    I bumped a tree limb with my tractor last week and put a crack in the fairly new muffler, which is aluminized steel.
    Can the aluminum plating (I'm assuming that is how it is done) be ground off and then the steel welded? I'm using ER70S6 wire and 75/25 gas.

  2. #2
    Join Date
    Oct 2007
    Location
    Near Dayton, OH
    Posts
    2,497
    Post Thanks / Like

    Re: Aluminized muffler

    yes you can do what you said. Maybe a flap disk or scotchbrite wheel will be good enough to strip the aluminum without making the metal underneath any thinner that it already is.
    Benson's Mobile Welding - Dayton, OH metro area - AWS Certified Welding Inspector

  3. #3
    Join Date
    Jul 2007
    Location
    Murphysboro, IL
    Posts
    204
    Post Thanks / Like

    Re: Aluminized muffler

    I should have clarified, I was thinking a flap wheel or scotch brite pad on a grinder and not an aluminum oxide grinding wheel.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,108,416.12619 seconds with 13 queries