    ALPHA TIG 200X water cooler set up part #1

    Installing the 220 volt 20 amp receptacle for your water cooler.

    This setup will give you the receptacle to run your water cooler so you don't need to turn the cooler on every time you turn on the welder. When you turn on your welder the receptacle gets power and the cooler comes on ( you leave the switch on the cooler on all the time).

    I will try to post these pictures in order from start to finish, but sometimes it will post them in the wrong order.Name:  STA77718.JPG
Views: 1012
Size:  55.5 KBName:  STA77719.JPG
Views: 982
Size:  56.4 KB
    Remove covers and find a good place to install the receptacle
    Name:  STA77724.JPG
Views: 988
Size:  55.0 KBName:  STA77729.JPG
Views: 980
Size:  54.4 KB
    Then mark the place to drill the hole with a hole saw, this one was 1 3/8"
    Attached Images Attached Images  
    Last edited by mechanic416; 06-14-2015 at 05:11 PM.
    www.georgesplasmacuttershop.com
    Plasma Cutter and Welder Sales and Repairs--Ebay store
    Tec.Mo. Dealer Consumables for the PT and IPT torch's

  2. #2
    Join Date
    Mar 2010
    Location
    Delaware
    Posts
    2,960
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    install receptacle and mark for screw holes. Drill screw holes and install receptacle to see how everthing lines up.
    Name:  STA77734.JPG
Views: 961
Size:  54.7 KBName:  STA77735.JPG
Views: 966
Size:  54.3 KBName:  STA77739.JPG
Views: 967
Size:  55.6 KB
    Remove receptacle so you can wire it. You will need 3 pieces of 12 gauge wire about 12" long and some wire ends. Make up the wires and install them on the receptacle and install the receptacle in the welder.
    Attached Images Attached Images   
    Last edited by mechanic416; 06-14-2015 at 05:14 PM.
    www.georgesplasmacuttershop.com
    Plasma Cutter and Welder Sales and Repairs--Ebay store
    Tec.Mo. Dealer Consumables for the PT and IPT torch's

  3. #3
    Join Date
    Mar 2010
    Location
    Delaware
    Posts
    2,960
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    Remove power wires from power PCB and install them on the wire ends you installed on your wires and wire tie them. Next install the wires on the PCB in the same places you took them off of.
    Name:  STA77746.JPG
Views: 974
Size:  55.2 KBName:  STA77748.JPG
Views: 964
Size:  55.1 KB
    Make sure you clean all the metal shavings from in side the welder from drilling the holes (blow them out with air). In stall the cover and front panel and start all the screws (don't tighten them) install the rear panel and see were the plug is, memove the panel and remove the vent fins from the panel. Install the rear panel and handle install the screws and tighten them.
    Name:  STA77755.JPG
Views: 969
Size:  54.6 KB

    Your done with part one.

    Part two will be installing the cooler and torch.
    Last edited by mechanic416; 06-14-2015 at 05:15 PM.
    www.georgesplasmacuttershop.com
    Plasma Cutter and Welder Sales and Repairs--Ebay store
    Tec.Mo. Dealer Consumables for the PT and IPT torch's

  4. #4
    Join Date
    May 2011
    Location
    Andover, Ohio
    Posts
    2,568
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    Looking good.
    Lincoln A/C 225
    Everlast P/A 200

  5. #5
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,320
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    And this doesn't void the warranty?
    Miller Multimatic 255

  6. #6
    Join Date
    Mar 2010
    Location
    Delaware
    Posts
    2,960
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    Maybe or maybe not.

    But I really don't care this welder is not under warranty anyway.

    If you want to find out if it will void your warranty call AHP and ask, thats not hard to do.

    And why do you care anyway you sold yours.
    www.georgesplasmacuttershop.com
    Plasma Cutter and Welder Sales and Repairs--Ebay store
    Tec.Mo. Dealer Consumables for the PT and IPT torch's

  7. #7
    Join Date
    Jan 2017
    Location
    Colorado Rockies
    Posts
    28
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    Not to wake an old thread... but were you happy with this method? I'm thinking of doing it on my gen 4.

  8. #8
    Join Date
    Mar 2010
    Location
    Delaware
    Posts
    2,960
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    It works great, crank it up to 200 amps use all the amps you need anytime you need them and weld away.
    www.georgesplasmacuttershop.com
    Plasma Cutter and Welder Sales and Repairs--Ebay store
    Tec.Mo. Dealer Consumables for the PT and IPT torch's

  9. #9
    Join Date
    Jan 2017
    Location
    Colorado Rockies
    Posts
    28
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    Great info, thanks for the thread. I'm thinking of using it with the HTP Artic Chill.

  10. #10
    Join Date
    Mar 2010
    Location
    Delaware
    Posts
    2,960
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    Quote Originally Posted by fixer View Post
    Great info, thanks for the thread. I'm thinking of using it with the HTP Artic Chill.
    That,s the cooler I used.
    Attached Images Attached Images  
    www.georgesplasmacuttershop.com
    Plasma Cutter and Welder Sales and Repairs--Ebay store
    Tec.Mo. Dealer Consumables for the PT and IPT torch's

  11. #11
    Join Date
    Feb 2013
    Posts
    1
    Post Thanks / Like

    Re: ALPHA TIG 200X water cooler set up part #1

    Thanks for the instructions!
    Which water cooler did you decide to go with?
    Last edited by hank3fan; 02-12-2019 at 09:18 AM.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,860,566.62024 seconds with 14 queries