    Question Digital Elite Question ?

    Hello, I am going to be taking a beginning arc welding class at my school and it will be my first time stick welding and tig welding. Can anyone give me some settings for these kinds of welding ?

  2. #2
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,253
    Post Thanks / Like

    Re: Digital Elite Question ?

    Download a welding calculator onto your phone. There is a free one that is pretty fair at the millerwelds.com site.

    Oh, do you mean for the hood? If so, shade 10, the delay is how long the shade sticks after you break the arc, mine is near minimum, but a little delay would be nice if until you get rid of the random arc strikes.
    Last edited by walker; 07-26-2015 at 07:19 PM.

  3. #3
    Join Date
    Jul 2011
    Location
    Utah
    Posts
    2,190
    Post Thanks / Like

    Re: Digital Elite Question ?

    I use shade 11 for everything, some people use 10, I find that it is too bright and hurts my eyes after a while.

    Adjust the sensitivity by looking at the brightest light source visible from your location, then turning up the sensitivity until it goes dark, then back off a notch or two. This will eliminate false triggers from overhead lights, the sun, etc.

    The delay setting controls how long it stays dark after you finish welding. Not really critical... its used for situations like when you're running pulse and the hood is constantly switching states and you cant see anything.
    Welding/Fab Pics: www.UtahWeld.com

  4. #4
    Join Date
    Jul 2015
    Posts
    3
    Post Thanks / Like

    Re: Digital Elite Question ?

    join this fascinating posting notice

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,351,015.38558 seconds with 11 queries