    My diy tig torch cooler

    She's finally finished.

    Some specs...

    3.5 gallon 16 guage stainless tank
    45 psi shureflow pump 12v. #8005-292-139
    125cfm fan. 12v and way overkill. But it's what I had.
    850 watt computer power supply. Again, what I had.
    9x12 aux radiator from ebay. $50.
    16x24 aluminium base. 12 gauge.

    Finished product:

    Name:  uploadfromtaptalk1406412368839.jpg
Views: 3271
Size:  73.8 KB
    Attached Images Attached Images   

  2. #2
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Some of the build highlights...

    Name:  uploadfromtaptalk1406412636793.jpg
Views: 3239
Size:  60.7 KB
    Attached Images Attached Images   

  3. #3
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    And...
    Attached Images Attached Images     

  4. #4
    Join Date
    Apr 2014
    Location
    Greensboro, North Carolina, United States
    Posts
    594
    Post Thanks / Like

    Re: My diy tig torch cooler

    That's really cool Robert, a nice use of "stuff I had lying around". What would you say it cost you to build? not including labor of course.
    Thermal arc 211i
    Ck flex-loc 150 & 130
    Clamps, saws & grinders
    Harbor freight 80 amp inverter

  5. #5
    Join Date
    Nov 2010
    Location
    Texas
    Posts
    580
    Post Thanks / Like

    Re: My diy tig torch cooler

    Man that looks good Robert! Maybe I should say "cool"!!!!!

  6. #6
    Join Date
    Jun 2011
    Location
    Aiken SC area
    Posts
    1,192
    Post Thanks / Like

    Re: My diy tig torch cooler

    Mount an indoor/outdoor thermometer on it, drop the outdoor probe through the fill cap (small hole big enough for the probe to fit through and bango, instant temperature indicator. I think you will be surprised at how little the coolant temperature rises with all that cooling apparatus you have there. Nice job! Best Bob

  7. #7
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,862
    Post Thanks / Like

    Re: My diy tig torch cooler

    Nice job!

    Building coolers is fun!
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  8. #8
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by Austin Bennett View Post
    That's really cool Robert, a nice use of "stuff I had lying around". What would you say it cost you to build? not including labor of course.

    Thanks Austin,

    I think I have around $225 in to it with materials, and shop crap in to it. I did buy the stainless bungs, the radiator, and the pump. I had the stainless and aluminum.

  9. #9
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by rhunt View Post
    Mount an indoor/outdoor thermometer on it, drop the outdoor probe through the fill cap (small hole big enough for the probe to fit through and bango, instant temperature indicator. I think you will be surprised at how little the coolant temperature rises with all that cooling apparatus you have there. Nice job! Best Bob

    Interesting thought. I have a pressure gauge and it may mount in the bottom of the switch panel. Right now I want to glue some big metal.

  10. #10
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    And thank you, Kuzineddie, Shovelon, Steve. The praise is much appreciated.

  11. #11
    Join Date
    Jul 2011
    Location
    Utah
    Posts
    2,190
    Post Thanks / Like

    Re: My diy tig torch cooler

    You really need an air trap on the outlet to act as a pulsation damper. Positive displacement pumps like these diaphragm ones make some pretty crazy vibration in the torch lines. Before I put one on mine it drove me crazy cuz the torch would vibrate.
    Are you just running the internal pressure switch to regulate the pressure? Does it cycle on and off like every second? Try running it off the 5v tap on your power supply (or even 3.3v), you may get better performance.
    Last edited by MikeGyver; 07-27-2014 at 03:15 AM.
    Welding/Fab Pics: www.UtahWeld.com

  12. #12
    Join Date
    Jul 2011
    Location
    Long Island, Socialist Republic of NY
    Posts
    2,900
    Post Thanks / Like

    Re: My diy tig torch cooler

    Robert,

    That looks great. Great job. How big is it? Tough to get perspective.

    That's one crazy a$$ piece of copper block you got there.

  13. #13
    Join Date
    Dec 2013
    Posts
    462
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by MikeGyver View Post
    You really need an air trap on the outlet to act as a pulsation damper. Positive displacement pumps like these diaphragm ones make some pretty crazy vibration in the torch lines. Before I put one on mine it drove me crazy cuz the torch would vibrate.
    Are you just running the internal pressure switch to regulate the pressure? Does it cycle on and off like every second? Try running it off the 5v tap on your power supply (or even 3.3v), you may get better performance.
    Love it.

    Yes the trap is the bees knees. They are like $7 at home depot. The small 1/2" diameter one works fine like MG mounted it. And the little filters are on McMaster for not much money. I run a 3/8" line into the pump to avoid any starvation from the filter (bigger inline filter).

