Page 1 of 3 123 LastLast
Results 1 to 25 of 67

Thread: The DEFINITIVE Welding Gas Costs Thread.

  1. #1
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    The DEFINITIVE Welding Gas Costs Thread.

    Click here to enter your welding gas cost information: ► Survey

    Then click here to view everyone else's responses: ► Responses
    Last edited by MinnesotaDave; 07-24-2019 at 03:17 PM. Reason: User requested
    1st on WeldingWeb to have a scrolling sig!



  2. #2
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    3,582
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Thanks for doing this. I entered my purchase of C25 from March of this year. Do you think there is any value to entering the date of the gas purchase? I have receipts going back a few years that I can enter if you want.
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  3. #3
    Join Date
    Apr 2014
    Location
    Illinois
    Posts
    3,309
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Thank you for taking the time to do this for everyone. I added my C25 purchase from May of this year and will add another entry next time I purchase acetylene.
    MM 211
    Smith Tru Lite O/A set, Thanks Bob!
    Lincoln AC-225
    --
    But you must not change one thing, one pebble, one grain of sand, until you know what good and evil will follow on that act. The world is in balance, in Equilibrium- Ursula K. Le Guin

  4. #4
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Quote Originally Posted by psacustomcreations View Post
    Thanks for doing this. I entered my purchase of C25 from March of this year. Do you think there is any value to entering the date of the gas purchase? I have receipts going back a few years that I can enter if you want.
    As far as the date, anything recent is good. "Going back a few years" would only be good if and only if a) the price is still valid and honored at that LWS at the time of the survey and b) one of the survey responses differs somehow from another entry of yours.

    For example: if the entry you just submitted was for a 125 tank of C25, but two years ago you purchased C25 fill for a 330 tank and the price at that LWS is still honored, then yes it would be a good submission at the time of the survey.

    It doesn't do anyone any good to see a response in the spreadsheet that you paid $15 for argon in 1987. That's not something that would legitimately be of any use to pretty much anyone looking to purchase argon in that area. Unless they still sell it for $15

    Also, I added C100 to the list in the survey, can't believe I forgot about that one.
    Last edited by Oscar; 07-03-2016 at 12:00 PM.
    1st on WeldingWeb to have a scrolling sig!



  5. #5
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Thanks to everyone who has submitted their info.

    I did delete the Seneca, SC row in the Responses Spreadsheet because the NAME of the LWS was not input. Please submit again with the NAME of the place. Please remember, this is to HELP people who are potentially wanting to buy welding gases. Of what good is it to those people if they see "LWS" in the name column? Thanks for your understanding. IF by some weird chance, the name of the LWS is actually "LWS", then I apologize and will re-insert that row.
    1st on WeldingWeb to have a scrolling sig!



  6. #6
    Join Date
    Jun 2016
    Posts
    13
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Great idea, I put in all my gas purchase for the last year. I am looking forward to see what info pops up.

  7. #7
    Join Date
    Jun 2015
    Location
    The wheat fields of Kansas,in a large metal building
    Posts
    311
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    While the time stamp is OK, an actual purchase month/year would be helpful. I added my two recent refills from last week, that could be old news in a year.
    Steve from SoCal now in Hutch

    Miller Dynasty 300DX Coolmate3 Speedway Torch
    Miller XMT 450 MPa plus with D-74 MPa Plus
    Miller Bobcat 225 NT
    Hypertherm Powermax 45
    And a whole bunch of machines

  8. #8
    Join Date
    Jan 2008
    Location
    Lansing, MI
    Posts
    6,117
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    I'll make this a sticky Oscar. I've been out almost all day.

    Let me know if you need anything from me on this. I'm gonna be pretty busy over the next week so if I don't get right back with you that's why.

  9. #9
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Quote Originally Posted by Steve from SoCal View Post
    While the time stamp is OK, an actual purchase month/year would be helpful. I added my two recent refills from last week, that could be old news in a year.
    That's ok. They're supposed to be old news in a year. Because the whole point of this is to keep it open forever, so long as it doesn't reach some kind of storage space limit with Google. When you filter it by state, scrolling down to the current date should be relatively quick.
    1st on WeldingWeb to have a scrolling sig!



  10. #10
    Join Date
    Feb 2015
    Location
    Austin, TX (now) -- Boston, MA (then)
    Posts
    270
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Very cool - added my fill costs.
    Millermatic 211 w/Spoolmate 150
    Hypertherm PMX45XP

    Wishlist:
    HTP Invertig 221

  11. #11
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Thanks for your entries. Its starting to look real good and it's interesting to quickly see what everyone else is paying in different areas.
    1st on WeldingWeb to have a scrolling sig!



  12. #12
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Let's get some more surveys submitted! I know that there's more than 40 welders on this forum! Thanks to those who have contributed.
    1st on WeldingWeb to have a scrolling sig!



  13. #13
    Join Date
    Feb 2012
    Posts
    4,442
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    I was paying $40 for 150cf of Argon. The last refill went up to $62. They even tried to give me a bottle with a neck ring. It said customer owned but also had the name of there old bizness on it. My LWS sold out to PRAXAIR. Is PRAXAIR good or bad?

  14. #14
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Quote Originally Posted by Insaneride View Post
    I was paying $40 for 150cf of Argon. The last refill went up to $62. They even tried to give me a bottle with a neck ring. It said customer owned but also had the name of there old bizness on it. My LWS sold out to PRAXAIR. Is PRAXAIR good or bad?
    I don't see your entry.
    1st on WeldingWeb to have a scrolling sig!



