    Saw this on another site. Couldn't help but share it...
    Name:  Trailer hitch.jpg
Views: 6269
Size:  25.4 KB

  2. #102
    Join Date
    Jul 2013
    Location
    La Porte, TX
    Posts
    3,676
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Canadian Welding View Post
    Saw this on another site. Couldn't help but share it...
    Name:  Trailer hitch.jpg
Views: 6269
Size:  25.4 KB
    Mind if I steal the idea for my 97 Olds?
    Gravel

    The difference between theory and practice is that in theory there is no difference.

  3. #103
    Join Date
    Jul 2011
    Location
    Bossier Parish La.
    Posts
    5,845
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Canadian Welding View Post
    Saw this on another site. Couldn't help but share it...
    Name:  Trailer hitch.jpg
Views: 6269
Size:  25.4 KB
    Isn't that called a Red Neck, Goose Neck hitch? What trailer weight rating is it good for? Ought to be good for at least 12,000 Lbs.

  4. #104
    Join Date
    Dec 2013
    Location
    Canada
    Posts
    798
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Bistineau View Post
    Isn't that called a Red Neck, Goose Neck hitch? What trailer weight rating is it good for? Ought to be good for at least 12,000 Lbs.
    Aw ya. 12000 easy. Throw some hockey pucks in there for a bump stop and you will have 30000 EASY!

  5. #105
    Join Date
    Dec 2013
    Location
    Canada
    Posts
    798
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Gravel View Post
    Mind if I steal the idea for my 97 Olds?
    Go ahead. I am now installing them on civics as well!

  6. #106
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,402
    Post Thanks / Like

    Re: Trailer fail pics

    This is still my fav

    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  7. Likes Garfield43 liked this post
  8. #107
    Join Date
    Dec 2013
    Location
    near dayton ohio
    Posts
    589
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Canadian Welding View Post
    Saw this on another site. Couldn't help but share it...
    Name:  Trailer hitch.jpg
Views: 6269
Size:  25.4 KB

    I saw one of these on a Cadillac coup deville once. the guy pulled a skid loader and hay bales on a dove tail gooseneck trailer. atleast he did have a brake controller in it too.
    Lincoln 225 ac (my first machine)
    farmhand 115vac 70amp mig/fc toy
    miller aead 200le (my main machine)

  9. #108
    Join Date
    Apr 2014
    Location
    California
    Posts
    112
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Canadian Welding View Post
    Saw this on another site. Couldn't help but share it...
    Name:  Trailer hitch.jpg
Views: 6269
Size:  25.4 KB
    Yikes!

  10. #109
    Join Date
    Dec 2013
    Location
    near dayton ohio
    Posts
    589
    Post Thanks / Like

    Re: Trailer fail pics

    the one I saw was attached to the frame through the trunk and had a guard between the ball and the window.
    Lincoln 225 ac (my first machine)
    farmhand 115vac 70amp mig/fc toy
    miller aead 200le (my main machine)

  11. #110
    Join Date
    Sep 2009
    Posts
    69
    Post Thanks / Like

    Re: Trailer fail pics

    Name:  IMG_0747.jpg
Views: 5239
Size:  65.7 KB
    I saw this one on the way home last night. I didn't want to stay behind it to get a better picture.

  12. #111
    Join Date
    Sep 2009
    Posts
    69
    Post Thanks / Like

    Re: Trailer fail pics

    Sorry don't know how to rotate the picture

  13. #112
    Join Date
    Jul 2013
    Location
    La Porte, TX
    Posts
    3,676
    Post Thanks / Like

    Re: Trailer fail pics

    Name:  IMG_0747.jpg
Views: 5259
Size:  112.3 KB

    Won't hurt a bit if it hits your grill.
    Gravel

    The difference between theory and practice is that in theory there is no difference.

  14. #113
    Join Date
    Sep 2009
    Posts
    69
    Post Thanks / Like

    Re: Trailer fail pics

    I should mention the gate was in the trailer because it broke off and took the rear cross member of the trailer with it. Those boards were waving at people, and the side were flexing all over the place on every bump. The lights weren't working either, but that is pretty common around here.

  15. #114
    Join Date
    Sep 2013
    Location
    west texas
    Posts
    2,372
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Michgriz View Post
    The lights weren't working either, but that is pretty common around here.
    What state is that?
    old Miller spectrum 625
    Lincoln SP-135 T, CO2+0.025 wire
    Miller model 250 and WP-18V torch
    Craftsman 100amp AC/DC and WP-17V torch
    Century 115-004 HF arc stabilizer
    Home made 4 transformer spot welder
    Home made alternator welder

  16. #115
    Join Date
    Sep 2009
    Posts
    69
    Post Thanks / Like

    Re: Trailer fail pics

    Michigan, I would say about half the trailers I see don't have working lights. I think there is something about if you can see the tow vehicle lights you don't need them or something like that. My trailers get checked out before every trip and don't leave unless all lights are working.

