    SS pressure pipe ticket

    On Tuesday I passed my pressure pipe stainless 6G tig weld test with the TSSA. Love that feeling.
    The test was 2" sch 60 316 SS pipe tig welded in 6G, uphill only.
    Visual root and cap inspections were done along with 2 root and 2 face bends.
    Machine I used was a Miller syncrowave 250 on 575v 3 phase power.
    Last edited by snoeproe; 09-12-2009 at 11:44 PM.