Re: Mod-Your-151 How-To Guide
Does that new pancake (muffin) fan put out more CFM of air than the original bladed type fan? That seems counter-intuitive to me. I have upgraded several HF mig boxes that came with NO FAN at all, and the fans I have put in actually look like the one you took out at the first part of your project. Nothing in my opinion makes things live longer than keeping them cool. Good job by the way on the descriptions and photos. I love seeing projects like this.
Miller Syncrowave 350
Millermatic 252/ 30A spoolgun
Miller Bobcat 225g w/ 3545 spoolgun
Lincoln PowerArc4000
Lincoln 175 Mig
Lincoln 135 Mig
Everlast 250EX Tig
Century ac/dc 230 amp stick
Victor O/A
Hypertherm 1000 plasma