    childrens snowmobile

    This is a '92 Arctic Cat kitty cat childrens snowmobile that I am refurbishing. The chassis is getting some weld repairs.
    The thin steel belly pan and bulkhead had several cracks that needed to be repaired. All tig welds, 50 amps, Most of the filler is Esab spoolarc 65 (ER70S-2).



    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  2. #2
    Join Date
    Aug 2008
    Location
    Dansville NY
    Posts
    5,141
    Post Thanks / Like

    Re: childrens snowmobile

    Wow !! I guess It did need some repairs to make it safe for the kids to ride on it.
    Co-Own CNC shop:Miller :1251 plasma cutter, MaxStar 700 TIG/Stick, & XMT 456 Multiprocess Welder.& 2 Hypertherm HPR260's Plasma Cutter

    Sorry I had a bad stroke but now I am back.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,628,150,538.51703 seconds with 11 queries