    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    This is a plow problem prevention post..
    Truck....
    Name:  20161209_125501.jpg
Views: 718
Size:  80.1 KB

    Now with most Fisher set ups you have a safety chain or some call it the over the road chain.
    Nice to have but not the ideal set up from the factory.
    The chain slack constantly gets caught between the angle piston and the A frame.
    Constant crushing can cause angle piston failure.
    To combat that all you need is a heavy duty spring and 2 attaching gizmos that I can't recall what they are...
    Name:  20161209_125414.jpg
Views: 722
Size:  87.3 KB

    Chain stays out of the way but will have the "strech" needed for those downhill adventures while the plow is in "Float" mode.

    Works great!..


    ...zap!


    I am not completely insane..
    Some parts are missing

    Professional Driver on a closed course....
    Do not attempt.

    Just because I'm a dumbass don't mean that you can be too.
    So DON'T try any of this **** l do at home.

  2. #52
    Join Date
    Nov 2016
    Location
    North NJ
    Posts
    12
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Had to re-skin the board of a 8ft Fisher. one piece of 10 gauge brake bent.
    Attached Images Attached Images    

  3. #53
    Join Date
    Jan 2015
    Location
    Minnesota
    Posts
    18
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    These are from last year, but i've done the same thing half a dozen times this year too. Just extending the wing to match new cutting edge.

    Name:  20150107_152851.jpg
Views: 511
Size:  31.8 KBName:  20150107_152515.jpg
Views: 510
Size:  103.0 KBName:  20150107_163246.jpg
Views: 510
Size:  30.2 KBName:  20150107_164449.jpg
Views: 505
Size:  143.1 KB

  4. #54
    Join Date
    Jan 2015
    Location
    Minnesota
    Posts
    18
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Same thing, also from last year, but with a new 1/2 plate behind the cutting edge, which is how I usually do it.
    Name:  20151120_111416_LI.jpg
Views: 502
Size:  65.7 KBName:  20151120_110109.jpg
Views: 507
Size:  33.4 KBName:  20151120_111359.jpg
Views: 505
Size:  56.1 KBName:  20151120_120437_LI.jpg
Views: 503
Size:  57.4 KB

  5. #55
    Join Date
    Jun 2013
    Location
    BIG SKY COUNTRY
    Posts
    645
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Snowplows
    Always something broken, or about to.

    Front end feels light... OK, found the problem.
    Name:  IMG_0656.jpg
Views: 471
Size:  75.3 KB
    Name:  IMG_0655.jpg
Views: 466
Size:  67.3 KB

    Rig it up however, haul it back to the shop.
    Name:  IMG_0659.jpg
Views: 472
Size:  70.9 KB
    Hobbyist - At what point is a "hobby" out-of-control?

  6. #56
    Join Date
    Jun 2013
    Location
    BIG SKY COUNTRY
    Posts
    645
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Nosepiece broken & rewelded several times, A-frame ends fatigued. Time for a more serious repair. Chopped, spliced, ground.
    New pivot plates, longer length to reach fresh metal.
    Cleaned well, then multipassed with 7018.

    Name:  IMG_0716.jpg
Views: 518
Size:  60.7 KB
    Name:  plow2.jpg
Views: 481
Size:  51.5 KB
    Name:  rebuilt nose.jpg
Views: 485
Size:  48.9 KB

    Name:  finished.jpg
Views: 477
Size:  70.9 KB

    Let it snow, let it snow, let it snow....
    Hobbyist - At what point is a "hobby" out-of-control?

  7. #57
    Join Date
    Sep 2016
    Location
    Near Traverse City, Mi.
    Posts
    348
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Anyone familiar with the Boss VXT?

    I am replacing my A - Frame, not repairable and $300 and change for a new one is money well spent.

    However, the bushing the pin slides through to hold the A-Frame to the center section appears to have a partially cracked weld. I was thinking of grinding out the old weld where its broke and re-welding while the pin is inserted to keep it aligned. Make sense? Or do I repair the weld without the pin in and then ream?
    Miller Dynasty 280 DX, Lincoln 210 MP

  8. #58
    Join Date
    Sep 2016
    Location
    Near Traverse City, Mi.
    Posts
    348
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Well, welded it up with the pin in it. I dare say it slides in and out easier.
    Miller Dynasty 280 DX, Lincoln 210 MP

  9. #59
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    14,972
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    I love it when a plan comes together...
    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Vevor MIG 200A
    Victor Medalist 350 O/A
    Vevor Cut 50 Plasma
    Les

  10. #60
    Join Date
    Feb 2022
    Posts
    25
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Hi
    My friend made a plow for my skid steer out of an old tractor 3pt hitch grader.
    The plow was below the attachment plate which was causing damage to the skidsteer arms.
    I've since got my own welder (last year)and started to modify/improve the design the plow.
    I've been looking at plow design and notice the all have springs/give.
    Is there any point to working on this plow, or should I start over?
    The skidsteer is a mini.
    Any advice is welcome, thank you

    Sent from my SM-G950W using Tapatalk

  11. #61
    Join Date
    Jun 2008
    Location
    Hardwood Lands, Nova Scotia, Canada
    Posts
    2,684
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Gonna be hard on gear with no trip springs for sure.

  12. #62
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,585
    Post Thanks / Like

    Re: Official Snowplow Repair Thread! Post Up Your Repairs And Pics!

    Any loader based plow has geometry not conducive to plowing in float. The angle of push frame to ground makes the machine want to act like a pole vaulter. When the blade catches, the tractor tries to climb over it.

    Only successful plow used on a loader frame must lock the loader in a position close to the ground. Plow then pivots from there. All plows need a trip mechanism. Snow pushers use only a flexible cutting edge. It folds to pass over an obstacle.

    Another problem of loader mounted snow plows is the inability to tilt to conform to the discrepancy between tractor & grade. Snow pushers tilt up to 4" each side to conform. Pickup mounted plows are a bit sloppy for the same purpose.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,239,699.78433 seconds with 21 queries