    Something I have been working on.
    26" dia. 14" high
    10g steel.
    CNC plasma cut.
    All welded construction using 1/8 7018-1
    Aprox weight: 50lbs.





    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  2. #2
    Join Date
    Jun 2007
    Location
    Wadsworth Ohio
    Posts
    1,518
    Post Thanks / Like

    Re: custom fire ring project

    Looks great. That is something else I have to add to my list of to-do projects.
    Dave Reber
    Wadsworth Ohio

  3. #3
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    3,461
    Post Thanks / Like

    Re: custom fire ring project

    I used high heat bbq paint (650f). It will be interesting to see if it holds up to the fire heat.
    I don't have a metal roll thus the reason for a 6 sided ring.
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  4. #4
    Join Date
    Mar 2011
    Location
    Westmont, IL
    Posts
    397
    Post Thanks / Like

    Re: custom fire ring project

    You spelled "Cubs" wrong. Otherwise it's cool.
    __
    David Hillman

  5. #5
    Join Date
    Jun 2011
    Location
    North Florida
    Posts
    397
    Post Thanks / Like

    Re: custom fire ring project

    Was it supposed to say "Cubs"? If so, that is a huge mistake. I could see "Cubbs", but Cobbs??

  6. #6
    Join Date
    Sep 2010
    Location
    Tucson
    Posts
    65
    Post Thanks / Like

    Re: custom fire ring project

    Really nice. Only one problem. The side with the Vikings cut into it will probably flame up really hot, then retire, then make you think its comeing back, then retire, then come back..... and repeat.

  7. #7
    Join Date
    Dec 2007
    Location
    forest lake minnesota
    Posts
    685
    Post Thanks / Like

    Re: custom fire ring project

    Quote Originally Posted by mattlago View Post
    Really nice. Only one problem. The side with the Vikings cut into it will probably flame up really hot, then retire, then make you think its comeing back, then retire, then come back..... and repeat.
    that's funny I think the vikings side will lay down and wine about stadium.


    nice job looks pretty cool
    Pound to fit, paint to match

  8. #8
    Join Date
    Jun 2007
    Location
    Apache Junction, AZ
    Posts
    99
    Post Thanks / Like

    Re: custom fire ring project

    How has the high temp paint held up on these?

  9. #9
    Join Date
    Dec 2011
    Location
    S.W. Michigan
    Posts
    386
    Post Thanks / Like

    Re: custom fire ring project

    Nice job, and it doubles as a floor stencil.
    Hammer
    File
    Big Hammer
    ------------------------------
    Here, let me Google that for you...

  10. #10
    Join Date
    Feb 2012
    Location
    ny
    Posts
    6,178
    Post Thanks / Like

    Re: custom fire ring project

    Quote Originally Posted by David Hillman View Post
    You spelled "Cubs" wrong. Otherwise it's cool.
    I went back and checked.
    I hate being bi-polar it's awsome




    My Heroes Have Always Been Cowboys

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,253,080.13515 seconds with 20 queries