Page 3 of 614 FirstFirst 123451353103503 ... LastLast
Results 51 to 75 of 15334

Thread: Show us what you welded today

  1. #51
    Join Date
    Feb 2012
    Location
    ny
    Posts
    6,178
    Post Thanks / Like

    Re: Show us what you welded today!

    I started making a shark. 6hrs in about 200 more to go! Name:  get-attachment.jpg
Views: 10126
Size:  28.5 KB
    I hate being bi-polar it's awsome




    My Heroes Have Always Been Cowboys

  2. #52
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by weldermike View Post
    I started making a shark. 6hrs in about 200 more to go!
    When you get done with that shark you can come down here and catch one.
    Attached Images Attached Images  
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

  3. #53
    Join Date
    Feb 2012
    Location
    ny
    Posts
    6,178
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by SquirmyPug View Post
    When you get done with that shark you can come down here and catch one.
    The one I'm building already looks bigger than that!
    I hate being bi-polar it's awsome




    My Heroes Have Always Been Cowboys

  4. #54
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by weldermike View Post
    The one I'm building already looks bigger than that!
    Just a small one, was 4' 8" from tip of the nose to the fork in the tail
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

  5. #55
    Join Date
    May 2013
    Posts
    108
    Post Thanks / Like

    Re: Show us what you welded today!

    Pretty cool to see all the different things other guys are up to. Nice to see how you guys are making money. I am a small shop and do some field work. I have ASME R stamp and do some structural stuff also, so we do so many different things in any giving week. Its nice to keep it mixed up if we can.

    A few jobs from this week....

    Finished and installed a boiler condensate tank...
    Name:  ImageUploadedByTapatalk1387082592.083274.jpg
Views: 9897
Size:  51.7 KB

    Fabed and installed steel awning turnbuckles....

    Name:  ImageUploadedByTapatalk1387082669.649799.jpg
Views: 9901
Size:  60.8 KBName:  ImageUploadedByTapatalk1387082685.349188.jpg
Views: 9814
Size:  23.6 KB

    Field welded some aluminum flanges with a trailblazer/high freak box ...

    Name:  ImageUploadedByTapatalk1387082769.649144.jpg
Views: 9779
Size:  37.1 KB

    Nick

  6. #56
    Join Date
    Jul 2005
    Posts
    29
    Post Thanks / Like

    Re: Show us what you welded today!

    Well, it actually took 3 days, I just finished it TODAY. I only get the opportunity to do welding one day a week. My REAL job of managing a lumberyard pays the bills.

    Anyway, a local eye clinic recently installed solar panels on the their roof, and miscreants keep steeling the electronics that are on the wall.
    This will hopefully slow them down.
    96" wide, 65" tall, 18" deep, with double doors.
    Name:  1.jpg
Views: 9738
Size:  68.4 KBName:  2.jpg
Views: 9740
Size:  66.2 KBName:  3.jpg
Views: 9736
Size:  59.8 KBName:  4.jpg
Views: 9730
Size:  63.3 KB

  7. #57
    Join Date
    Jun 2013
    Location
    Raleigh, NC
    Posts
    140
    Post Thanks / Like

    Re: Show us what you welded today!

    Great projects! Has anyone built a welding screen? Typically a steel frame with either heavy canvas or some other type of dark burn resistant material so your welding flash and grinding sparks don't fly out of your work area. I was thinking of building some for my garage shop, need some ideas!

  8. #58
    Join Date
    Apr 2013
    Location
    NE
    Posts
    441
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by Bipestuff View Post
    Great projects! Has anyone built a welding screen? Typically a steel frame with either heavy canvas or some other type of dark burn resistant material so your welding flash and grinding sparks don't fly out of your work area. I was thinking of building some for my garage shop, need some ideas!
    You can get those screens at Northern or Harbor Fraud, and then I would just build a small 1x1 square tube frame for them!

  9. #59
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    2,132
    Post Thanks / Like

    Re: Show us what you welded today!

    This is a table I built for a co-worker. It will have a black granite top left over from his remodeling project.
    He plans to have it powder-coated a charcoal gray.

    Name:  TonyTable6.jpg
Views: 9600
Size:  66.3 KB
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 120

    www.10FtDrillBit.com
    www.MyWelds.com - pictures of my work

  10. #60
    Join Date
    Oct 2012
    Posts
    407
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by Bipestuff View Post
    Great projects! Has anyone built a welding screen? Typically a steel frame with either heavy canvas or some other type of dark burn resistant material so your welding flash and grinding sparks don't fly out of your work area. I was thinking of building some for my garage shop, need some ideas!
    I have a 4x10 welding table and am building a 5x10 at school. I am going to build a screen that sits on top of my table. It will be about 30" tall and about 8 feet long. It will have posts that I can move around the table, and build my screen to fit the project to keep from flashing people. I hope this makes sense. The posts will have a heavy base so they are free standing and easily moved around the table. It could be like a ping pong table net or three sided walls around a project what ever configuration you need.

    Maybe someone else has done this and can explain it better.

  11. #61
    Join Date
    Oct 2013
    Location
    Franklin County,VA
    Posts
    245
    Post Thanks / Like

    Re: Show us what you welded today!

    Car hauler, I don't like the fenders we put on it. We put plain sheet metal fenders on it, think it would look much better with some steel diamond plate fenders on it.
    Name:  car hauler.jpg
Views: 9233
Size:  39.5 KB
    93 Bobcat 225G
    MillerMatic 135
    HF Tig 91811

  12. #62
    Join Date
    Jun 2008
    Location
    The Cove
    Posts
    273
    Post Thanks / Like

    Re: Show us what you welded today!

