Re: Scrap metal art or projects
I am making a garden bell out of an old CO2 tank. Since I am using 4"x4" wooden posts, a standard 4x4 tube will not fit. I bent up some 1/8" plate into right angles and welded them together. 
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
Even though I have a plasma cutter, I decided to cut the designs in the top plate with a right angle cut off wheel and a jig saw. It was faster for me to do it that way than plasma and grind the dross and errors.

That welding created a bow in the top plate, so tomorrow I am going to try to flame straighten the piece.

Last edited by psacustomcreations; 03-19-2016 at 06:09 PM.
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
"Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi
-
Re: Scrap metal art or projects
I posted yesterday that when I welded the top rib and bottom ring that the piece became distorted. Today was my first attempt at using heat to straighten out metal. I ended up over doing it on one portion and had to resort to hammering it flat. Overall I was pretty happy with learning how to do it and the results.




Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
Wow. Some Amazing art work! Very cool!!!
-
Re: Scrap metal art or projects
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
Lamp made from parts off old bicycles. It is about 4 feet tall if you make it go almost straight up. The center tube is the tube that goes from a sprocket to the seat on a bike. I cut off the rear forks and forward tubes. The gears and chain rotate.


Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects

Originally Posted by
psacustomcreations
Would be nice if you could turn the bike pedal to turn the lamp on. just a thought?
Mullets&Pullets
-
Re: Scrap metal art or projects
That was the plan but i was running into issues with holding the sprockets and still allowing it to rotate
Sent from my SM-G930V using Tapatalk
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
I used an old scuba tank to make a couple of bells shaped like Spartan helmets.




Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Scrap metal art or projects
Those helmets look slick. How do they sound ? Does the cutouts have a greater affect on the sound ?
-
Re: Scrap metal art or projects

Originally Posted by
BD1
Those helmets look slick. How do they sound ? Does the cutouts have a greater affect on the sound ?
Here is a video of the helmet from the top of the tank. The cut outs do affect the sound and I hoped to show it on the video.
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: Scrap metal art or projects
Beautiful! Great concept! This comment was for Kevin Caron's "fly" sculpture!
Last edited by Dale Salisbury; 03-26-2016 at 10:24 PM.
Some kind of Big Blue constant current welding machine
Another smaller yet, Blue machine (it's got wire in it)
-
Re: Scrap metal art or projects
This is something I did last year. This image is only part of the sculpture, showing a crocodile swimming under a log then jumping out of the water!
Some kind of Big Blue constant current welding machine
Another smaller yet, Blue machine (it's got wire in it)
-
Re: Scrap metal art or projects
This post refers to the Tennsmith product. They make these guys like 15 miles down the road from where I live!
Last edited by Dale Salisbury; 03-26-2016 at 10:33 PM.
Some kind of Big Blue constant current welding machine
Another smaller yet, Blue machine (it's got wire in it)
-
Re: Scrap metal art or projects
Dale,
The crocodile looks great. Do you have any more pics of it or other work?
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
A couple of bells made from scuba tanks with a design plasma cut into them to look like The Punisher from the comic books and American Sniper




Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
Current welder
Hobart Handler 187
Dead welders
HF 151 dual mig
Craftsman Welder 20511
Craftsman Welder 80amp Flux
I killed them LOL!!!!
-
Re: Scrap metal art or projects
I'm glad the Mig welds I do are better than the ones on the "Big Time C-Clamp" in the video!
-
Re: Scrap metal art or projects
Ya its been awhile and my welder is acting funny.
Current welder
Hobart Handler 187
Dead welders
HF 151 dual mig
Craftsman Welder 20511
Craftsman Welder 80amp Flux
I killed them LOL!!!!
-
Re: Scrap metal art or projects

Originally Posted by
SWells
Was jw what all you used for the hot rod would be very interesting build
Thanks
WelderTurner 

-
Re: Scrap metal art or projects
One of my neighbors gave me a pile of horseshoes. I made this bell using one. I am going to give him one like it as thanks.

Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com
-
Re: Scrap metal art or projects
The Talent here is amazing , true artists .
Last edited by DLHCC; 04-21-2016 at 11:33 PM.
-
Re: Scrap metal art or projects
i did some more pieces
rob



-
Re: Scrap metal art or projects

Originally Posted by
rob214
i did some more pieces
rob
More nice pieces. I am glad to see you are incorporating copper, wood and other textures or materials. I think they help the look. Maybe you can use some copper flashing or tubing or stainless steel rods or blots to add even more.
Millermatic 252 MIG
Miller Dynasty 200DX TIG
Miller Spectrum 625 Plasma
Altas 12x36 Metal Lathe
Bridgeport Milling Machine
www.psacustomcreations.com