    Couple of questions

    Good morning.

    First question, is it ok to tack weld with smaw and finish weld with fcaw? Does one need to worry about the differences in the weld metal?

    Second, has anyone welded T-1 to C1045? I hear it's hard to do, but can be done with the right preheat and interpass temps. Tips from your success will be appreciated.

    Third, is there any truth in a statement made that if you are certified smaw overhead, you are automatically certified to weld fcaw overhead, even though they are 2 different processes?

    Thank you!

  2. #2
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Couple of questions

    I was the supervisor on 1-mile of pipe tray in a Chevron refinery. The raising gang tacked with 7018, the welding crew ran NR-212.

    I've never seen it where SMAW certs were used for FCAW.
    Donít pay any attention to me
    Iím just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  3. #3
    Join Date
    Jan 2014
    Location
    Hallieford, VA
    Posts
    2,473
    Post Thanks / Like

    Re: Couple of questions

    Welcome to the forum.
    30+ yrs Army Infantry & Field Artillery, 25 yrs ago

    Miller 350LX Tig Runner
    TA 210, spool gun
    Lincoln 250/250 IdealArc
    ESAB PCM 500i Plasma
    Kazoo 30" vert BS
    Kazoo 9x16 horiz BS
    Clausing 12x24 lathe
    20T Air Press

  4. #4
    Join Date
    Oct 2014
    Posts
    2
    Post Thanks / Like

    Re: Couple of questions

    Thank you storeman and CEP.
    Why do they think QA has all the answers anyway?

  5. #5
    Join Date
    Oct 2007
    Location
    Louisville, KY
    Posts
    472
    Post Thanks / Like

    Re: Couple of questions

    Welcome to the nut house..... Errrr forum.


    Sent from my iPhone using Tapatalk
    Qualified & experienced at welding scrap metal

  6. #6
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    3,461
    Post Thanks / Like

    Re: Couple of questions

    No smaw welding ticket qualifies you to weld with fcaw
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,638,902,111.58827 seconds with 11 queries