  1. #1
    Join Date
    Apr 2009
    Location
    Marshall, NC
    Posts
    952
    Post Thanks / Like

    Some of the ugliest welds you ever did see...

    ...and I did them on purpose.

    Client wanted a "bottle tree" so I figured while I'm at it I'll get enough material to make a couple of extras.

    Name:  0206121452.jpg
Views: 2957
Size:  87.5 KB

    Name:  0206121539b.jpg
Views: 2950
Size:  65.2 KB

    Name:  0206121549.jpg
Views: 2957
Size:  64.0 KB

    Name:  0206121642d.jpg
Views: 2958
Size:  84.9 KB

    Name:  0206121643.jpg
Views: 2947
Size:  71.9 KB
    Brian Leonard
    Appalachian Ironworks L.L.C.
    434 Long Branch Rd, Marshall, NC 28753
    828 649 9966
    828 702 0697
    brian@appironworks.com
    www.appironworks.com

  2. #2
    Join Date
    Mar 2011
    Location
    red rock country
    Posts
    263
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Is it to put empty wine bottle, etc. on the branches?
    They look nice, whatever they're for. I'm always amazed by the artistry I see in your projects. you can tell there's a lot of thought and effort put into them. the bark almost looks natural. nice job

  3. #3
    Join Date
    Mar 2007
    Location
    MidWest
    Posts
    537
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    I think they look pretty good, what ever the customer wants to use them for. On top of that Brain, look at all the experience you have gained running the machine cold.
    Geezer
    Power Mig 255C
    185 TIG
    Blue 175 MIG
    Ranger 8 Kohler 20HP
    1974 5K Lincoln/Wisconsin Powered (Cherry)
    Victor/Harris O/A
    K 487 Spool Gun

  4. #4
    Join Date
    Jan 2010
    Location
    Detroit
    Posts
    741
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Nice job! Glad 2 see u have an "iron thumb"

  5. #5
    Join Date
    Jul 2011
    Location
    Western Washington
    Posts
    3,656
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    wow, those are cool. who much wire did you go through with those?
    There are no problems. There are only solutions. It's your duty to determine the right one.

    Hobart Handler 210
    Airco 225 Amp MSM Stinger

  6. #6
    Join Date
    Nov 2008
    Location
    Lincoln, Ne.
    Posts
    680
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Very cool. A bottle forest...

    (Retired) Professional firefighter, amateur everything else I try to do...
    Oh yeah: Go Big Red! (You know: one of the 12 members of the Big 10 cuz we left the 10 members of the Big 12...)

  7. #7
    Join Date
    Feb 2009
    Location
    Calg, AB
    Posts
    719
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    SWEEEEET!
    I plan on putting one of those together for this Spring! Yours are Fantastic!

    BTW, how long of a Stake do you require on something of that weight and size to keep it 'planted firmly' (pun intended) in the ground?

    Cheers,
    Miller Diversion 165
    120 amp Buzz Box
    Victor Oxy/Ace Oxy/LPG
    Smith "Little" Oxy/LPG
    Hypertherm Powermax 30
    Lot's of Misc. tools n' crap....

  8. #8
    Join Date
    Jul 2011
    Location
    Utah
    Posts
    2,190
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    I feel sorry for the poor bastard who tries to walk through those trees.
    Welding/Fab Pics: www.UtahWeld.com

  9. #9
    Join Date
    Nov 2010
    Location
    NH
    Posts
    1,647
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Very cool stuff!
    Buy American, or don't whine when you end up on the bread line.

  10. #10
    Join Date
    Jun 2010
    Location
    Niagara on the lake Canada
    Posts
    1,401
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    that looks like it took some time. Is it harder to do all those stringers knowing that it isn't for the sake of attaching something but just for decoration? Also not "ugly" it's perfect decorativity..
    Miller thunderbolt 250
    Decastar 135E
    Recovering tool-o-holic
    ESAB OA
    I have been interested or involved in Electrical, Fire Alarm, Auto, Marine, Welding, Electronics ETC to name a just a few. So YES you can own too many tools.

  11. #11
    Join Date
    Jan 2012
    Posts
    5
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by MikeGyver View Post
    I feel sorry for the poor bastard who tries to walk through those trees.
    I would love to put one of these in my yard to see how the deer react to it. Try rubbing your horns on that!
    Though on a serious note I think you did a great job! Thanks for sharing.

  12. #12
    Join Date
    Apr 2009
    Location
    Marshall, NC
    Posts
    952
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by Birdwell4 View Post
    Is it to put empty wine bottle, etc. on the branches?
    They look nice, whatever they're for. I'm always amazed by the artistry I see in your projects. you can tell there's a lot of thought and effort put into them. the bark almost looks natural. nice job
    Yeah you put wine bottles on the branches, stems from some old hoodoo root doctor kind of stuff. Something about catching spirits in the bottles.

