    Re: cutting railroad rail -plasma / band saw? need some advice

    You line the track up on the edge of your table and tack weld hangers from the bottom of your table out past the table were you will be able to sit the rail lower and parallel to the the track. Lower obviously to get height adjustment out of the torch head. Parallel so you can cut it long ways. I do it all the time when I split 5*5 Solid hex bar for jobs. I will try and set it up so you can get a visual.

  2. #27
    Join Date
    Nov 2006
    Posts
    6,088
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    Quote Originally Posted by bfastwelder View Post
    You line the track up on the edge of your table
    . . . Parallel so you can cut it long ways.
    I think that Gator wants to cut perpendicular to the flange, not parallel.
    Which of course the perpendicular cut brings up lots of issues for any "hot" cut method.

    Quote Originally Posted by gator9329 View Post
    . . . I need to cut an 8" railroad rail in half (two 4" sections). I am making book ends. . .

  3. #28
    Join Date
    Nov 2011
    Location
    Wakefield, MA
    Posts
    138
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    OK here's an update. I tried to do it on my 14 inch chop saw. tried: (verb) not sucessful at ... I got half way through it and hit the thick webbing. It was taking a long long time time. I am going to the steel ditributor down the road with a case of beer a pocket full of cash. hopefully they will just put it on the big band saw for me.
    Thanks for the advice guys, will post pictures when done.

  4. #29
    Join Date
    Dec 2011
    Location
    Colma, CA
    Posts
    313
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    Call your closest welder I'm sure they will be glad to cut it for a couple bucks!
    AEAD 200LE, Lincoln precision tig 185, Millermatic 251, Spectrum 625 extreme, Victor torch , Smithy 1220LTD. and Do all C-4 band saw , Always adding.

  5. #30
    Join Date
    Mar 2009
    Location
    MN
    Posts
    5,219
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    Quote Originally Posted by gator9329 View Post
    OK here's an update. I tried to do it on my 14 inch chop saw. tried: (verb) not sucessful at ... I got half way through it and hit the thick webbing. It was taking a long long time time.
    You probably got the blade too hot and it glazed over. You need to cut thick stuff in short spurts. Lean on it, back off, lean on it, back off....
    My name's not Jim....

  6. #31
    Join Date
    Sep 2006
    Location
    Marlborough, The Peoples Republik of MA
    Posts
    3,549
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    I did a big RR track scrapping job a few years ago, oxy propane, with a bulldog tip, and it was like cutting butter.
    Disclaimer; "I am just an a$$hole welder, don't take it personally ."

  7. #32
    Join Date
    Feb 2008
    Location
    North of Philly
    Posts
    20,159
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    Quote Originally Posted by Boostinjdm View Post
    You probably got the blade too hot and it glazed over. You need to cut thick stuff in short spurts. Lean on it, back off, lean on it, back off....
    That's my guess exactly to what happened. If the blade gets loaded up and glazed over, some times if you pull the material out and cut some thin vertical stock or even a brick it will "clean" up the blade. All you want to do is get the top layer of the blade to wear off and expose some clean material. After that you will find the blade cuts fine as long as you don't glaze the blade again.
    .



    No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth!

    Ronald Reagan

  8. #33
    Join Date
    Apr 2004
    Location
    Maryland
    Posts
    718
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    I regularly cut railroad track. I run the amada (ellis bandsaw brand blades) blades in my 1974 rockwell bandsaw. Just put the blade on slow with a slow feed rate. Coolant is a must. I can cut 115lb rail in less than 3 minutes. I probably have cut at least 50 pieces of track this way.
    Lincoln
    300 Vantage 2008
    300 Commander 1999
    SA250 1999
    SA200 1968

    Miller
    Syncrowave 200
    XMT350MPA/S-52E/xr-15
    Xtreme 12vs
    Millermatic 251 w/30A
    Millermatic 251
    Dialarc 250

    Hypertherm 1250
    GEKA & Bantom Ironwokers

  9. #34
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,329
    Post Thanks / Like

    Re: cutting railroad rail -plasma / band saw? need some advice

    You may have gotten your track cut already, but for future reference, you can cut track surprisingly easily with zip wheels. It takes 2-3 wheels, but for a single cut, very little cleanup afterward, and very little equipment, it is a very good way to do it.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,833,537.98457 seconds with 13 queries