Page 609 of 614 FirstFirst ... 109509559599607608609610611 ... LastLast
Results 15,201 to 15,225 of 15334

Thread: Show us what you welded today

  1. #15201
    Join Date
    Sep 2015
    Location
    West coast of Florida
    Posts
    589
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Sberry View Post
    Everyone knows what gorilla welds are?
    Ugly but strong
    Richard
    West coast of Florida

  2. #15202
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,835
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by LtBadd View Post
    Ugly but strong
    That seems to be the theme with folks on The Forum.

    Sent from my Lincoln Buzzbox using Tapatalk

  3. #15203
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    8,425
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by 52 Ford View Post
    That seems to be the theme with folks on The Forum.

    Sent from my Lincoln Buzzbox using Tapatalk
    speak for yourself, please
    :

  4. Likes 12V71, whtbaron, 52 Ford, xmmancharl, shortarc liked this post
  5. #15204
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    8,069
    Post Thanks / Like

    Re: Show us what you welded today

    Yea.... probably not that strong anymore....
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  6. Likes N2 Welding liked this post
  7. #15205
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    4,222
    Post Thanks / Like

    Re: Show us what you welded today

    I got some that have much better appearance, those were simply showing how to heater up. Guy can get distracted with personal lessons.
    Attached Images Attached Images     

  8. Likes xmmancharl liked this post
  9. #15206
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,786
    Post Thanks / Like

    Re: Show us what you welded today

    It is a good weld.

    Dave

    Quote Originally Posted by Sberry View Post
    I got some that have much better appearance, those were simply showing how to heater up. Guy can get distracted with personal lessons.

  10. #15207
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    4,222
    Post Thanks / Like

    Re: Show us what you welded today

    Found these 2 pieces I had made for temp deal 30 yrs ago, maybe more. At the time we never considered a grinder or any way to do this but a torch. Wanted a 3/4 draw pin and 7/8 hole. Well 13/16 . Today had to really look after some time and weather to see this all hand cut in couple minutes, only finish was chipping hammer.
    Attached Images Attached Images   

  11. #15208
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,835
    Post Thanks / Like

    Re: Show us what you welded today

    I just really got into using magnets for positioning. I almost always use clamps and squares.

    Well, I learned something... actually 2 things... that black layer between the two pieces of steel on a welding magnet is PLASTIC (rubber?). Also, the fumes from that black layer burning are enough to really screw up a weld.

    Sent from my Lincoln Buzzbox using Tapatalk

  12. #15209
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,441
    Post Thanks / Like

    Re: Show us what you welded today

    Can’t get it that close to the weld or it will pull the wire into the magnet. I’m surprised you got the magnet to that point

  13. Likes xmmancharl liked this post
  14. #15210
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,835
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by motolife313 View Post
    Canít get it that close to the weld or it will pull the wire into the magnet. Iím surprised you got the magnet to that point
    Stick welding - if the magnet is big enough to bend a 6011, I'd be afraid to be near it. Plus, I was welding a corner joint on pretty thin metal. I DID notice a bit of funky arc blow and I do know that was from the magnet, I expected that.

    I never considered that it'd pull welding wire around, though. That's really interesting! I might have to try that... probably been 2 years since I plugged in the MIG... maybe a year and a half. Total, I probably have 20 hours on a MIG machine couldn't count the hours on a stick machine. I just never took the time to get proficient with wire welding.

    Like I said, I never really used magnets before. Just decided I'd try something different. I didn't expect I'd have to learn how to use a freakin magnet. LOL

    Sent from my Lincoln Buzzbox using Tapatalk

  15. #15211
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,441
    Post Thanks / Like

    Re: Show us what you welded today

    I used to have a problem even getting a tack on with mig at my last job, if the magnet was too close. You were hear the metal undercut from the wire getting dragged a crossed it too fast towards the magnet. I’m surprised you stick weld if u got a mig. I got a lot to learn with stick, I was just thinking about firing one of mine up yesterday, I got 3 stick welders

  16. #15212
    Join Date
    Jan 2004
    Location
    Brethren, Mi
    Posts
    4,222
    Post Thanks / Like

    Re: Show us what you welded today

    For a real career welder wants to move around good stick skills are outstanding. Same for use of a torch.

  17. Likes motolife313, xmmancharl, 52 Ford liked this post
  18. #15213
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,835
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by motolife313 View Post
    I used to have a problem even getting a tack on with mig at my last job, if the magnet was too close. You were hear the metal undercut from the wire getting dragged a crossed it too fast towards the magnet. Iím surprised you stick weld if u got a mig. I got a lot to learn with stick, I was just thinking about firing one of mine up yesterday, I got 3 stick welders
    I was tought to stick weld when I was really young. Just seems easier to me. Once you get your technique down, welding 16 gauge or thinner isn't a problem.

    I didn't realize how out of practice I am till a few days ago when I was welding some 14 gauge. 2 or 3 years ago, I was welding up 16 gauge exhaust pipe without an issue. Just 3/32 6010 and 6011. I started with the wire welder, then decided I was better off with the stick machine LOL

    I've just never taken the time to REALLY learn MIG.

    Sent from my Lincoln Buzzbox using Tapatalk

  19. #15214
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,062
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by motolife313 View Post
    I got a lot to learn with stick, I was just thinking about firing one of mine up yesterday, I got 3 stick welders
    Drag it outside on a nice day and burn some rod. nothing more satisfying than seeing a 4" caterpillar of 7018 slag curling up off a hot weld bead.

