    I found a 47 short hood a year or so ago and am just starting to work on it but the exhaust manifold is broke. I have a newer parts machine { black face } It looks like the exhaust manifolds interchange ? Is that correct ?

  2. #2
    Join Date
    Dec 2013
    Location
    Pa
    Posts
    896
    Post Thanks / Like

    Re: Exhaust manifold

    Broke as in parts are missing? Or broke as in it can be repaired?
    Millermatic 211
    Miller Syncrowave 350lx with cooler and tigrunner
    Thermal Dynamics cutmaster 81
    1955 National Cylinder Gas O/A setup with original patina

  3. #3
    Join Date
    Mar 2015
    Posts
    248
    Post Thanks / Like

    Re: Exhaust manifold

    Well it has had a attempt to repair it once before and it was not a good attempt gonna take it off tomorrow am just checking out my options.

  4. #4
    Join Date
    Dec 2013
    Location
    Pa
    Posts
    896
    Post Thanks / Like

    Re: Exhaust manifold

    How are your welding skills? Grind the weld out and braze, stick, tig, or mig it to repair the manifold.
    Millermatic 211
    Miller Syncrowave 350lx with cooler and tigrunner
    Thermal Dynamics cutmaster 81
    1955 National Cylinder Gas O/A setup with original patina

  5. #5
    Join Date
    Mar 2009
    Posts
    3,554
    Post Thanks / Like

    Re: Exhaust manifold

    F162/F163 Continental will fit either or.

    This thread is from a couple of years ago so price of a new one has gone up from $100 to now $130ish for a new one. Or go with Duane's super awesome repair if you're that awesome. (I am not )

    http://weldingweb.com/vbb/showthread.php...61#post4660161
    "You can't out puke a buzzard"

  6. #6
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,396
    Post Thanks / Like

    Re: Exhaust manifold

    I think it was member castweld that pointed out a long time ago that older exhaust manifolds suffer from a significant loss of nickel from the cast iron due to heat degradation making it difficult if not impossible to weld or braze.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  7. #7
    Join Date
    Sep 2008
    Location
    Los Angeles
    Posts
    198
    Post Thanks / Like

    Re: Exhaust manifold

    Quote Originally Posted by duaneb55 View Post
    I think it was member castweld that pointed out a long time ago that older exhaust manifolds suffer from a significant loss of nickel from the cast iron due to heat degradation making it difficult if not impossible to weld or braze.
    I've never attempted it but am fascinated by guys like Fenner and Abom79 that show how it's done on cast repairs. I never knew about nickel loss. A good preheat and right filler I guess can't overcome this? The nickel actually leaches from the iron from long term use and heat cycles? Does it just sublimate from the surface? Something is tickling my memory, I think it was super-missile? Supposed to be a wonder filler for some things?

  8. #8
    Join Date
    Mar 2015
    Posts
    248
    Post Thanks / Like

    Re: Exhaust manifold

    Well as long as they interchange I will change it . Thanks . I have tried fixing and like Duane said I have found some of them impossible to weld and by the looks of the first repair I am going to assume that is the case Thanks again

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,638,788,520.50502 seconds with 13 queries