    Newbie question: Mystery welder

    Hello everyone. I am a very inexperienced welder but I am eager to learn to be more proficient! That being said I know very little. I was recently given a 220V Arc/Tig machine. I was told it was a german preproduction model. It has absolutely no markings or brand names anywhere inside or outside. I have the arc welding leads but I would like to get the Tig leads for it. I already have an argon setup waiting to attach. I attached a photo pf the front plate and if necessary I can pull it out and get outside/inside shots of the rig. Can anyone identify it or what setup I would need to complete the tig setup? Im assuming from the front plate it is a scratch start setup? It also has a wiring diagram on the inside cover if that would help identify it. Thanks guys for the advice ahead of time! The metal and hose in front of the welder is the motor being rebuilt for my Samurai Crawler project!

    Name:  welder.jpg
Views: 456
Size:  57.2 KB

  2. #2
    Join Date
    May 2011
    Location
    Andover, Ohio
    Posts
    2,568
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    Welcome...
    Lincoln A/C 225
    Everlast P/A 200

  3. #3
    Join Date
    Dec 2015
    Posts
    1,392
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    Yeah,

    Interesting!

    It looks like it may not have a gas solenoid for TIG. But there is what looks like a remote outlet plug for a pedal or contactor switch, which may mean that it could have a high frequency TIG start ability. And a foot pedal will take a 5-wire plug, at a minimum.

    Is there a gas inlet barb or fitting at the back of the machine?

    If not, you'd need a TIG torch with a gas valve on it, which are easy to find.

    Have you struck an arc with the Stick leads to ensure it functions?

  4. #4
    Join Date
    Feb 2012
    Posts
    4,442
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    It goes to 400 amps? Is it a 3 phase machine?

    As mentioned by C Livingstone; you probly need a torch with a valve. A close up of the remote connector might help identify the connector you need for remote use but you could use it as a scratch start in SMAW mode.

  5. #5
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,123
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    How about ESAB LHF 400? 3-phase, requires 400-550V power. (EDIT: For some other markets, maybe 220 or higher.)

    Name:  tig-welding-machine.jpg
Views: 325
Size:  24.4 KB

    Name:  shapeimage_2.png
Views: 339
Size:  41.8 KB

    http://www.esabasia.com/asia/en/prod...uctCode=430015

    Link to the manual: http://www.esab.com/gb/en/support/up...800-070108.pdf Here's a different manual that includes the 230V input wiring: http://valvolodin.narod.ru/schems1/L...630-LHF800.pdf

    Name:  ESAB_LHF_400_Welder.jpg
Views: 318
Size:  49.6 KB
    Last edited by Oldendum; 01-18-2017 at 11:39 AM.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  6. #6
    Join Date
    Dec 2015
    Posts
    1,392
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    Oh,

    It's a match!

    The ESAB literature, doesn't give much information, but does state an optional HF box was available, not that I'd try to look for one today.

    So, is yours 1-phase, 220 volt, unlike the ESAB branded ones?
    Last edited by C. Livingstone; 01-18-2017 at 11:42 AM.

  7. #7
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,123
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    Hopefully the wiring diagram on the inside cover will show the proper connections for power. I seriously doubt that it is a single-phase unit.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  8. #8
    Join Date
    Dec 2015
    Posts
    1,392
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    Yeah,

    I'm guessing it's not either.

    I mean, if it is, it would undoubtedly have to be a high-amp 220-240 volt circuit, with a fat cord to output 400 amps. But, most things electrical are above my so-called pay grade.


    Quote Originally Posted by Oldendum View Post
    Hopefully the wiring diagram on the inside cover will show the proper connections for power. I seriously doubt that it is a single-phase unit.

  9. #9
    Join Date
    Jan 2017
    Posts
    3
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    You guys are awesome!! I have not run it since it is missing the connector on the power cord. I haven't wanted to plug it in or run it without knowing exactly what it is I have.Name:  IMG_0059.JPG
Views: 256
Size:  117.2 KB
    Name:  IMG_0060.JPG
Views: 277
Size:  97.2 KB
    Name:  IMG_0061.JPG
Views: 272
Size:  107.1 KB

  10. #10
    Join Date
    Dec 2015
    Posts
    1,392
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    Well, then,

    It's probably an 3-phase unit, which probably has little value to you as an resididual use TIG unit.

    It's undoubtedly more of a liability, than an asset, then!


    Quote Originally Posted by ederasu View Post
    You guys are awesome!! I have not run it since it is missing the connector on the power cord. I haven't wanted to plug it in or run it without knowing exactly what it is I have.Name:  IMG_0059.JPG
Views: 256
Size:  117.2 KB
    Name:  IMG_0060.JPG
Views: 277
Size:  97.2 KB
    Name:  IMG_0061.JPG
Views: 272
Size:  107.1 KB

  11. #11
    Join Date
    Jan 2017
    Posts
    3
    Post Thanks / Like

    Re: Newbie question: Mystery welder

    After looking at the wiring schematic closer I can see it is 3 phase. Unfortunately it will now just be taking up precious garage floor space! But thank you guys so much for the help! I can see now why this is the best welding forum on the inter-webs!

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,160,222.25843 seconds with 14 queries