  17. #116
    Join Date
    Sep 2013
    Location
    west texas
    Posts
    2,372
    Post Thanks / Like

    Re: Trailer fail pics

    Thats too bad.
    I would say most of the new trailers have working lights. Most of the old ones dont.
    Problem is most of the trailers around here are real odd.

    Most trailer light problems are caused by bad ground, where they connect the wire to the frame. I think that is idiotic unless you can some how avoid ever coming in contact with liquid water.
    Its not really not that hard to put all the lights on a ground wire and use all weather proof connectors.
    If you do that you wont have a light problem till a bulb burns out or you let some one barrow your trailer and they break a light or 2 off.

    I replaced the lights with LEDs on my trailer and put everything on a ground wire with sealed connectors in 2008 and I may have replaced a flat 4 connector since then.
    old Miller spectrum 625
    Lincoln SP-135 T, CO2+0.025 wire
    Miller model 250 and WP-18V torch
    Craftsman 100amp AC/DC and WP-17V torch
    Century 115-004 HF arc stabilizer
    Home made 4 transformer spot welder
    Home made alternator welder

  18. #117
    Join Date
    Mar 2014
    Posts
    127
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Canadian Welding View Post
    Saw this on another site. Couldn't help but share it...
    Name:  Trailer hitch.jpg
Views: 6269
Size:  25.4 KB
    Nifty idea. I should add one of those to my 1992 Chevy Silverado 1/2 ton pickups hood. No really I should as a hood ornament.

    Course I wouldn't actually use it to move a trailer.

    Chad

  19. #118
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by MinnesotaDave View Post
    This is still my fav

    I remember seeing something like that when I was a kid...ohh..the campgrounds we went to.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  20. #119
    Join Date
    May 2012
    Location
    Ontario, Canada
    Posts
    1,505
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Canadian Welding View Post
    Saw this on another site. Couldn't help but share it...
    Name:  Trailer hitch.jpg
Views: 6269
Size:  25.4 KB
    Well hell, we've seen this photo six times already, let's go for 7

  21. #120
    Join Date
    Dec 2013
    Location
    Canada
    Posts
    798
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by Chad22 View Post
    Nifty idea. I should add one of those to my 1992 Chevy Silverado 1/2 ton pickups hood. No really I should as a hood ornament.

    Course I wouldn't actually use it to move a trailer.

    Chad
    Haha, that would be great!

  22. #121
    Join Date
    Dec 2012
    Location
    Woodstock, Ga
    Posts
    606
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by toofast_28 View Post
    Attachment 699801
    Maybe this isn't a total fail, but a buddy picked this up at auction for $100 and wanted me to fix it. It's getting scrapped. From the best we can tell it got rear ended. Still rolls though. Probably salvage the axle.


    Lights still good LOL
    Magazines have issues, everything else has problems

  23. #122
    Join Date
    Dec 2012
    Location
    Woodstock, Ga
    Posts
    606
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by MinnesotaDave View Post
    This is still my fav

    Just goes to show ya, one really cannot make a VW look any worse that the manufacture .
    Magazines have issues, everything else has problems

  24. #123
    Join Date
    Sep 2009
    Posts
    69
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by 7A749 View Post
    I almost thought I recognized that truck.

    Anywhere near the Lansing area?
    Could be, I work on the NE side of Grand Rapids. It was heading North toward Rockford.

  25. #124
    Join Date
    Sep 2013
    Location
    west texas
    Posts
    2,372
    Post Thanks / Like

    Re: Trailer fail pics

    One coming out of the scrap yard.
    Attached Images Attached Images   
    old Miller spectrum 625
    Lincoln SP-135 T, CO2+0.025 wire
    Miller model 250 and WP-18V torch
    Craftsman 100amp AC/DC and WP-17V torch
    Century 115-004 HF arc stabilizer
    Home made 4 transformer spot welder
    Home made alternator welder

  26. #125
    Join Date
    Dec 2013
    Location
    Canada
    Posts
    798
    Post Thanks / Like

    Re: Trailer fail pics

    Quote Originally Posted by mad welder 4 View Post
    One coming out of the scrap yard.
    It shoulda stayed in there.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,271,180.66939 seconds with 20 queries