    My old man rarely gave me compliments and I worked with him every day until he died

    He had high standards and his expectations were that everything was to be done right. (probably from his stint in the army)

    Silence was his form of praise.


    Sent from my iPhone using Tapatalk
    :

  2. Likes Kirtman0405 liked this post
  3. #14677
    Join Date
    Nov 2009
    Location
    Seward, Ak
    Posts
    379
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by IAMsteelworker View Post
    Yeah I'm not sure if it was or not. If it was someone did a decent job hiding it. No evidence of being welded before to the eye.

    Sent from my SM-N950U using Tapatalk
    The piece on the left looks like there is some undercut from another weld, where this break happened

  4. #14678
    Join Date
    Nov 2009
    Location
    Seward, Ak
    Posts
    379
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by ArcTan View Post
    It will make more sense tomorrow. It's an adapter to increase a 6" pole to 8" for a small solar array. The 6" pole is already mounted in concrete I presume, so this will be welded to the top of it to allow an 8" pole mount to be installed.



    Thanks. Unfortunately Go Fund Me hasn't funded a PAPR yet. I wore my regular respirator and kept my head far enough away that the cross breeze took away most of the smoke.
    "Go fund me" The millennial version of the organ grinders monkey, with sunglasses holding a tin cup

  5. #14679
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,266
    Post Thanks / Like

    Re: Show us what you welded today

    Name:  EADB7641-25DA-4A9C-8060-A130C28A85A8.jpg
Views: 493
Size:  70.5 KBwhy I think guys should use core wire at home and you can weld little small stuff with it. .045 core wire at 25 volts and about 300 wire speed. 3/16 plate overhead weld. Usually I run hardwire here but last 2 boxes I ran the core wire. Really tough to run it downhill tho. I’ve learned to long arc it to make it run colder downhill.

  6. Likes whtbaron, Lis2323, ezduzit, Don52 liked this post
  7. #14680
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,342
    Post Thanks / Like

    Re: Show us what you welded today

    Fenders on the welder cart today







    Sent from my iPhone using Tapatalk
    :

  8. #14681
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,779
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Lis2323 View Post
    Fenders on the welder cart today







    Sent from my iPhone using Tapatalk
    You should sell those.

    Very nice.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  9. #14682
    Join Date
    Apr 2016
    Location
    CA
    Posts
    8,922
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by John T View Post
    You should sell those.

    Very nice.
    with all the stuff he has built and sold lately ^ this was my though as to why he is building it.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  10. #14683
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    8,622
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Lis2323 View Post
    Fenders on the welder cart today







    Sent from my iPhone using Tapatalk
    Jeeeesus!!! You got that much free time, I'd put you to work.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  11. Likes whtbaron, LtBadd liked this post
  12. #14684
    Join Date
    May 2022
    Location
    Barbados ����
    Posts
    5
    Post Thanks / Like

    Re: Show us what you welded today!

    Nicee....When I Always Have Problems Cleaning After Welding Up Handrails...Speaking Of Round Bar Though...I Think I Gotta Start My Welds A Different Spot🤦🏾*♂️

  13. #14685
    Join Date
    May 2022
    Location
    Barbados ����
    Posts
    5
    Post Thanks / Like

    Re: Show us what you welded today

    Now That's Clean....How'd You Get Your Measurements?

  14. #14686
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    1,169
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Lis2323 View Post
    Fenders on the welder cart today







    Sent from my iPhone using Tapatalk
    I like it! Have ya thought about a spring loaded latch for that swingy-outy bit? One less thing to drop on the ground and bounce up under the workbench.

    Sent from my Lincoln Buzzbox using Tapatalk

  15. #14687
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,342
    Post Thanks / Like

    Show us what you welded today

    Quote Originally Posted by 52 Ford View Post
    I like it! Have ya thought about a spring loaded latch for that swingy-outy bit? One less thing to drop on the ground and bounce up under the workbench.

    Sent from my Lincoln Buzzbox using Tapatalk
    that was the plan but the only ones I had in my parts room were too big and I didn't feel like going to the store




    so i went full blown farmer fab lol






    Sent from my iPhone using Tapatalk
    :

  16. Likes whtbaron liked this post
  17. #14688
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    1,169
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Lis2323 View Post
    that was the plan but the only ones I had in my parts room were too big and I didn't feel like going to the store




    so i went full blown farmer fab lol






    Sent from my iPhone using Tapatalk
    Nothing wrong with that! I have a bunch of those "hex head pins" kicking around. A lot of them have cross pins made out of bent stick electrodes.

    "It ain't stupid if it works!"

    Sent from my Lincoln Buzzbox using Tapatalk

  18. Likes Lis2323 liked this post
  19. #14689
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,342
    Post Thanks / Like

    Re: Show us what you welded today

    Modified forklift LPG tank clamps for securing my welding cart tanks. Used weld on hinges




    this cart is taking a while. Limiting myself to one part/section a day to prolong the fun


    Sent from my iPad using Tapatalk
    :

  20. #14690
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    502
    Post Thanks / Like

    Re: Show us what you welded today

    That's a really nice cart. An enormous amount of time goes into a nice tricked up cart like that, but once it's done it's there for life and shows off your skills to anyone that comes through your shop. You also see it every day with pride and it can become a family heirloom even. Fitting addition to a well organised shop with top notch tools and gear in it.

