    Hello guys, in my welding class today I got my electrode ready to be struck and I have a flip down hood I got ready to drop it and for some reason I moved my hand and struck the arc. I was looking right at it, I was seeing a big dot like after you look at a bright light. I looked away really quick but I still got it I had my safety glasses on that say they block out 99.9% uv light I have been flashed before and did not get flash burned, do you think I will get a flash burn even though I had the glasses on?

  2. #2
    Join Date
    Jan 2015
    Location
    Bellingham, MA
    Posts
    430
    Post Thanks / Like

    Re: Flashed!!!

    I know the time I got welders flash I had to go to the ER because my eyes burned so bad I couldn't stand it. I think if you got welder's flash you would know it

  3. #3
    Join Date
    Apr 2015
    Posts
    18
    Post Thanks / Like

    Re: Flashed!!!

    Quote Originally Posted by Smartdave View Post
    I know the time I got welders flash I had to go to the ER because my eyes burned so bad I couldn't stand it. I think if you got welder's flash you would know it
    It literally just happened like 10 mins ago xD I was just wondering if I should expect it

    Sent from my LGLS990 using Tapatalk

  4. #4
    Join Date
    Sep 2010
    Location
    China
    Posts
    1,063
    Post Thanks / Like

    Re: Flashed!!!

    I have yet to get it and have been welding 5-6 years, I have looked at the arc so many times but only for a split second. I think you are fine, it does blind you for a hot second though haha.
    Miller Maxstar 200 SD
    Piperliner #10 Gold

  5. #5
    Join Date
    Nov 2010
    Location
    Houston Pennsylvania USA
    Posts
    4,061
    Post Thanks / Like

    Re: Flashed!!!

    Dead meat.

  6. #6
    Join Date
    Nov 2013
    Location
    Bay Area Cali
    Posts
    918
    Post Thanks / Like

    Re: Flashed!!!

    Clear safety glasses should protect you for the occasional flash. It's the continuing exposure usually reflected off something to the side or behind you and back into the hood then off the welding lens that will get you.


    Sent from my iPhone using Tapatalk
    Long after the price is forgotten, the quality will remain.

    Both of my Poppy's 1954 Short Hoods -Third generation to weld with it and teaching a fourth
    SA 2## - Bought and sold more than I can remember or care to list, 8 in the shop right now

  7. #7
    Join Date
    Apr 2010
    Posts
    2,963
    Post Thanks / Like

    Re: Flashed!!!

    RmRider15

    'Buck up' - the really-bad aspects of welding are years ahead of you . . .

    This is an edited reprint from 01/19/15 - Arc eye!?

    You may be attributing two distinct phenomenon into one causality.

    For lack of proper medical terminology: I'll call the 1st an Optic-Flash,
    momentary blindness; and the 2nd - a Flash-Burn - the sand in the eyes feel.

    The first: you usually get from yourself as a result of a split-second fumble
    of a hood flip, lead snag, or a surprise from a co-worker. Instantly all you
    can see: is the big-white-light we all know.

    The Retina is the interior lining of the eye which transmits optic message to the
    brain; it has been over stimulated, and simply requires sometime to normalize.

    Repeated intense Optic-Flashes have been associated with retinal detachment,
    and the incident is slightly higher in near-sighted individuals [glasses]. All we
    can do is to be careful.

    A Flash-Burn: the 'sand in the eyes pain' which is so celebrated, occurs when
    the Sclera - the white outer wall of the eye - gets sunburned. Unless you have
    painted the inside of your hood silver and placed a mirror behind you while
    welding you cannot get this from yourself. A Flash-Burn occurs from prolonged
    exposure to indirect, oblique light, typically from the welding going on around
    you.

    Prolonged-exposure multiplies vectors intensity. Portable welding shields are
    the simplest prevention.


    Opus

  8. #8
    Join Date
    Oct 2014
    Posts
    3,774
    Post Thanks / Like

    Re: Flashed!!!

    If you got flashed, you'll know it about 2 am when it feels like your eyes are being sandblasted. A flash normally clears up by the next morning but sometimes a bad flash might require you to wear an eye patch for a day. If your eyes get sore try not to rub them but if they stay sore don't assume it was a flash. Get to the Dr. to have them checked to make sure there is nothing that got in them.

  9. #9
    Join Date
    Nov 2013
    Location
    Livingston, New Jersey, United States
    Posts
    1,086
    Post Thanks / Like

    Re: Flashed!!!

    If they burn put a slice of raw potato on each eye lid. Works for me
    John

    Sent from my XT1254 using Tapatalk

  10. #10
    Join Date
    Jun 2015
    Location
    Southern, VA
    Posts
    202
    Post Thanks / Like

    Re: Flashed!!!

    You rang

  11. #11
    Join Date
    Nov 2010
    Location
    Houston Pennsylvania USA
    Posts
    4,061
    Post Thanks / Like

    Re: Flashed!!!

    Whatever you do don't update the thread.

  12. #12
    Join Date
    Oct 2012
    Location
    Sacramento, California
    Posts
    1,632
    Post Thanks / Like

    Re: Flashed!!!

    Quote Originally Posted by mikecwik View Post
    Whatever you do don't update the thread.
    He's blind now, can't find it.

  13. #13
    Join Date
    Apr 2015
    Posts
    18
    Post Thanks / Like

    Re: Flashed!!!

    Quote Originally Posted by Fnord5 View Post
    He's blind now, can't find it.
    Lol my bad you guys. I actually did not get any burn from the flash none of the sand in the eyes or redness. I guess the safety glasses do what they say xD

    Sent from my LGLS990 using Tapatalk

  14. #14
    Join Date
    Jan 2006
    Location
    In A Nice Comfy Chair
    Posts
    18,766
    Post Thanks / Like

    Re: Flashed!!!

    I have yet to get the burning at night because of flashing myself.
    And I have done it MANY times in 40 years.

    What you do to prevent it and some think I am nuts/kidding...

    When you get the flash..if there is flourecent lighting where you are as soon as you can stare at the light for about a minute...

    Put mask down and continue welding.

    It works.
    It really does.


    ...zap!


    I am not completely insane..
    Some parts are missing

    Professional Driver on a closed course....
    Do not attempt.

    Just because I'm a dumbass don't mean that you can be too.
    So DON'T try any of this **** l do at home.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,827,885.98249 seconds with 11 queries