    Quote Originally Posted by geezer View Post
    I think they look pretty good, what ever the customer wants to use them for. On top of that Brain, look at all the experience you have gained running the machine cold.
    Thanks, but I was already pretty good at that.

    Quote Originally Posted by ThorsHammer View Post
    wow, those are cool. who much wire did you go through with those?
    Less than 3 lbs per tree total. The bark welding wasn't enough to make a difference on my cheap bathroom scale.

    Quote Originally Posted by strube1369 View Post
    Very cool. A bottle forest...
    Well they're only 5' tall and only three so maybe a bottle hedgerow?

    Quote Originally Posted by jman View Post
    SWEEEEET!
    I plan on putting one of those together for this Spring! Yours are Fantastic!

    BTW, how long of a Stake do you require on something of that weight and size to keep it 'planted firmly' (pun intended) in the ground?

    Cheers,
    There are loops at the end of each root for anchors if it's going on a hard surface, or you could sink a post in the ground and set them over it. A couple three feet or so should be plenty. They're fairly stable as they stand.

    Quote Originally Posted by MikeGyver View Post
    I feel sorry for the poor bastard who tries to walk through those trees.
    Tell me about it. I feel sorry for the poor bastard who welded them up and stabbed himself several times in the process.

    Quote Originally Posted by dumb as a stump View Post
    that looks like it took some time. Is it harder to do all those stringers knowing that it isn't for the sake of attaching something but just for decoration? Also not "ugly" it's perfect decorativity..
    I think you just made up a new word, cool.

    Nah the stringers were a cinch. Go as fast as I can and let my old shaky hands shake all over.

    Quote Originally Posted by BoostingAmerica View Post
    I would love to put one of these in my yard to see how the deer react to it. Try rubbing your horns on that!
    Though on a serious note I think you did a great job! Thanks for sharing.
    That reminds me of a joke: What do you call a blind doe?

    I'll bet they won't nibble the leaves off either.

    I've got a little of the "tree bark" embossed bar left, I'm thinking it would be cool to make a nice 8 or 10 point rack with it.
    Brian Leonard
    Appalachian Ironworks L.L.C.
    434 Long Branch Rd, Marshall, NC 28753
    828 649 9966
    828 702 0697
    brian@appironworks.com
    www.appironworks.com

  13. #13
    Join Date
    Jul 2011
    Location
    Bossier Parish La.
    Posts
    5,824
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by app-ironworksllc View Post

    That reminds me of a joke: What do you call a blind doe?

    .
    A NoSeeDoe?


    The easiest way to get a bottle tree in your yard is to plant a bottle about 3" deep, water well and hope for the best.

  14. #14
    Join Date
    Apr 2009
    Location
    Marshall, NC
    Posts
    952
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by Bistineau View Post
    A NoSeeDoe?




    The easiest way to get a bottle tree in your yard is to plant a bottle about 3" deep, water well and hope for the best.
    I wonder if you put money in the bottle you'd get a money tree?

    Try it and show me where they are so I can "check" on them for you.
    Brian Leonard
    Appalachian Ironworks L.L.C.
    434 Long Branch Rd, Marshall, NC 28753
    828 649 9966
    828 702 0697
    brian@appironworks.com
    www.appironworks.com

  15. #15
    Join Date
    Nov 2008
    Location
    Huntsville, Al
    Posts
    129
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Care to share how you "necked down" the crotch of the tree?
    Thanks
    Allen

  16. #16
    Join Date
    Sep 2010
    Location
    southwest VA
    Posts
    633
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by minner View Post
    Care to share how you "necked down" the crotch of the tree?
    You perverts on the internet always wantin' to see "neck-ed crotches".

  17. #17
    Join Date
    Jan 2006
    Location
    In A Nice Comfy Chair
    Posts
    18,764
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    I think they are pretty funny...

    How much do they weigh?

    ...zap!


    I am not completely insane..
    Some parts are missing

    Professional Driver on a closed course....
    Do not attempt.

    Just because I'm a dumbass don't mean that you can be too.
    So DON'T try any of this **** l do at home.

  18. #18
    Join Date
    Sep 2008
    Location
    Louisiana
    Posts
    786
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Brian, nice stuff.
    If you have too many customers that want stuff like that I will be happy to take them off your hands... I don't have enough of those. The ones that want stuff like that but don't want to pay for it--------- I have too many of!
    Peter
    Equipment:
    2 old paws
    2 eyes (that don't look so good)
    1 bad back

  19. #19
    Join Date
    Jul 2011
    Location
    Bossier Parish La.
    Posts
    5,824
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by app-ironworksllc View Post
    I wonder if you put money in the bottle you'd get a money tree?

