    What is the secret if any to removing the rheostat knob on SA-200's without completely destroying the whole rheostat and or faceplate? Of the 13 SA's I have had in my lifetime only one has ever came off with the teeny tiny 3/32 allen wrench that Lincoln made them with, after soaking it in penetrating oil overnight and even using Kroil at times. In addition you can only use the long end of the allen wrench which gives you even less of a bite on the allen screw because unlike the selector switch knob which they put it in the side of it instead of the end like the rheo knob. I am about to attempt to remove another one, but before I do I would like any advice you all may have for a workaround for what is an obvious engineering flaw on Lincolns part.

    Another question:
    I have a knob I removed a few weeks back and I ended up destroying the rheostat getting it off. Has anyone ever put one back together? I was thinking epoxy or something.

  2. #2
    Join Date
    Mar 2009
    Posts
    3,552
    Post Thanks / Like

    Re: SA-200 Rheostat Knob Removal

    If you have a small two finger puller (or make one) you can drill a hole through the knob and pull them off the shaft. Then weld up the hole when you're done and drill / tap a new set screw.
    "You can't out puke a buzzard"

  3. #3
    Join Date
    Jun 2014
    Location
    Southern Illinois
    Posts
    940
    Post Thanks / Like

    Re: SA-200 Rheostat Knob Removal

    I lucked out on my old 66. I soaked both in penetrating oil, got the set screws out and soaked them more and the both came off with no damage


    Sent from my iPhone using Tapatalk
    Steve

    Miller Dialarc 250 (1990)
    Miller Maxstar 140 STR (2003)
    Lincoln SA200 Redface Pipeliner (1966)
    Lincoln MP210 (2015)
    Victor and MECO torches

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,371
    Post Thanks / Like

    Re: SA-200 Rheostat Knob Removal

    Protect the faceplate with one or more pieces of sheet metal and heat the center of the knob with a propane torch until red. This usually allows removing the set screw. Reheat and the knob should gently work off with a couple crow foot pry bars. At least that's my usual procedure.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  5. #5
    Join Date
    Apr 2021
    Posts
    1
    Post Thanks / Like

    Re: SA-200 Rheostat Knob Removal

    Hi....I got it stripped down got the exiter out. presently do I take the entire arm. lodging off with the exiter lodging as one piece or two?when I do get it beat liberated from the shaft that is. is that square headed set screw holding the bearing or does it go to the shaft? do you obstruct the motor a piece when you take the lodging off it would seem that theres no engine mounts on the end.

Posting Permissions