    PowCon 300ST. Old School. Unit currently not in hand.Test driving her in Stick and TIG mode next weekend.

    Will standard Tweco male connectors interface to the aft female connectors on the machine? No connectors appear visible on the unit from the supplied pictures.

    Appreciate any insight. Mahalo.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  2. #27
    Join Date
    May 2010
    Location
    Sparks, NV
    Posts
    9,636
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Quote Originally Posted by ManoKai View Post
    PowCon 300ST. Old School. Unit currently not in hand.Test driving her in Stick and TIG mode next weekend.

    Will standard Tweco male connectors interface to the aft female connectors on the machine? No connectors appear visible on the unit from the supplied pictures.

    Appreciate any insight. Mahalo.
    Yep standard Tweco connectors

    Sent from my VK815 using Tapatalk
    Tiger Sales: AHP Distributor www.tigersalesco.com
    AHP200x; AHP 160ST; MM350P, Spoolmatic 30A; Everlast PowerTig 185; Thermal Dynamics 60i plasma.
    For Sale: Cobra Mig 250 w/ Push-pull gun. Lincoln Wirematic 250

  3. #28
    Join Date
    Jan 2013
    Location
    ...Shoulder of Orion...
    Posts
    3,509
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Mahalo Southpaw.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  4. #29
    Join Date
    Jan 2013
    Location
    ...Shoulder of Orion...
    Posts
    3,509
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Closing out a comment from posts #26 and 27.

    The PowCon 300ST we acquired from a CL seller is run'n great in both SMAW and scratch TIG. She's now become our primary rig for stick welding in the shop.

    Learned today, after patiently waiting for 3 weeks, that our LWS can recertify/fill the K cylinder that came with the welder package. The cylinder is stamped for 4400 psig and configured with a CGA-680 vintage Airco regulator. The regular is hefty/hefty and in excellent shape.

    Looking forward to having the increased volume of Ar for work.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  5. #30
    Join Date
    May 2010
    Location
    Sparks, NV
    Posts
    9,636
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Good to hear. They are really nice stick welders. Same goes for the old TA machines like the LM300 I have. Both excellent choices for inverter stick machines. The TA are quite a bit lighter than the similar Powcon. About 15-20lb difference between your 300 and mine
    Tiger Sales: AHP Distributor www.tigersalesco.com
    AHP200x; AHP 160ST; MM350P, Spoolmatic 30A; Everlast PowerTig 185; Thermal Dynamics 60i plasma.
    For Sale: Cobra Mig 250 w/ Push-pull gun. Lincoln Wirematic 250

  6. #31
    Join Date
    Jan 2013
    Location
    ...Shoulder of Orion...
    Posts
    3,509
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Quote Originally Posted by soutthpaw View Post
    Good to hear. They are really nice stick welders. Same goes for the old TA machines like the LM300 I have. Both excellent choices for inverter stick machines. The TA are quite a bit lighter than the similar Powcon. About 15-20lb difference between your 300 and mine
    DJ - thanks for your help re the connectors. And don't be mentioning any other machines to 'consider'......the bride's gun'a slay me if another item, strategically covered in old towels, is found in the shop.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  7. #32
    Join Date
    Jan 2013
    Location
    ...Shoulder of Orion...
    Posts
    3,509
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Correction re post #29: closer inspection of the vintage Airco regulator/flow meter revealed a max inlet pressure....stamped on the brass boss...of 3000psi. No es beuno to integrate onto the 4500psig working pressure cylinder.

    Will have to source a CGA-680 regulator/flow meter, and prob sell our vintage Airco.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  8. #33
    Join Date
    Jun 2021
    Posts
    1
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Your name plate seems to be in great shape. Could you take some hi res pics of it and post? My name plate was worn completely smooth. Would be nick to know max amps etc.
    Thanks,
    Dave

  9. #34
    Join Date
    Jun 2020
    Posts
    22
    Post Thanks / Like

    Re: Powcon 300 ST... Got a few questions before purchase

    Quote Originally Posted by Lafayette G View Post
    Your name plate seems to be in great shape. Could you take some hi res pics of it and post? My name plate was worn completely smooth. Would be nick to know max amps etc.
    Thanks,
    Dave
    The topic is five years old, I don't think anyone will answer you.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,634,442,578.95110 seconds with 13 queries