    I need to fire up my old Idealarc also.... love that machine.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  20. Likes ArcTan, IAMsteelworker, whtbaron liked this post
  21. #15215
    Join Date
    Feb 2015
    Location
    Texas
    Posts
    328
    Post Thanks / Like

    Re: Show us what you welded today

    Welding up these display bases and after a dozen or so get burned out on the squirt gun and decided to play around with some aluminum. Butt welded these pieces with 4043 and put in the vise to check the quality. I make a lot of steel stars but the aluminum ones are more fun and lots of practice. Pieces are .125 6061 and welded with 4043.

    Name:  357EDE7F-600C-4D07-AA33-C74F411C8052.jpg
Views: 721
Size:  91.9 KB

    Name:  34578E3E-CF06-4DEA-9F54-0FCE7615DB8B.jpg
Views: 713
Size:  134.4 KB

    Name:  4ECEA0E5-F9B2-4484-B22A-9F5033CBA636.jpg
Views: 719
Size:  109.6 KB

    Name:  000BCFCE-7769-43CC-B511-3F5B78D76A32.jpg
Views: 727
Size:  94.1 KB
    Miller 350 Dynasty
    Miller Trailblazer
    Miller 625 Plasma
    Died and needs a new circuit board so its an expensive boat anchor now
    Lincoln Power MIG
    Victor oxy/acetylene
    Hyperthem 85

  22. #15216
    Join Date
    Jun 2016
    Posts
    857
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by BluCllrPlt View Post
    Welding up these display bases and after a dozen or so get burned out on the squirt gun and decided to play around with some aluminum. Butt welded these pieces with 4043 and put in the vise to check the quality. I make a lot of steel stars but the aluminum ones are more fun and lots of practice. Pieces are .125 6061 and welded with 4043.

    Name:  357EDE7F-600C-4D07-AA33-C74F411C8052.jpg
Views: 721
Size:  91.9 KB




    Name:  34578E3E-CF06-4DEA-9F54-0FCE7615DB8B.jpg
Views: 713
Size:  134.4 KB

    Name:  4ECEA0E5-F9B2-4484-B22A-9F5033CBA636.jpg
Views: 719
Size:  109.6 KB

    Name:  000BCFCE-7769-43CC-B511-3F5B78D76A32.jpg
Views: 727
Size:  94.1 KB

    nicE trick bending the aluminum first and then tig welding back together in the vice!!! LOL
    lincoln 125sp
    dayton 250 ac/dc
    miller 211 w/spool gun
    ahp 200 sx tig
    lotos ltp5000d
    kubota b3200 FEL BH
    of course duramax diesel

  23. Likes 52 Ford, LtBadd liked this post
  24. #15217
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    6,693
    Post Thanks / Like

    Re: Show us what you welded today

    First job in 2 weeks that required welding, Had a Cat C15 in yesterday with 4 broken exhaust manifold studs. Used the wirefeed to build up the broken stud and then welded a nut to the nub. All of them were broken off 1/2 a thread in.
    Name:  20220819_060900.jpg
Views: 567
Size:  95.0 KBName:  20220819_060918.jpg
Views: 569
Size:  67.8 KBName:  20220819_061031.jpg
Views: 569
Size:  122.4 KB

  25. #15218
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    9,004
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by 12V71 View Post
    First job in 2 weeks that required welding, Had a Cat C15 in yesterday with 4 broken exhaust manifold studs. Used the wirefeed to build up the broken stud and then welded a nut to the nub. All of them were broken off 1/2 a thread in.
    Name:  20220819_060900.jpg
Views: 567
Size:  95.0 KBName:  20220819_060918.jpg
Views: 569
Size:  67.8 KBName:  20220819_061031.jpg
Views: 569
Size:  122.4 KB
    And the victory is sweet!
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  26. Likes 12V71, labparamour, 52 Ford liked this post
  27. #15219
    Join Date
    Apr 2016
    Location
    CA
    Posts
    9,576
    Post Thanks / Like

    Re: Show us what you welded today

    took me a couple weeks to complete but it's done and drying now. Explorer Seat Bracket to Bronco floor board.

    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  28. #15220
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    608
    Post Thanks / Like

    Re: Show us what you welded today

    Gettin' some roots dye pen tested

  29. #15221
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    2,835
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by N2 Welding View Post
    took me a couple weeks to complete but it's done and drying now. Explorer Seat Bracket to Bronco floor board.

    Nice. How long are you gonna let those welds dry for?

    Sent from my Lincoln Buzzbox using Tapatalk

  30. #15222
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    7,786
    Post Thanks / Like

    Re: Show us what you welded today

    Like the dye pen test.

    Dave

    Quote Originally Posted by Woznme View Post
    Gettin' some roots dye pen tested

  31. #15223
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    10,441
    Post Thanks / Like

    Re: Show us what you welded today

    Uphill 1/4Ē weld from today. We donít weld uphill often. The last time was probably the last pic I posted hereName:  76CF5F8C-ACE9-4DBA-BFD4-4D41A8B7D57F.jpg
Views: 319
Size:  92.9 KB

  32. #15224
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    608
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by Woznme View Post
    Gettin' some roots dye pen tested
    Caps dye pen tested. All good.

  33. Likes whtbaron, LtBadd, Lis2323 liked this post
  34. #15225
    Join Date
    Apr 2016
    Location
    CA
    Posts
    9,576
    Post Thanks / Like

    Re: Show us what you welded today

    Quote Originally Posted by 52 Ford View Post
    Nice. How long are you gonna let those welds dry for?

    Sent from my Lincoln Buzzbox using Tapatalk
    plenty dry by now. its already been bolted up for a few days now.

    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  35. Likes 52 Ford liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,876,627.44838 seconds with 15 queries