    2" 316L SS sch 60, 6G.

    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  2. #2
    Join Date
    Mar 2009
    Location
    upland, ca
    Posts
    1,102
    Post Thanks / Like

    Re: SS 316L 6G pipe Tig welded

    looks just a-boat right, eh? nice job

  3. #3
    Join Date
    Aug 2009
    Posts
    178
    Post Thanks / Like

    Re: SS 316L 6G pipe Tig welded

    Looks good, nice job
    keith
    The older the boys, the more expensive the TOYS!!
    Previous owned;
    Linde 300 Amp welder
    Miller Gas drv welder, Tumbstone,Dayton
    Miller ac to dc converter,High frequency unit
    Longevity LS60P
    Currrently owned;
    Longevity WeldAll 200PI

  4. #4
    Join Date
    Feb 2009
    Location
    El Paso, TX
    Posts
    41
    Post Thanks / Like

    Re: SS 316L 6G pipe Tig welded

    personally i would have a tighter smoother weave, but it still looks good!

  5. #5
    Join Date
    Nov 2008
    Posts
    607
    Post Thanks / Like

    Re: SS 316L 6G pipe Tig welded

    try stick for your filler/cap pass's works very nice once you get the hang of it. Also stick roots are a very useful skill to learn, no purge! not to mention the cashola you can make holding a ticket such as this.

  6. #6
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    3,461
    Post Thanks / Like

    Re: SS 316L 6G pipe Tig welded

    This was the last practice piece I welded the evening before I passed my stainless pipe tig test. No stick was allowed for that test, it was tig all the way out. I did manage to tighten up my weave/puddles a bit more for the test, that was needed for sure.
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,628,147,088.13367 seconds with 11 queries