Hi, this my first post hopefully in the right forum. Anyway I have 95 225g plus with 937 hrs, every thing works fine except for the constant voltage,when selected it puts out about 42 volts and will not adjust lower with the fine adjust. And when in the cc mode the current adjusts as it should. Also just incase its related the idle soleniod doesn't work unless i work the ignition switch back and forth fron run to idle. I'd appreciate any input anyone may have, THANKS,"RODBUSTER"