    Alternatives methods of joining of perpendicular thin steel sheet

    Name:  Lugged.jpg
Views: 250
Size:  24.7 KB

    Name:  Perp Weld.jpg
Views: 240
Size:  25.8 KB

    Hi I am researching alternatives methods of joining of thin perpendicular mild hardened or stainless steel sheet

    As the attachment describes I have a thin vertical 2mm steel sheet strips that has must be assembled perpendicular to the supporting horizontal plate of similar 2mm thickness
    This horizontal plate has had has receiving slots laser cut into it. The purpose of these slots is just to hold the perpendicular components in place.


    For the prototype I had joined these perpendicular pieces by extending the vertical strips past the horizontal plate to form lugs that I bent over against the horizontal surface
    This is quite strong but the protruding bent lugs present a problem on the outside and I would prefer to get rid of them.

    in mass production I had envisaged that I could weld these vertical strips into the slots from the outside (there is a lot of these vertical strips and slots closely spaced so access on the 'inside" is limited) perhaps by robot in a form of T weld from base but I was wondering if there is a better fabrication technique for this type of join that someone could suggest.

    I also would like these vertical strips to be as rigid as possible so was hoping to put them under tension thru the process any ideas ?

    Many thanks

  2. #2
    Join Date
    Mar 2015
    Location
    Milwaukee, WI
    Posts
    615
    Post Thanks / Like

    Re: Alternatives methods of joining of perpendicular thin steel sheet

    If the protrusion on the vertical piece is short, maybe it could be swaged in the opening like a rivet. That requires that tooling and maybe the geometry of your product doesn't allow this. Still, the swaged ends might look better than the protruding lugs.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,301,881.61358 seconds with 21 queries