    Re: You Have to check this out!!!

    Too much unsupported overhang ,wind and not following erection plan to fill in as set. That will be the findings. Hurry up work hope no one was hurt.

  2. #27
    Join Date
    Dec 2009
    Location
    Stevens Point, WI
    Posts
    5,032
    Post Thanks / Like

    Re: You Have to check this out!!!

    Why is the center section of the one beam darker than the others? It has the look of being heated and cooled.
    12v battery, jumper cables, and a 6013.
    I only have a facebook page. https://www.facebook.com/pages/VPT/244788508917829

  3. #28
    Join Date
    Feb 2010
    Location
    Northern MN
    Posts
    1,301
    Post Thanks / Like

    Re: You Have to check this out!!!

    Cranes are spendy, local contractor here had a whole stick framed building come down around them when they pushed ahead too fast and set all the trusses without completing their bracing as they went. A million dollar building turned into toothpicks in 10 minutes because they didn't want to pay for another few hours of crane time. Lateral bracing was left out and the walls weren't properly braced and sheathed, trusses started to tip and the shift caused the walls to hinge. A couple hours of of sheathing walls instead of setting trusses would have kept the building up, a few more of putting in lateral bracing would have kept the whole thing from happening. At most they would have lost a day or two of progress on the roof, instead they saw dollars burning in crane time and it cost them all their progress and the building.

    Looks like the same thing happened here, instead of loosing a few days to do it right, they tried to take a shortcut and it cost them the bridge and a year of time.

  4. #29
    Join Date
    Oct 2014
    Posts
    3,728
    Post Thanks / Like

    Re: You Have to check this out!!!

    Now the contractor is footing the bill to bring in a huge 1200 tonne crane that can pick up the whole assembly. They think the beams might be spring back straight. The crane is too big to move in one piece and has to be assembled on site. Apparently there are only 7 of these cranes in N. America.

  5. #30
    Join Date
    Feb 2011
    Location
    South Plainfield NJ
    Posts
    1,035
    Post Thanks / Like

    Re: You Have to check this out!!!

    Are you kidding they are scrap , take em down and refabricate. Hurry up erection goes wrong!

  6. #31
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,065
    Post Thanks / Like

    Re: You Have to check this out!!!

    Here's an interesting before/after picture (use the slider). Happened in the span of about 15 minutes and not much in the rigging appears to have changed.

    http://edmonton.ctvnews.ca/groat-roa...ions-1.2282110
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  7. #32
    Join Date
    Jan 2004
    Location
    Northern Cal., Shasta County
    Posts
    9,327
    Post Thanks / Like

    Re: You Have to check this out!!!

    This was one of those where the clock was ticking. It could have failed later when some guys were out there adding the missing cross bracing.
    "The things that will destroy America are prosperity at any price, peace at any price, safety first instead of duty first, the love of soft living and the get rich quick theory of life." -Theodore Roosevelt

  8. #33
    Join Date
    Feb 2011
    Location
    South Plainfield NJ
    Posts
    1,035
    Post Thanks / Like

    Re: You Have to check this out!!!

    It may not be the fault of the erector but girder stability should have been checked. The design appears to be very light to USA standards and could be a problem.Thin narrow flanges deep webs and light crossframes may not be stable untill the pans and deck poured. We had a similar problem on the Isod Arena in NJ our erection engineer told us the roof truses would not support their weight untill the roof deck was installed we told the authority and the said we were wrong. Built a truss on the ground picked it with a 4100 /9299/ 7700 Lima and it started to bend and set it back on the ground. A 3.5 MILLION change order for bracing we put it up.

  9. #34
    Join Date
    Jan 2011
    Posts
    41
    Post Thanks / Like

    Re: You Have to check this out!!!

    Quote Originally Posted by DSW View Post
    Yeah probably one of those

    "Hurry up! Quit messing with that junk. We can put the rest of those cross braces in later. 3 is fine for now. We need to get these beams set and get those cranes out of here. We're running behind and need to pick up the pace! ..."
    Sounds about right
    Isn't that always the story?We're running behind!!!

  10. #35
    Join Date
    Jun 2014
    Posts
    101
    Post Thanks / Like

    Re: You Have to check this out!!!

    It wasn't the pigeons - it was the pigeon poop.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,736,775.23624 seconds with 13 queries