    I have the Miller 125c.

    Put in new electrode and it won't fire up correctly.

    Put in the old one and it works just fine.


    Simple piece of copper- can't see why the new ones won't work.



    Correct part number on packaging and they look identical.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  2. #2
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    5,754
    Post Thanks / Like

    Re: Plasma cutter electrode ?

    I believe you're mistaken. There is a [usually] hafnium-based electrode in the center of the copper tip.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  3. #3
    Join Date
    Jan 2013
    Location
    ...Shoulder of Orion...
    Posts
    3,509
    Post Thanks / Like

    Re: Plasma cutter electrode ?

    @ Broccoli - never ran that cutter you have. This is the Miller 196925 electrode you need for your 125C plasma cutter.

    Electodes are mostly Cu, with an axial "button" emitter of Hf, for cutter systems.
    Last edited by ManoKai; 10-21-2016 at 04:43 PM.
    "Discovery is to see what everybody else has seen, and to think what nobody else has thought" - Albert Szent-Gyorgyi

  4. #4
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    8,223
    Post Thanks / Like

    Re: Plasma cutter electrode ?

    Yup
    That's the part I got.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  5. #5
    Join Date
    Jun 2004
    Location
    NE Oregon
    Posts
    367
    Post Thanks / Like

    Re: Plasma cutter electrode ?

    Genuine OEM and not aftermarket?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,395,194.02376 seconds with 11 queries