Page 1 of 22 12311 ... LastLast
Results 1 to 25 of 543

Thread: Some everyday railings (and other cool stuff)

  1. #1
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Some everyday railings (and other cool stuff)

    So I do a lot of "wrought iron" railings, fencing and gates, so I figure I'll share my work, for anyone interested.

    Questions, comments and criticisms are all welcome.

    So I'll start with some projects I did last year, and keep updating as I do more work.

    Enjoy!

  2. #2
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    So here's a pool fence I did in greenwich, lovely property.






    Last edited by MetalMan23; 02-02-2016 at 09:46 PM.

  3. Likes whtbaron liked this post
  4. #3
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Here's a topper fence along a curved stone wall





    I bent the horizontal rails with the HF hydraulic tubing bender with some custom dies I made

  5. Likes Joegreen02 liked this post
  6. #4
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Ok here's a gate a made to match some existing stuff. Again this one's in greenwich ,

    The last one ^^^^^ was in greenwich too





    Lol a couple days before the install, after it was all painted, I realized that I had forgotten to put the knuckles in the middle of the pickets, so I ordered some snap on plastic ones, luckily they matched, and they blend in too

  7. Likes Joegreen02, whtbaron liked this post
  8. #5
    Join Date
    Mar 2008
    Location
    Georgetown, Texas
    Posts
    2,033
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    You killed it on that curved one. They all look really nice and are all money makers.

  9. #6
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Quote Originally Posted by Bob View Post
    You killed it on that curved one. They all look really nice and are all money makers.
    Thanks! I love doing stuff like that, it's rewarding.

    yeah I definitely made some money on the curved one, it was about 75 linear ft total.


    I made some radius railings a couple years ago, I'll see if I can find the pics

  10. #7
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,823
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Nice job, matches the homes .

  11. #8
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Quote Originally Posted by BD1 View Post
    Nice job, matches the homes .
    Thanks BD1

    yeah these people got money$$

  12. #9
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    14,946
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    I like your work - nicely done
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  13. #10
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,547
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Nice work. Nice curves. Plastic is great in right situation and fast and fits well and doesn't rust.
    .

  14. #11
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Quote Originally Posted by MinnesotaDave View Post
    I like your work - nicely done
    Thank you sir

  15. #12
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Mick120, tapwelder, thanks

    I'll have some more pics tomorrow.

  16. #13
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,301
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    You are working in the right part of the state.

    Nice work.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  17. #14
    Join Date
    May 2007
    Posts
    3,755
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    nice. i tell customers, theres a difference between a "welder that makes a fence, and a fence man that welds". around where i live, it is industry standard for fence co's, to not weld the underside of the bottom tube rail. the co i once worked for, it was also noted in there contracts in sorta fine print. its a almost guaranteed rott out in time, especially on fences running through grass w/ sprinklers. i try to avoid fence work these days, other than repairs, or small jobs when i get roped into it for somebody i know. i feel i done enough to last me the rest of my natural life. back in the early aughts, when marlboro and all the other tabaccoo companies got sued, or settled out, the public schools got a chunk of that, and it seemed every public school was replacing there chain link fences w/ ornamental iron panels that were powder coated over galvanized tubing. i could get into living in that house

  18. #15
    Join Date
    Jan 2004
    Location
    Canton, Ga.
    Posts
    31
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Hey Metalman,
    The curved rail looks great!
    What material are you using to anchor in stone?
    Thanks,
    Mike

  19. #16
    Join Date
    Mar 2012
    Location
    Charlottetown,PE.Canada
    Posts
    714
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    I bent the horizontal rails with the HF hydraulic tubing bender with some custom dies I made[.

    You took what usually is a boring looking everyday railing and turned it into something very attractive with those curves! Well done!!!

  20. #17
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    123weld, thanks that's a good point, I'm a welder who makes fencing. I try to make the best quality I can.

    d110pickup,
    i use anchoring cement, comes in 1 gallon buckets, it's a type of hydraulic cement, expanding slightly as it cures, which only takes about 45 min. Now I've neen using a blend of anchoring cement and water stop cement, it hardens in about 10 min, and cures in about 45 min.


    BrianC,
    thanks! I love it when someone is willing to pay for radius/ curved stuff, it's definitely a challenge that I enjoy. and it really adds a level of quality to the job.

  21. Likes Joegreen02 liked this post
  22. #18
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Ok so I found some pics of the radius stuff, this house had 2 porches off the back of the second floor.





    And here's some pics in summer when I came back to touch up the paint





    This job was fun to do, my first real radius job. I took a template with a price of plywood, and again I used the HF tubing bender with custom dies to bend the caprail the hard way.

  23. Likes Joegreen02, whtbaron liked this post
  24. #19
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)



    Here's something I'm working on today.

    Still have to drill and tap for hinges, and paint

  25. Likes Joegreen02, whtbaron liked this post
  26. #20
    Join Date
    Sep 2011
    Location
    The Dalles, OR
    Posts
    117
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Beautiful work, thanks for sharing.

  27. #21
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    My pleasure,


    Here's a couple more Gates:






    And here's some interior gates, I did 3 inside this customers house, to help keep dogs out of certain rooms



  28. #22
    Join Date
    Jan 2015
    Location
    Edmonds, WA
    Posts
    616
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Did you use the HF bender or roller for your radii?

  29. #23
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    I use the their regular bender for the easier stuff, and for the hard stuff, like tubing or cap rail the hard way, I use their hydraulic tubing bender,

    Here's a pic of my cap rail dies in the bender:




    And here's the bender set up with my square tubing dies:







    I really should be using a roller for the tubing, but I don't have 2" dies for my pyramid roller. So this works.

  30. Likes whtbaron liked this post
  31. #24
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,420
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    If the piece o steel I'm bending is not too heavy I'll just stick it between 2 slats of my old table, and pull/jump on it to get the bend. I've done a lot of bending like that, irregular curves and such.

  32. #25
    Join Date
    Apr 2008
    Location
    Charlotte NC
    Posts
    919
    Post Thanks / Like

    Re: Some everyday railings (and other cool stuff)

    Damn Nice Work!
    Miller TrailBlazer 251
    Miller HF-250-1
    Miller MaxStar 150 STL
    HyperTherm PowerMax 380 plasma
    Lincoln PowerMig 180
    Millermatic 252
    Miller Diversion 180

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,820,977.45579 seconds with 12 queries