    National torch tip info

    I just bought a partial torch kit from a pawn shop for 40.00. It is an older Victor torch and regulators but came with quite a few National brand tips for it. 3 extra cutting tips and 5 heating/brazing/welding tips. It also appears there is an adapter to attach the non cutting tips to the torch since it is not a 2 piece torch. I was wandering if anyone was familiar with that brand and what they maybe used for? Some have quite large holes in them, much much larger than the size tip we use at school to braze copper with.(I'm a current HVAC student) The cutting tips are marked AA1,AA2 and AA6 and the non cutting tips are marked P2,P6,P5,and 9.

  2. #2
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,823
    Post Thanks / Like

    Re: National torch tip info

    I don't know about that model but I have a SMITH cutting head and it came with a ROSEBUD [ heating tip ] that fits in the cutting head which is the same dimensions as the cutting tip. It's not like a real rosebud but works. Set your torch up and light up each tip to see what you have.

  3. #3
    Join Date
    Mar 2014
    Posts
    2
    Post Thanks / Like

    Re: National torch tip info

    I guess I will set my torch up when I get some oxygen and acetylene. Now another question is, my torch only has a knob for the gas side and a knob at the top i'm guessing that controls the oxygen. Is that normal?

  4. #4
    Join Date
    Sep 2011
    Posts
    115
    Post Thanks / Like

    Re: National torch tip info

    I used National torches extensively in the early 80's, and still have one. That was oxy/propane and oxy/hydrogen for scientific glassblowing.
    Miller XMT304 CC/CV
    Bernard TIG cooler
    SSC foot pedal

    "It's a poor craftsman who blames his tewls toles TOOLS" (!^$#% keyboard)

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,794,455.04834 seconds with 11 queries