Quote Originally Posted by littlefuzz
How well does the HF needle scaler work? It's about half price of others I've seen. I never have liked cheap pneumatics but it won't be used everyday, just wondering if it was worth it.
I have one that I've used for cleaning thin set tile cement from concrete. It works pretty well, but I've never used any other needle scaler to compare it to.