MM252 because it is less expensive and gives excellent penetration. There can be more spatter than Argon mix but it can be controlled with liberal use of welding gel.
    Miller Millermatic 252
    Miller Syncrowave 200
    Liincoln AC-DC 225
    Victor O-A Set

  15. #15
    Join Date
    Aug 2013
    Posts
    76
    Post Thanks / Like

    Re: How long does Argon last?

    Quote Originally Posted by tmind View Post
    Hi tom86951
    Argon in a tank is a gas and it last at the rate you use it in cfh (cubic feet per hour). when it gone it's gone. Carbon dioxide is a liquid in the tank and it changes (vaporizes) to a gas as you use it until all the liquid is gone. Thus a smallish tank of carbon dioxide lasts much longer.
    Now that makes sense and explains why this argon goes so much faster. Thanks.

  16. #16
    Join Date
    Dec 2011
    Location
    Idaho
    Posts
    364
    Post Thanks / Like

    Re: How long does Argon last?

    How long does it last??? Well, if you freeze it, it won't spoil for about a year. If you just keep it in the fridge, it'll last for about 3 months.

    Old rotten argon starts to really stink if its kept in the warm weather.
    "Hey I didn't come to look and learn, I came to turn and burn.... If I can't light up, I'm gonna light out!"
    -Jody

    Idealarc 250 "Fatman"
    MM 252
    MM 211 "Little boy"
    Victor Torches

  17. #17
    Join Date
    Feb 2013
    Location
    St.louis
    Posts
    126
    Post Thanks / Like

    Re: How long does Argon last?

    Hey Tom. I'm in the same situation. Cheaped out with the small tank when I bought my diversion 180 and I have already filled it 3-4 times with barely any use. I am definitely upping to a large tank ASAP! Lesson learned. To me, the lack of pre/post flow settings on the diversions sucks but it is meant to be plug n play as you know.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,191,882.18911 seconds with 13 queries