    Try it and show me where they are so I can "check" on them for you.
    Probably not, the bottle would keep the money dry and it would not germinate properly. Try it and see. I was wondering if I came up with the right answer to the blind doe question, a NoSeeDoe.

  20. #20
    Join Date
    Apr 2009
    Location
    Marshall, NC
    Posts
    952
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by Bistineau View Post
    Probably not, the bottle would keep the money dry and it would not germinate properly. Try it and see. I was wondering if I came up with the right answer to the blind doe question, a NoSeeDoe.
    All I have for the jar is jingly money, no folding money.

    Nope that's not it.

    No eye deer.

    What do you call a cow with no legs?
    Brian Leonard
    Appalachian Ironworks L.L.C.
    434 Long Branch Rd, Marshall, NC 28753
    828 649 9966
    828 702 0697
    brian@appironworks.com
    www.appironworks.com

  21. #21
    Join Date
    Aug 2006
    Location
    San Dimas, CA
    Posts
    3,028
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by app-ironworksllc View Post

    What do you call a cow with no legs?
    Dinner

    Nice work on the trees!
    http://all-a-cart.com

    Welding Cart Kits and accessories

  22. #22
    Join Date
    Apr 2009
    Location
    Marshall, NC
    Posts
    952
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by minner View Post
    Care to share how you "necked down" the crotch of the tree?
    Thanks
    Allen

    The short bent pieces of pipe get 4 long narrow notches on the branch end, then that end is beat together into a taper and welded up after getting fit to the 3/4" "tree bark" embossed bar.

    Then they are put together like the collector on a header, then welded to the trunk. The trunk is 3" pipe with a few plasma slices partially through to allow easy bending. Then they're welded up so they have a more organic curve to them.
    Name:  0203121554b.jpg
Views: 1843
Size:  46.5 KB

    Quote Originally Posted by dbotos View Post
    You perverts on the internet always wantin' to see "neck-ed crotches".
    Betcha a hundred bucks you don't want to see mine. Betcha two hundred bucks I don't want to show you.

    Quote Originally Posted by zapster View Post
    I think they are pretty funny...

    How much do they weigh?

    ...zap!
    44 lbs each. They stand 5' tall and about 3'-6" diameter. wild hold (18) empty wine bottles.

    Quote Originally Posted by castweld View Post
    Brian, nice stuff.
    If you have too many customers that want stuff like that I will be happy to take them off your hands... I don't have enough of those. The ones that want stuff like that but don't want to pay for it--------- I have too many of!
    Peter
    Peter I wish I had more. These actually stem from a swap ( I know, I know, never ever swap. But this was a good one.) with my land lord.

    One is his in exchange for a gold and diamond necklace he had that I gave my wife for Christmas. (BTW she loved it) He's a jeweler (as well as a machinist and plant maint. eng.)

    While I was making one I figured I'd get some extra material to defray the shipping costs and make 2 extras.

    So one will be my wife's Valentine's Day present. I think I'm going to add leaves and hooks and make it a bird feeder hanger. I'm thinking about incorporating a bird bath made from sheet that would look like the top center of the canopy, too.

    The 3rd one is for sale, $499.99 plus freight. I'm going to throw it in my truck (along with the afore mentioned deer head I've started) and see if any of the craft shops around here are interested in some artsy fartsy stuff.

    No eye deer, get it?
    Name:  0207121721.jpg
Views: 1843
Size:  61.7 KB

    After reading the box thread I might break out the o/a torch and give it a go old school on the skull, maybe even use a coat hangar for filler. It's kind of like a box, just not really like a box.
    Brian Leonard
    Appalachian Ironworks L.L.C.
    434 Long Branch Rd, Marshall, NC 28753
    828 649 9966
    828 702 0697
    brian@appironworks.com
    www.appironworks.com

  23. #23
    Join Date
    Apr 2009
    Location
    Marshall, NC
    Posts
    952
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Quote Originally Posted by ZTFab View Post
    Dinner

    Nice work on the trees!
    Thanks.

    Nope, ground beef.

    What do you call a cow with 2 legs?
    Brian Leonard
    Appalachian Ironworks L.L.C.
    434 Long Branch Rd, Marshall, NC 28753
    828 649 9966
    828 702 0697
    brian@appironworks.com
    www.appironworks.com

  24. #24
    Join Date
    Jul 2011
    Location
    Queens, NY
    Posts
    574
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Wow, that's some really cool work.
    IW Local 580 NY, NY

  25. #25
    Join Date
    Dec 2010
    Location
    Seattle
    Posts
    43
    Post Thanks / Like

    Re: Some of the ugliest welds you ever did see...

    Thats really creative I like it.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,926,491.11782 seconds with 14 queries