Re: The DEFINITIVE Welding Gas Costs Thread.
Thanks for starting this,, whenever that was,,,
I went to several welding supplies,, and I was shocked at the variation in pricing,,
I asked about 80 Cu Ft argon, and 80 Cu Ft 75-25 as I have those two tanks
I was quoted between $27 and $58 for each tank,, I did ask one place about filling my CO2 tank,, that was $25,,
I forgot to ask the other places about the CO2,,
I will enter data when I do get the tanks filled,,,
-
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I went today to swap my (owned) 125 argon at Airgas. The guy rang me up and said that will be $78. Huh? I asked if the price went up, I got a refill just two weeks ago and it was $61. He checked again, and said "ya, its $61". Makes me wonder if there are different price lists.
I entered it in the survey, the prices sure are all over the board.
Miller Dialarc 250
Hobart 140
HTP 220 MTS
Miller Legend AEAD 200LE Gas drive
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Originally Posted by
KenO
I went today to swap my (owned) 125 argon at Airgas. The guy rang me up and said that will be $78. Huh? I asked if the price went up, I got a refill just two weeks ago and it was $61. He checked again, and said "ya, its $61". Makes me wonder if there are different price lists.
I entered it in the survey, the prices sure are all over the board.
There usually are different prices.
Sincerely,
William McCormick
If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
T-tanks cost me $70
Sincerely,
William McCormick
If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Originally Posted by
KenO
I went today to swap my (owned) 125 argon at Airgas. The guy rang me up and said that will be $78. Huh? I asked if the price went up, I got a refill just two weeks ago and it was $61. He checked again, and said "ya, its $61". Makes me wonder if there are different price lists.
I entered it in the survey, the prices sure are all over the board.
It's called tiered pricing. Sucks if you aren't a bulk/big buyer.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Over the years I have talked to the guys at the big and small liquid carbonic plants and they pretty much told me to get the big tanks because they do not care about the gas as much as the aggravation and handling of the tanks. The smaller tanks pose problems for transporting and the large refillers charge the smaller distributors almost the same price whether it is small or large.
Sincerely,
William McCormick
If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Originally Posted by
KenO
I went today to swap my (owned) 125 argon at Airgas. The guy rang me up and said that will be $78. Huh? I asked if the price went up, I got a refill just two weeks ago and it was $61. He checked again, and said "ya, its $61". Makes me wonder if there are different price lists.
I entered it in the survey, the prices sure are all over the board.
Oh there definitely is different price list. Cash is 3 times a account holder price.
You are still getting robbed. 125 argon should be about $28 out the door price.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I'm envious as all hell of how cheap gas is in the states.
Here in Australia we get robbed blind since there is a duopoly for gas supply, BOC and supagas.
A 120 CuF of argon is $159 just for the gas here, same size of Co2 is $120.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Today I swapped out a 150 Argon, $30. for gas $0.35 surcharge for 150 cylinder and $2.28 tax total $32.63 North Fla.
DIY CNC Plasma table USB BOB Price THC
Hypertherm 65
Everlast PowerTig 255 EXT
Miler 180 Mig
13" metal lathe
Mill/ Drill
ECT, ECT,
-
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I have now sorry for the flub up
DIY CNC Plasma table USB BOB Price THC
Hypertherm 65
Everlast PowerTig 255 EXT
Miler 180 Mig
13" metal lathe
Mill/ Drill
ECT, ECT,
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I just swapped a 155 argon ( $66) and a 75 acetylene ($76) , put them in the data base too- seems like not too many entrys for 2022 yet- the cost seemed high but everything is going through the roof. Hard to judge a price increase with inflation raging. Filled up the van, 87 octane was 4.55, diesel is 4.99.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Good call. Things are changing rapidly now a days. Would be quite useful if everyone doing recent transactions recorded their figures in the spreadsheet.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Originally Posted by
Oscar
Good call. Things are changing rapidly now a days. Would be quite useful if everyone doing recent transactions recorded their figures in the spreadsheet.
I saw an interesting headline yesterday,
People now earning $15 an hour have less buying power than they did a year ago when earning $7.50 an hour.
Earning double does nothing when prices have tripled, or more,,,,,,,
This raising of minimum wage may just bankrupt the country,,,,,,,,,,,
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I put gas price in the survey (not bottle price). I didn’t actually buy a bottle but put it in based on a quote.
April 2022
124cf $231 for the bottle
C25 gas $81
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I rent the cylinders as they won’t fill customer cylinders over 80cf around here. $75 per cylinder per year. Just at home I have 6 damn cylinders. Just exchanged a small argon the other day was $78 for the gas and they added a hazardous material fee of $10 almost $90 for a small 155cf argon! I don’t know what we are paying at work as they don’t put a price on the invoice for a commercial account? I’m biting my tongue on my big 300 cf acetylene cylinder swap price. I’ll post the price next week when I swap it.
-
-
Re: The DEFINITIVE Welding Gas Costs Thread.
You might add a button for type of discount. For me, a student discount gets approximately $100 off on a 225 bottle of argon!
Millermatic 255
Everlast Typhoon 330
Ready Welder I
Hypertherm 30XP
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Originally Posted by
robert-r
You might add a button for type of discount. For me, a student discount gets approximately $100 off on a 225 bottle of argon!
Oops - that's a 220CuFt bottle.
Millermatic 255
Everlast Typhoon 330
Ready Welder I
Hypertherm 30XP
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I called here in Indiana to the local Air gas. The MC sized Acetylene and oxygen tanks here both together cost $79.78 to refill.
*B tank sized Oxgen tank will cost $56.80 and similar price for the Acetylene (just one tank not two/ each).
I will have B tanks as soon as I can purchase some used that are not rented but bought outright.
Going to shop around though for prices.
-
Re: The DEFINITIVE Welding Gas Costs Thread.
I had my 75 cu ft acetylene tank filled for $61 tax and all. I think the gas alone was around $57 or so. In Oklahoma at LWS.
-
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Oscar we need current dates since the post epidemic prices skew the statistics. No?
Price of a 330cf for acetalyne doesn't jive. Do they even make 330ft acete tank?
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Originally Posted by
Insaneride
Oscar we need current dates since the post epidemic prices skew the statistics. No?
Price of a 330cf for acetalyne doesn't jive. Do they even make 330ft acete tank?
Oops, the date is at far left. My device doesn't show the whole spreadsheet without scrolling
I still don't get 330cf acetalyne . Is that real?
-
Post Thanks / Like - 1 Likes, 0 Dislikes
-
Re: The DEFINITIVE Welding Gas Costs Thread.
Originally Posted by
Insaneride
Oops, the date is at far left. My device doesn't show the whole spreadsheet without scrolling
I still don't get 330cf acetalyne . Is that real?
https://www.unitedrentals.com/market...5-330-cubic-ft
Sent from my Lincoln Buzzbox using Tapatalk
Sent via smoke signals using my Lincoln buzzbox
-
Post Thanks / Like - 1 Likes, 0 Dislikes