    Please help, I can not figure a way to weld the flanges in my offset smoker doors with out the corners being sprung out. Not sure if it is when in cutting the doors out or welding the flanges on. I will take any advise anyone has. How can fix the doors now that the corners have sprung out. I'm looking for the tightest fit possible. 1/4 in hot rolled steel pipe, hypotherm plasma, hobart 140 mig, oxy/acetylene torch, are the tools I have plus anything I can buy to fix this problem.

  2. #2
    Join Date
    Jan 2013
    Location
    ...Shoulder of Orion...
    Posts
    3,509
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    Consult the sketches posted in thread # 5 of 13 of http://www.smokingmeatforums.com/t/5...r-smoker-doors.
    The diagrams will show you how to layout the main chamber opening and explain the cut/weld sequence for proper fitup & distortion control.

    Not a smoker pro fabricator, but currently preparing a design/build.
    Many welders here have fabricated some impressive smokers. They should be able to get you back on track and recover from your sprung geometry. Also, be sure to access the smoker build thread on the forum for additional insight.

    Best fortune with your smoker build.
    Last edited by ManoKai; 08-20-2014 at 05:19 AM.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  3. #3
    Join Date
    Dec 2013
    Location
    Hawaii
    Posts
    150
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    Also, check out the smoker build thread started by amusik. I think post #11,#12,#14 should fix you right up.

  4. #4
    Join Date
    Jun 2014
    Location
    DFW, Texas
    Posts
    75
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    Quote Originally Posted by golfingweldor View Post
    Also, check out the smoker build thread started by amusik. I think post #11,#12,#14 should fix you right up.
    Name:  uploadfromtaptalk1408570092657.jpg
Views: 724
Size:  27.7 KB

    Thats what I did to the back side of my door. Mine was 3/8" so you shouldn't need that much heat. Do one line and let it sit overnight.
    For the trim, I tack it every 6" and then fill in 6"-8" on each side of the door each day until its done. I also spot/tack weld it instead of running a solid bead. Looks a little cooler and keeps the heat lower.

    Now I have to update that thread tonight...been slacking

  5. #5
    Join Date
    Aug 2012
    Location
    AR
    Posts
    2,069
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    amusick, when you ran the diagonal beads to take out the warp, did you grind them flat afterwards? Or would that bring the warping back? I would suppose that if you did grind them, you would not let grinding heat build up and complicate things.

  6. #6
    Join Date
    Jun 2014
    Location
    DFW, Texas
    Posts
    75
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    I did grind them flat.

    The welds themselves are not what brings it back into shape, just the heat . I did the welds on the back so the heat would draw the door back closed. Same thing you notice when you weld a tab on something, it always wants to go toward the heat.

    I started with the door closed and marked a line from where it came out of line on each plane, opened the door and connected the dots as a guide for the weld. Each time it got closer and that's why they are spaced the way they are.

    I don't know if letting them sit overnight was necessary or not but I definitely did not want to screw it up more during my "fix".

    Didn't worry about grinding heat when I knocked the welds off, I had my Ironman 230 pegged when I ran those welds and it still took a few so I knew the grinder wouldn't introduce near that amount of heat.

    Sorry if that's a lousy explanation brother, I'm not exactly a wordsmith.

  7. #7
    Join Date
    Oct 2009
    Location
    Austin TX
    Posts
    823
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    Put the flange on the door opening, not the door itself. Much harder to warp a steel pipe than a thin slice of the pipe.
    Miller Syncrowave 350
    Millermatic 252/ 30A spoolgun
    Miller Bobcat 225g w/ 3545 spoolgun
    Lincoln PowerArc4000
    Lincoln 175 Mig
    Lincoln 135 Mig
    Everlast 250EX Tig
    Century ac/dc 230 amp stick
    Victor O/A
    Hypertherm 1000 plasma

  8. #8
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,302
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    Just use a big, semi flat faced hammer and smack them back into compliance after the fact.

  9. #9
    Join Date
    Jul 2013
    Location
    La Porte, TX
    Posts
    3,676
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    If you have a TIG you can use it to pull the door back in shape. Don't have to use filler so there is nothing to grind off afterwards.
    You are just heating it and letting it cool and it will shrink toward the side you heated. Could be done with an O/A or O/P torch as well.
    Gravel

    The difference between theory and practice is that in theory there is no difference.

  10. #10
    Join Date
    Aug 2012
    Location
    AR
    Posts
    2,069
    Post Thanks / Like

    Re: Flanges on smoker doors.......please help

    amusick,

    Your explanation of grinding out the welds was very clear. Thanks for the info...for future reference when I warp something..

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,634,472,450.50760 seconds with 14 queries