    A fan shroud would trick it out (and make the cooling a bunch more efficient if that matters). But you know that.

    The tank is awesome.

    Did you gouge those bend lines with a skill saw or something? Just curious.

    Thanks for posting. I love looking at different solutions to this problem.

  14. #14
    Join Date
    Apr 2010
    Location
    The Peoples Republic of Kalifornia
    Posts
    3,239
    Post Thanks / Like

    Re: My diy tig torch cooler

    Nice work Robert
    Backed my CATMA over your CARMA oops clusmy me

    What would SATAN do ??


    Miller Trailblazer 302 AirPak
    Miller Digital Elite
    Optrel Welding Hat
    Arcair K4000
    Suitcase 12RC / 12 VS
    Hypertherm PM-45
    Rage 3 saw
    Rusty old Truck

  15. #15
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by MikeGyver View Post
    You really need an air trap on the outlet to act as a pulsation damper. Positive displacement pumps like these diaphragm ones make some pretty crazy vibration in the torch lines. Before I put one on mine it drove me crazy cuz the torch would vibrate.
    Are you just running the internal pressure switch to regulate the pressure? Does it cycle on and off like every second? Try running it off the 5v tap on your power supply (or even 3.3v), you may get better performance.
    I think I saw the one you did, Mike. Did that work well for you?

    Thanks for the tip. Ill look into that for sure bud.

  16. #16
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by Drf255 View Post
    Robert,

    That looks great. Great job. How big is it? Tough to get perspective.

    That's one crazy a$$ piece of copper block you got there.
    Crazy a$$$$$$ is right. I had to sell my left n#+ for that, but it's +I+s.

    The tank is 12x12x6 and the base is 16x24.

  17. #17
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,835
    Post Thanks / Like

    Re: My diy tig torch cooler

    I dig it - nice work!

    i like the copper lines instead of rubber - looks cleaner
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  18. #18
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by atg View Post
    Love it.

    Yes the trap is the bees knees. They are like $7 at home depot. The small 1/2" diameter one works fine like MG mounted it. And the little filters are on McMaster for not much money. I run a 3/8" line into the pump to avoid any starvation from the filter (bigger inline filter).

    A fan shroud would trick it out (and make the cooling a bunch more efficient if that matters). But you know that.

    The tank is awesome.

    Did you gouge those bend lines with a skill saw or something? Just curious.

    Thanks for posting. I love looking at different solutions to this problem.
    I scored the lines with a table saw cutting about 60% through. The al won't take more than one bend but it's pretty stiff. I used that on all the 90 bends. Gives a real sharp 90 bend.

    The fan I have on out is 125 cfm and the fan itself is a 5" fan but sounds like a jet prop.

  19. #19
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by killdozerd11 View Post
    Nice work Robert
    Thx kd.

  20. #20
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by MinnesotaDave View Post
    I dig it - nice work!

    i like the copper lines instead of rubber - looks cleaner
    Thanks Dave. I wanted a more traditional look. In another life I was a pipe fitter. 8-)

  21. #21
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Quote Originally Posted by MikeGyver View Post
    Are you just running the internal pressure switch to regulate the pressure? Does it cycle on and off like every second? Try running it off the 5v tap on your power supply (or even 3.3v), you may get better performance.

    Running of 12v. Yes using the internal switch. It seems to be running smooth, but I'll give it a closer look.

    Again, thanks for the tips.

  22. #22
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,918
    Post Thanks / Like

    Re: My diy tig torch cooler

    good job bob. i probably could do the welding but never in a month of sundays could i assemble those components and come up with something that actually works.
    i.u.o.e. # 15
    queens, ny and sunny fla

  23. #23
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    Ha! I doubt that Doc.

    Regardless, thanks.

  24. #24
    Join Date
    Dec 2010
    Location
    Utah
    Posts
    2,071
    Post Thanks / Like

    Re: My diy tig torch cooler

    So, Mike, you were right about the duty cycle being messed up. It took a minute or two for me to notice it. I just bypassed the switch and let it run. It runs great.

    I think on the one hand you might overwork the pump if it has a blockage or something, on the other hand, using a lower voltage on a motor is hard on them too.

    Damned if you do Damned if you dont.

    And the vibration in the line is so slight I dont even notice it.

    Thanks again for the tips.

  25. #25
    Join Date
    Mar 2013
    Posts
    25
    Post Thanks / Like

    Re: My diy tig torch cooler

    My shurflo diaphragm pump gave out after about 2hrs of use. I should have looked more closely at the duty cycle before buying. Got hot as balls and quit.

    It was an 8000 something, direct wire with the pressure switch.

    Just a tip.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,628,046,019.15004 seconds with 14 queries