    Manganese welding fumes cause neurological injury

    Here's a short investigative article describing the history of the development of medical knowledge about the danger of manganese welding fumes that may be helpful to some readers.

    There's a lot of good reasons to wear a respirator while you're welding, folks. It's not just your lungs that can be damaged...

    http://www.motherjones.com/politics/...ke-and-mirrors

  2. #2
    Join Date
    Dec 2015
    Location
    Western New York State, USA
    Posts
    2,069
    Post Thanks / Like

    Re: Manganese welding fumes cause neurological injury

    a lot of metals are not good vanadium, lead, chrome, cadmium not to mention flux fumes. in the old days they used asbestos in 6010 rod flux.
    .
    that cheap welding rod that you have no ideal where it was made, can have many surprising things in it you are breathing

  3. #3
    Join Date
    Jan 2004
    Location
    Northern Cal., Shasta County
    Posts
    9,327
    Post Thanks / Like

    Re: Manganese welding fumes cause neurological injury

    Heavy on innuendo and opinion, light on data.
    "The things that will destroy America are prosperity at any price, peace at any price, safety first instead of duty first, the love of soft living and the get rich quick theory of life." -Theodore Roosevelt

  4. #4
    Join Date
    Mar 2014
    Posts
    4,394
    Post Thanks / Like

    Re: Manganese welding fumes cause neurological injury

    By way of coincidence....... here in a couple hours I've got an appointment at the local VA clinic for a routine annual check up. When I made the appointment I asked about screening for heavy metals, (Manganese in particular) and was told that it wouldn't be a problem. I'll know more about the procedure for it after I talk to the Doc and will report back on what I find out.
    Last edited by HT2-4956; 02-02-2016 at 10:47 AM.

  5. #5
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Manganese welding fumes cause neurological injury

    Wait a minute! Don’t you have to be touched in the head a little bit in the first place to ever want to be a welder?
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  6. #6
    Join Date
    Dec 2015
    Location
    Western New York State, USA
    Posts
    2,069
    Post Thanks / Like

    Re: Manganese welding fumes cause neurological injury

    i have known 2 welders who both had brain cancers. they say tungsten thoriated for tig is radioactive. not sure if brain cancer is more common in welders or if just a coincidence.

  7. #7
    Join Date
    Dec 2015
    Location
    Napa, CA
    Posts
    95
    Post Thanks / Like

    Re: Manganese welding fumes cause neurological injury

    That seems anecdotal.
    Miller XMT 350 CC/CV
    Miller S74-D
    Hobart Airforce 500i

  8. #8
    Join Date
    Aug 2009
    Location
    Northern NY
    Posts
    83
    Post Thanks / Like

    Re: Manganese welding fumes cause neurological injury

    @CEP *like*

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,304,424.12384 seconds with 20 queries