    Aluminum Chainsaw Storage Boxes

    I had some extra aluminum lying around, needed practice on aluminum outside corners and wanted a couple heavy duty chainsaw boxes for 2 chainsaws I carry on my ATV so .... These are 1/8" 5052 aluminum, I scored the joints with my circular saw, bent them manually over a table edge, and then welded them with my Everlast 255EXT. Specs for welding were ~110a on outside corners (~125a to 130a at beginning then lowered as metal got warm), no pulse, 3/32" tungsten and 5356 filler, 3 sec upslope and 3 sec down using an on/off torch switch and slope to control heat. Handles were made with some tubing and a couple pieces of plate. Aluminum hinges were purchased and welded on. Fun project, lots of TIG seat time, welder performed flawlessly.

    Name:  IMG_5165[2].jpg
Views: 2036
Size:  56.8 KB Name:  IMG_5159[1].jpg
Views: 2573
Size:  60.8 KBName:  IMG_5158[1].jpg
Views: 1956
Size:  48.6 KBName:  IMG_5163[2].jpg
Views: 1771
Size:  49.3 KB
    Last edited by Shipj0; 12-07-2016 at 10:46 AM.

  2. #2
    Join Date
    Apr 2015
    Location
    N 48° 38.680 W 080° 40.837
    Posts
    1,262
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Nice work!!

  3. #3
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Those look like they came out nice! Should stay safe in the boxes when trees are falling

  4. #4
    Join Date
    Nov 2016
    Location
    detroit
    Posts
    4
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Very nice work!!

  5. #5
    Join Date
    Apr 2011
    Location
    Dirty Coast
    Posts
    18
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Very cool! Tell us more about your sander/polisher. Never seen one like that.

  6. #6
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Nice job.

    Is there enough room to keep a plastic bar cover on ??

    If not, I'd be worried about the teeth making contact with the alum.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  7. #7
    Join Date
    Feb 2016
    Location
    Myrtle Beach
    Posts
    899
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Nice job I want to know about polisher also. I've seen them never used one.
    Lincoln 350MP
    Millermatic 350P
    Syncrowave 250
    1969 SA200
    HTP Invertig 221

  8. #8
    Join Date
    Nov 2004
    Location
    Southern Montana
    Posts
    1,081
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Quote Originally Posted by John T View Post
    Nice job.

    Is there enough room to keep a plastic bar cover on ??

    If not, I'd be worried about the teeth making contact with the alum.
    Are you worried about the teeth or about the aluminum?

  9. #9
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  10. #10
    Join Date
    Apr 2016
    Location
    CA
    Posts
    12,118
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Nice work. My initial thought is how hard is it to get it in there then I noticed that the blade cover slips on the blade before stored in the box. So after that I looked closer. I was like I wonder if it has a tendency of the blade cover bending upward from the bottom. Do you have a clip that sits on the inside of the box to keep it from bending up?
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  11. #11
    Join Date
    Aug 2015
    Location
    Alaska
    Posts
    84
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Thanks for all the compliments in the chainsaw boxes. The surfacing tool is a SCT by Eastwood. Good price on the tool and the extra drums, way better than similar tools by other manufacturers . Comes with the Red surfacing drum, which works well for Aluminum. Eastwood also has a sanding drum with sandpaper and a stripping drum. I have not tried either with aluminum; I have the stripping drum but looks pretty course for aluminum. The only issue I had was shipping to AK was expensive, to States in the Lower 48 shipping is probably a lot cheaper.

    http://www.eastwood.com/eastwood-contour-sct.html
    Last edited by Shipj0; 01-24-2017 at 04:41 AM.

  12. #12
    Join Date
    Aug 2015
    Location
    Alaska
    Posts
    84
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    When the chainsaw is in the box, the chain does not generally touch the aluminum. The clearance and angle was set up to keep the bar centered in the sleeve. There is not room for the plastic sleeve but I could cut up one of those flexible thin plastic cutting boards and glue it in if I thought it was needed. I am sure in a good hit or bump that the chain could contact the aluminum but figured the steel teeth would not be hurt by the aluminum. I will look for a photo of how the sleeve is held in place in the box to keep the sleeve from moving around. Basically, the bar sleeve has two plates spaced apart far enough to slide over the aluminum box that holds the sleeve from both sides. Thought through lots of options and this was the best I could come up with to make it easy to get the saw in and out. Was actually shooting for a narrower box but miss measured by about an inch. Decided to just leave it for now. Plastic box from Home Depot is $29.99, way cheaper and quicker if I didn't have spare aluminum lying around from another project but this was way more fun.

  13. #13
    Join Date
    Aug 2015
    Location
    Alaska
    Posts
    84
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    To make the box, I cut out the aluminum in a cross shape to the box size for the bottom and sides, scored the aluminum with a skil saw and then bent the sides over a bench to meet at the edges then TIG welded them together. This gave me lots of practice with outside corners, which was one of the goalS. I could have saved on some welding by bending the box instead of welding but would have had to have it done at a shop and the point was welding practice. Tops were done the same way. On one, I sanded off the welds, on the other, I left them. Not that I was thinking of it at the time but it lets me ID which saw I am grabbing without opening. Same saws but one has normal bar oil and is used for general cutting around the house, other has vegetable oil for bar oil and is used on moose hunts to cut camp wood and (with a little luck) cut up moose.

  14. #14
    Join Date
    Aug 2015
    Location
    Alaska
    Posts
    84
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Here are the pix of how the bar sleeve fits the box.

    Name:  IMG_1101.jpg
Views: 832
Size:  32.9 KB

    Name:  IMG_1102.jpg
Views: 830
Size:  68.1 KB

  15. #15
    Join Date
    Apr 2016
    Location
    CA
    Posts
    12,118
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Looks great.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  16. #16
    Join Date
    Aug 2015
    Location
    Alaska
    Posts
    84
    Post Thanks / Like

    Re: Aluminum Chainsaw Storage Boxes

    Quote Originally Posted by N2 Welding View Post
    Looks great.
    Thanks, appreciate it.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Tags for this Thread

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,291,695.47601 seconds with 19 queries