  21. Likes N2 Welding, Roert42 liked this post
  22. #14691
    Join Date
    Sep 2020
    Location
    VT
    Posts
    305
    Post Thanks / Like

    Re: Show us what you welded today

    Lis, your work is so nice it makes my project look like junk... Oh wait it actually is

    Name:  PXL_20220525_133414713.MP.jpg
Views: 275
Size:  273.5 KB

    Name:  PXL_20220526_001745710.jpg
Views: 275
Size:  136.8 KB

    Repairing/improving my ripper that I broke last fall.

    https://weldingweb.com/vbb/threads/3...23#post8837323
    Last edited by ArcTan; 4 Weeks Ago at 10:09 PM.
    Glen

    Red-D-Arc EX300 (Miller XMT304)
    Hobart Champion 16
    Hobart Hefty CC/CV
    Hobart Handler 140
    Lotos LTP5000D

  23. Likes ezduzit, motolife313, 52 Ford, albrightree liked this post
  24. #14692
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,342
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by ArcTan View Post
    Lis, your work is so nice it makes my project look like junk... Oh wait it actually is

    Name:  PXL_20220525_133414713.MP.jpg
Views: 275
Size:  273.5 KB

    Name:  PXL_20220526_001745710.jpg
Views: 275
Size:  136.8 KB

    Repairing/improving my ripper that I broke last fall.

    https://weldingweb.com/vbb/threads/3...23#post8837323
    That’s nice work, AT!. I’ve modified lots of loader buckets but never had to do any heavy repairs like that.
    :

  25. #14693
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,342
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Woznme View Post
    That's a really nice cart. An enormous amount of time goes into a nice tricked up cart like that, but once it's done it's there for life and shows off your skills to anyone that comes through your shop. You also see it every day with pride and it can become a family heirloom even. Fitting addition to a well organised shop with top notch tools and gear in it.
    Thank you, Woznme!


    Sent from my iPad using Tapatalk
    :

  26. #14694
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    1,169
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Lis2323 View Post
    Modified forklift LPG tank clamps for securing my welding cart tanks. Used weld on hinges




    this cart is taking a while. Limiting myself to one part/section a day to prolong the fun


    Sent from my iPad using Tapatalk
    I like that clamp setup. A lot better than a piece of chain or a ratchet strap.

    Have you considered a standing platform behind the cylinders and some electric motors on the wheels? That way you can just hop on the cart and drive it around the shop.

    Here I made you a picture

    Sent from my Lincoln Buzzbox using Tapatalk

  27. Likes Roert42, NotaVegetarian, SweetMK liked this post
  28. #14695
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,342
    Post Thanks / Like

    Show us what you welded today

    Quote Originally Posted by 52 Ford View Post
    I like that clamp setup. A lot better than a piece of chain or a ratchet strap.

    Have you considered a standing platform behind the cylinders and some electric motors on the wheels? That way you can just hop on the cart and drive it around the shop.

    Here I made you a picture

    Sent from my Lincoln Buzzbox using Tapatalk


    Seriously though I did try to buy the electric shopping cart retriever used in parking lots when Target closed up shops in Canada. The plan was to use it for moving a welding table.


    Sent from my iPad using Tapatalk
    Last edited by Lis2323; 4 Weeks Ago at 11:44 PM.
    :

  29. Likes 52 Ford, SweetMK liked this post
  30. #14696
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    1,169
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Lis2323 View Post


    Seriously though I did try to buy the electric shopping cart retriever used in parking lots when Target closed up shops in Canada. The plan was to use it for moving a welding table.


    Sent from my iPad using Tapatalk
    Really not a bad idea!

    Naturally, I have a solution for moving the welding table, too.

    Go buy a surplus M274 Mule. Already has a flat deck on it. It's about the right height. Just throw a piece of 1/2" plate on it there any yer good to go!

    Need to level it? Adjust the tire pressure!



    Sent from my Lincoln Buzzbox using Tapatalk

  31. Likes N2 Welding, SweetMK liked this post
  32. #14697
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    1,169
    Post Thanks / Like

    Re: Show us what you welded today

    No spare tire? No problem!

    Sent from my Lincoln Buzzbox using Tapatalk

  33. Likes N2 Welding, NotaVegetarian liked this post
  34. #14698
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    7,342
    Post Thanks / Like

    Re: Show us what you welded today

    Pretty cool. I’ve never seen one before. I LIKE it!


    Sent from my iPad using Tapatalk
    :

  35. Likes 52 Ford liked this post
  36. #14699
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    3,248
    Post Thanks / Like

    Re: Show us what you welded today

    I like the cart, perfect job to do a piece at a time. Time makes for great finish and paint.

  37. #14700
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    3,248
    Post Thanks / Like

    Re: Show us what you welded today

    I built a few things we sand, tape the welding joints and prime before assembly. Spatter doesnt stick, easy to resand and prime again. Not that it matters in the case of shop equipment, most paint looks and lasts but where we using epox primers, usually an industrial grade to reduce the cost they can mottle a little etc, doesnt hurt on most equipment but show piece or car truck finish we scotchbrite a little between coats. They blame it on thje paint sometimes when its really the primer. I got a bunch of equipment paint tricks and paint follows welding. Its what is seen in the end.
    You should be shipping that stuff somewhere to a "collector: crowd, you have good design, useful art. Benches should be in a "gallery"

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,656,332,359.71614 seconds with 15 queries