    Forgot to turn on gas...bad?

    I just attached plug welded two pieces of 16 gauge mild steel together with my trusty mig welder, but I forgot to turn on the gas. It was popping and crackling more than normal, but I thought that's because I used weld-thru primer on the metal. Turns out I forgot to turn on the gas (75/25 argon/co2 normally).

    It's a single plug weld that holds a bracket to the underside of a battery box (box 16 gauge and sprayed with weld-thru primer).

    I ground down the weld and it looks shiny and normal once ground flush. But should I drill it out and start over? It's not structural per se (light little bracket, seems secure, etc.). Or it is a rust hole waiting to happen no matter how well I seal it up?

  2. #2
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,875
    Post Thanks / Like

    Re: Forgot to turn on gas...bad?

    Let's see a pics of what you tried to accomplish

  3. #3
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,209
    Post Thanks / Like

    Re: Forgot to turn on gas...bad?

    If it looks good leave it. Unless you de pressure your reg after turning off the bottle, there was likely enough pressure to make one decent plug weld.

  4. #4
    Join Date
    Aug 2013
    Posts
    76
    Post Thanks / Like

    Re: Forgot to turn on gas...bad?

    Well, I couldn't handle it and drilled it out. The weld looked "ok" (not great) on the outside after grinding, but I think the grinding essentially polished it to look better. The closer I got to the bottom piece, the more it looked like lava rock, and there was almost zero penetration. Live and learn.

  5. #5
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,285
    Post Thanks / Like

    Re: Forgot to turn on gas...bad?

    start over. It can't be good.

  6. #6
    Join Date
    Nov 2014
    Posts
    3,200
    Post Thanks / Like

    Re: Forgot to turn on gas...bad?

    LOL, usually when I forget to connect ground clamp I also next discover I forgot the gas. Call myself Sponge Bob rest of day and reach for grinder

    Mostly now in habit of first thing cranking open bottle, flipping welder to spoolgun and squeezing trigger 1 second foot of torch lead while I tweek gas flow...But sometimes forget where weld start great then Sponge Bob

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,196,490.76561 seconds with 13 queries