Results 1 to 8 of 8

Thread: hobat stickmate lx ,leads

  1. #1
    Join Date
    Oct 2013
    Location
    holly mi
    Posts
    7
    Post Thanks / Like

    hobat stickmate lx ,leads

    picked up this welder leads were removed . I am sure they go to the select switch ,but to what lugs? any help will be great.thanks.

  2. #2
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,159
    Post Thanks / Like

    Re: hobat stickmate lx ,leads

    A pict of the inside would help us explain where you need to hook them up.
    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  3. #3
    Join Date
    Oct 2013
    Location
    holly mi
    Posts
    7
    Post Thanks / Like

    Re: hobat stickmate lx ,leads

    will post sunday ,thanks

  4. #4
    Join Date
    Oct 2013
    Location
    holly mi
    Posts
    7
    Post Thanks / Like

    Re: hobat stickmate lx ,leads

    Name:  Photo11101658.jpg
Views: 169
Size:  37.7 KBName:  Photo11101659.jpg
Views: 173
Size:  43.6 KBName:  Photo11101659_1.jpg
Views: 181
Size:  63.2 KB I have one screw out of the buss , and one where the connection is off . hope this helps.

  5. #5
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,159
    Post Thanks / Like

    Re: hobat stickmate lx ,leads

    OK, It's an AC only machine, so you don't need to worry about which connection is typically + or - like on an AC/DC unit. It won't matter which lead is the ground and which is the stinger on an AC only machine.

    here's the manual for that machine I believe.

    http://www.hobartwelders.com/om/0900/o950c_hob.pdf

    If I'm reading the wiring schematic correctly, it looks like one lead attaches to where those screws are missing on each terminal. Maybe Duane or Steve can double check me since I don't do a whole lot with wiring diagrams.

    Name:  AC stickmate.jpg
Views: 159
Size:  26.2 KB


    Since you have to put all new leads on anyways, I'd look at either adding panel quick connects or short leads with quick connects on them so you can add or subtract lead as needed. I upgraded my Miller Thunderbolt ( same basic machine you have) to them so I could use my extra leads on it if I needed to.
    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  6. #6
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,879
    Post Thanks / Like

    Re: hobat stickmate lx ,leads

    leads connect to terminals 6 and 2,
    2 should be the one with the transformer lead, 6 is just below the mount.
    looking at the back of the switch, count clock wise from two to six. look close at switch, numbers might be molded into switch

  7. #7
    Join Date
    Oct 2013
    Location
    holly mi
    Posts
    7
    Post Thanks / Like

    Re: hobat stickmate lx ,leads

    Thanks guys , that is the same drawing on the cover inside. What is off is there are 4 transformer legs on the switch ,two on one lug but i think also where i pulled the screws were the correct spots. As for the leads , i run a thirty foot extenson on my 220. That way it brings my mig & stick out to the same work areas. I will get her wired up today and try it out. thanks on the manual link seems to be correct always helpful with a used unit. let you know how it works out.

  8. #8
    Join Date
    Oct 2013
    Location
    holly mi
    Posts
    7
    Post Thanks / Like

    Re: hobat stickmate lx ,leads

    Must say i am welding again ,connections were correct, thanks all.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,137,138.91869 seconds with 14 queries