    Lots of nice projects, SquirmyPug, What are the threaded studs for?
    American by birth Southern by the Grace of God

  13. #63
    Join Date
    Dec 2013
    Location
    near dayton ohio
    Posts
    589
    Post Thanks / Like

    Re: Show us what you welded today!

    this is what I have been working on for a while a bumper for my 95 f 350 far from finished but well on my way.

    Name:  100_2649.jpg
Views: 9114
Size:  50.9 KBName:  100_2664.jpg
Views: 9103
Size:  48.0 KBName:  100_2665.jpg
Views: 9061
Size:  49.6 KB
    Lincoln 225 ac (my first machine)
    farmhand 115vac 70amp mig/fc toy
    miller aead 200le (my main machine)

  14. #64
    Join Date
    Dec 2009
    Location
    NY
    Posts
    318
    Post Thanks / Like

    Re: Show us what you welded today!

    Cold as hell and no real welding to do so I gave my first attempt at razor blades think I need glasses to see what i am doing better.

    .5 preflow settings 5amp start 20amp 20% 280hz 4 sec post .40 rare earth tungsten 308L .035

    Name:  IMG_3321.jpg
Views: 9056
Size:  68.2 KB

    Name:  IMG_3322.jpg
Views: 9049
Size:  63.4 KB
    Last edited by nikodell; 01-01-2014 at 07:14 PM.

  15. #65
    Join Date
    Oct 2012
    Posts
    407
    Post Thanks / Like

    Re: Show us what you welded today!

    [QUOTE=nikodell;3501291]Cold as hell and no real welding to do so I gave my first attempt at razor blades think I need glasses to see what i am doing better.

    You can always put a magnifying lense in your helmet. It made a world of difference for me.

  16. #66
    Join Date
    Jan 2013
    Location
    Cozad, NE
    Posts
    122
    Post Thanks / Like

    Re: Show us what you welded today!

    Im doing a Dumping cart!! I'm just getting started. This is the frame.

    Name:  IMG_20131231_172935821.jpg
Views: 8892
Size:  49.3 KB

    It will be similar to this

    Name:  FB-ATV.jpg
Views: 8882
Size:  39.4 KB
    Millermatic 211
    Dewalt 14" Chopsaw
    Dewalt 4 1/2" Grinder
    Craftsman

  17. #67
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,451
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by 74fencer View Post
    Lots of nice projects, SquirmyPug, What are the threaded studs for?
    Its for a tool we sell called a Knucklemate. Usually the studs are only mig welded from one side, but the customer wants some with smaller pins. The way they are machined left a bit of a gap with the washers we use and one side has a sharp corner/reduced diameter where some material was removed for the smaller diameter. Just had to fill the gap and fill the corner in some so it doesn't lose as much strength compared to normal size. Until we have a large order of them its cheaper to modify pins we have vs having them made like they should be.
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200 (stolen)
    Miller Maxstar 150STL
    Miller AEAD200LE (welding and generating power)
    Hobart MIG

  18. #68
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,918
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by Bipestuff View Post
    Great projects! Has anyone built a welding screen? Typically a steel frame with either heavy canvas or some other type of dark burn resistant material so your welding flash and grinding sparks don't fly out of your work area. I was thinking of building some for my garage shop, need some ideas!
    i re-purposed some discarded privacy screens from the prison hospital and attached a piece of that blue translucent protective stuff they use for weld booths. it's even got wheels so it's very portable. thankfully i'm nowhere near my shop till next week or i'd post a pic.
    i.u.o.e. # 15
    queens, ny and sunny fla

  19. #69
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,032
    Post Thanks / Like

    Re: Show us what you welded today!

    Tis the season for plow repair! This thing today between all my other work.






  20. #70
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,061
    Post Thanks / Like

    Re: Show us what you welded today!

    Got tired of broken ax handles...

    Name:  ax1.jpg
Views: 8707
Size:  44.3 KBName:  ax2.jpg
Views: 8700
Size:  47.3 KB
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  21. #71
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,032
    Post Thanks / Like

    Re: Show us what you welded today!

    I broke the handle on my rubber mallet the other day and have been wondering how to fix it if I even can fix it.

  22. #72
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,061
    Post Thanks / Like

    Re: Show us what you welded today!

    I DID wrap the handles in a good 1/8" of electrical tape... otherwise hitting a knot would ring yer bell...

    I only use them for chopping up kindling wood.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  23. #73
    Join Date
    Dec 2009
    Location
    Sutton, MA
    Posts
    702
    Post Thanks / Like

    Re: Show us what you welded today!

    First welds of the new year.


    Derek G by Zanconato Custom Cycles, on Flickr


    Derek G by Zanconato Custom Cycles, on Flickr


    Derek G by Zanconato Custom Cycles, on Flickr

  24. #74
    Join Date
    Dec 2013
    Posts
    115
    Post Thanks / Like

    Re: Show us what you welded today!

    bought a new miller 211 so I decided to play around with some different settings
    Attached Images Attached Images    

  25. #75
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,061
    Post Thanks / Like

    Re: Show us what you welded today!

    Quote Originally Posted by Casey g View Post
    bought a new miller 211 so I decided to play around with some different settings
    How do you like the Autoset feature?
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments