    Hi guys, I'm sure this has already been asked before but since I'm new I'm going to ask again. I have 2 welded table legs that have 2' flat bar as the base and top. They started straight but the top now has a slight bow to it. Is this something that I can exert a little sweat with a mallet and get back into shape or is the answer more involved?

    Name:  Legs.jpg
Views: 894
Size:  52.8 KB

    Thanks so much for your help/expertise!!

  2. #2
    Join Date
    Sep 2009
    Location
    Sedona, Arizona
    Posts
    1,016
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Looks like you are going to use the upper flat bar to lag bolt the legs to a wood surface. Not how I would ever do it but the lag bolts will pull the flat bar flush to whatever you are mounting them to.

    If you use a single row of lag bolts to hold the leg to a wood surface, you just installed a pivot that will wobble no matter how wide your flat bar is. You need two rows of lag bolts to not be a pivot. Consequently the width of your flat bar is important. Especially with what looks like standing height table legs.

    FYI I would never condone using lag bolts in furniture.

  3. #3
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Something that thin, Iíd smack it with a hammer. Any thicker, then Iíd heat shrink it back into shape.
    Donít pay any attention to me
    Iím just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  4. #4
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    483
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    your problem has many good solutions, and the same end result can come from many different methods.

    with that said, this is what i would do;

    -first, try a hammer if you have a big enough hammer and a sturdy enough 'anvil' to beat against. of course hammer may leave unacceptable markings.

    -second, clamp the piece in a vise and use the length of the leg as a lever to bend maybe even a a pump jack to put enough force on it. this may lead to an offset bend the will leave you with a more or less flattened piece but with a noticeable bend.

    -third, heat pulled it down... heat can pull it back. you can use a torch on the opposite side on the weld, use a flame that will heat the metal just short of melting or cutting. then run the torch opposite of the weld moving on as the metal is 'cherry' hot. one pass you want direct focused heat, not a back and forth that allows the heat to spread, just one slow pass. little bit more of a learning curve than brute force, but you get back waht you put in


    *you may find that combining methods, ie clamp heat then bend, yield best result.
    ** to avoid problem in the first place firmly clamp to suitable work surface then weld, remove once weld has cooled.
    Last edited by tracymobilecnc; 12-05-2015 at 05:36 PM.

  5. #5
    Join Date
    Dec 2015
    Posts
    7
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    That was how I was planning to do it. Can you go into a bit more explanation about the pivot that will cause the wobble just so I can understand? The width is 2" so If they were staggered I could have two rows of lag bolts. Would that help? The height is only 29" so its sitting height if that affects anything. If not lag bolts, what would you recommend?

  6. #6
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    If you heat shrink, Iíd use a large welding tip, or a cutting tip. Heat where the red lines are. Spray water on the heated lines. Wait until the heated area is dead cold to the naked hand. If this is not enough, move towards the center an inch or two, and heat another line. Spray with water, wait until the heated line is dead cold to the naked hand.
    Attached Images Attached Images  
    Donít pay any attention to me
    Iím just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  7. #7
    Join Date
    Dec 2015
    Posts
    7
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Luckily for me, smacking it with a hammer is within my skill set. I was reading about using heat shrinking but I don't have the tools to do it. I made these at a maker space and they have a welder but that's about it. Would a local metal fab place be able to heat shrink it if the hammer doesn't work you think?

  8. #8
    Join Date
    Dec 2015
    Posts
    7
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Quote Originally Posted by Jimmy_pop View Post
    Looks like you are going to use the upper flat bar to lag bolt the legs to a wood surface. Not how I would ever do it but the lag bolts will pull the flat bar flush to whatever you are mounting them to.

    If you use a single row of lag bolts to hold the leg to a wood surface, you just installed a pivot that will wobble no matter how wide your flat bar is. You need two rows of lag bolts to not be a pivot. Consequently the width of your flat bar is important. Especially with what looks like standing height table legs.

    FYI I would never condone using lag bolts in furniture.
    That was how I was planning to do it. Can you go into a bit more explanation about the pivot that will cause the wobble just so I can understand? The width is 2" so If they were staggered I could have two rows of lag bolts. Would that help? The height is only 29" so its sitting height if that affects anything. If not lag bolts, what would you recommend?

  9. #9
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Anybody with a torch can do this. Iím just a hobbyist, and I can do it.
    Donít pay any attention to me
    Iím just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  10. #10
    Join Date
    Dec 2015
    Posts
    7
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Quote Originally Posted by CEP View Post
    If you heat shrink, I’d use a large welding tip, or a cutting tip. Heat where the red lines are. Spray water on the heated lines. Wait until the heated area is dead cold to the naked hand. If this is not enough, move towards the center an inch or two, and heat another line. Spray with water, wait until the heated line is dead cold to the naked hand.
    Luckily for me, smacking it with a hammer is within my skill set. I was reading about using heat shrinking but I don't have the tools to do it. I made these at a maker space and they have a welder but that's about it. Would a local metal fab place be able to heat shrink it if the hammer doesn't work you think?

  11. #11
    Join Date
    Dec 2015
    Posts
    7
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Quote Originally Posted by CEP View Post
    Anybody with a torch can do this. I’m just a hobbyist, and I can do it.
    That's good to know! Since I'm new to this forum, is there a place that has listing where people with torches etc who have posted there info that can be searched by location? Something like 100K Garages but for welders?

  12. #12
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Look in your local telephone book for a fab / welding shop. Or stop by a welding supply, theyíll know who can do this for you.
    Donít pay any attention to me
    Iím just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  13. #13
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,899
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    To prevent this next time , only weld parallel with the flat bar , the long way
    Last edited by BD1; 12-05-2015 at 08:36 PM.

  14. #14
    Join Date
    Feb 2012
    Location
    Sweden
    Posts
    689
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Quote Originally Posted by jswtraveler View Post
    I was reading about using heat shrinking but I don't have the tools to do it.
    That's a truth with a modification. The original warp occurred because of heat shrinking - the hot weld shrinking as it cools down, pulling the metal to an unwanted shape. It might not be ideal, but making welds in strategic places can make metal warp the way you need it to, just as well as poorly placed welds can f*ck things up.

  15. #15
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    8,497
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    What are you using as a top?
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  16. #16
    Join Date
    Dec 2015
    Posts
    7
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    Quote Originally Posted by Broccoli1 View Post
    What are you using as a top?
    I'm not sure yet. I've got some inch thick live edge pine but I'm not sure it's completely dry yet. My other thought was a SC door with some feather finish to give it a concrete look.

  17. #17
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    483
    Post Thanks / Like

    Re: Straighten bent steel from weld?

    if a welder is what you got, thats fine doesn't have to be a torch.

    grind a small relief along the heat line and weld it. let cool then if needed grind down the weld that sits too high. when i make metal to wood furniture i would never want to have a wood top pull the metal back into place, its potential to damage the top isn't worth it.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,360,330.28911 seconds with 14 queries