MST300 erratic welding output
The display doesnt flash and turning the weld level pot doesn't change the output and it seems stuck on 100% welding current. Tried a remote 5k pot and it lowered the output but would randomly go back to 100%. I checked the pot on the panel and it is good. Blew out all the dust before starting it up the first time today. Checked the connections to the PWBs. The amps reading on the front shows "c04" or "c05". I looked at all the caps and nothing seems blown. Wondering if anyone else had this type of problem. Thx
Powcon MST300
Powcon 400SMT
Powcon 300SS
Powcon 300ST
Powcon 300SM
'71 SA200
'75 SAM400
'88 SAM650
XMT350
MM200
Linde VI402
Mig35
SWM23
LN25
-
Re: MST300 erratic welding output
Fixed it. Talked to Eddie and he said it was possibly the hall sensor so $28 for the part from newark, soldered it in, and it works perfectly. HA!
-
Re: MST300 erratic welding output
Posting Permissions
- You may not post new threads
- You may not post replies
- You may not post attachments
- You may not edit your posts
-
Forum Rules
Page generated in 1,659,932,262.06048 seconds with 11 queries