  15. #15
    Join Date
    Apr 2014
    Location
    Illinois
    Posts
    3,309
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Do me a favor please.... I just added another entry and screwed up. Thought I checked C25 and in looking at it, I see my purchase is appearing as 100% argon. Everything else is correct. That just needs to be changed to C25. Sorry about that.
    --
    And when you have a spare moment, how do I filter results to see what others are paying in my state?
    MM 211
    Smith Tru Lite O/A set, Thanks Bob!
    Lincoln AC-225
    --
    But you must not change one thing, one pebble, one grain of sand, until you know what good and evil will follow on that act. The world is in balance, in Equilibrium- Ursula K. Le Guin

  16. #16
    Join Date
    Jun 2015
    Location
    Texas
    Posts
    11
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Apparently my phone corrected austin to a austin a and there is no option for 60 cuft.

  17. #17
    Join Date
    Aug 2016
    Posts
    33
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Purchased 80 cubic ft tank from Arc3 in Durham, NC for 155.92 and cost to fill with 100% argon was 13.16. I think the guy range me up wrong but not complaints from me!

    Added the fill cost to the sheet but no option to add just tank cost.

  18. #18
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    most places sell tanks already full, that's why there's no option. Never hear of anyone wanting to buy a tank of welding gas at the LWS, that was completely empty. What you can do is post the cost of the tank + gas in one entry, and then in another entry, post the cost of the refill only, even if you didn't actually buy the refill. Using subtraction, a decently intelligent individual would be able to figure out the raw cost of an empty tank if necessary for what ever reason.

    While there may not be an option for a 60 cuft'er, it is also not meant to be an all-inclusive list. Simply picking something close should get someone new who has no idea what is what, into the ballpark. It's not for me to know what you're buying for my purposes. It's to help others near your area who may want to see what to get where, and near what price. Oh, and I fixed the "Austin".
    Last edited by Oscar; 09-07-2016 at 08:21 PM.
    1st on WeldingWeb to have a scrolling sig!



  19. #19
    Join Date
    Jun 2015
    Location
    Texas
    Posts
    11
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Quote Originally Posted by Oscar View Post
    most places sell tanks already full, that's why there's no option. Never hear of anyone wanting to buy a tank of welding gas at the LWS, that was completely empty. What you can do is post the cost of the tank + gas in one entry, and then in another entry, post the cost of the refill only, even if you didn't actually buy the refill. Using subtraction, a decently intelligent individual would be able to figure out the raw cost of an empty tank if necessary for what ever reason.

    While there may not be an option for a 60 cuft'er, it is also not meant to be an all-inclusive list. Simply picking something close should get someone new who has no idea what is what, into the ballpark. It's not for me to know what you're buying for my purposes. It's to help others near your area who may want to see what to get where, and near what price. Oh, and I fixed the "Austin".
    Thanks, I figured 55 was close enough. Just figured I would point out where it had gaps.

  20. #20
    Join Date
    Sep 2016
    Location
    Southern Michigan
    Posts
    14
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Thanks for taking the time to set this up Oscar! I will fill out my gas purchases later this week when I have my receipts handy!
    Old Welders (at work)
    Miller Deltaweld 452
    Miller Syncrowave 250
    Lincoln 180c powermig
    Current Welders (at work)
    Millermatic 252
    Millermatic 350
    Miller Syncrowave 250DX
    My Welders
    CE Dual Mig 170
    CE Inverter Arc/Tig

  21. #21
    Join Date
    Sep 2016
    Location
    Southern Michigan
    Posts
    14
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    FYI....When filling out my gas costs I noticed there's no option for 60cf tanks....I selected 75cf and made a note of 60cf in the cost section.
    Old Welders (at work)
    Miller Deltaweld 452
    Miller Syncrowave 250
    Lincoln 180c powermig
    Current Welders (at work)
    Millermatic 252
    Millermatic 350
    Miller Syncrowave 250DX
    My Welders
    CE Dual Mig 170
    CE Inverter Arc/Tig

  22. #22
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    6,668
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Quote Originally Posted by strokedbronco View Post
    FYI....When filling out my gas costs I noticed there's no option for 60cf tanks....I selected 75cf and made a note of 60cf in the cost section.
    Yep, that will work. Its enough info that one can get a reasonable idea of what is available if they are searching in your area.
    1st on WeldingWeb to have a scrolling sig!



  23. #23
    Join Date
    Nov 2016
    Posts
    21
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Please update the spreadsheet to include #60 bottles..................
    Miller CST 280
    MillerMatic 211
    Lincoln Square Wave 200
    Oxy-A Big & Small Tanks/Torches
    ESAB Plasma Cutter

  24. #24
    Join Date
    Oct 2011
    Location
    Hamlin, NY
    Posts
    1,279
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    Bump. I just added a few recent bottles refills. Keep it going!
    Ryan

    Miller Multimatic 200 tig/spool gun/wireless remote
    Millermatic 350P, Bernard/XR Python guns
    Miller Dynasty 350, Coolmate 3.5 & wireless remote
    CK WF1 TIG wire feeder
    Miller Spectrum 375 Xtreme
    Optrel e684
    Miller Digital Elite
    Miller Weld-Mask

  25. #25
    Join Date
    Dec 2016
    Location
    New Jersey
    Posts
    220
    Post Thanks / Like

    Re: The DEFINITIVE Welding Gas Costs Thread.

    well - great info - re-affirming I am overpaying!!!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments