    I needed a key ring for my knife. I used 1/8 mild steel welding rod and bent it in a small circle. I welded it with a Lincoln 140 MIG welder using the lowest wire feed and lowest voltage. I could only tack weld it on several sides. I ground it smooth and this is the result. It holds well enough for a key ring. Any suggestions on a better technique?


    Sent from my iPhone using Tapatalk

  2. #2
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,270
    Post Thanks / Like

    Re: Key ring

    Next time use a Tig welder.
    Dont pay any attention to me
    Im just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  3. #3
    Join Date
    Sep 2015
    Location
    SE Pa
    Posts
    1,918
    Post Thanks / Like

    Re: Key ring

    Or braze it

  4. #4
    Join Date
    Feb 2015
    Location
    North Sewickley Pa. Shop in Monaca
    Posts
    212
    Post Thanks / Like

    Re: Key ring

    A key ring ........really...... Next guys will want to be showing " coat hangars " they made........

  5. #5
    Join Date
    May 2010
    Location
    Sparks, NV
    Posts
    9,636
    Post Thanks / Like

    Re: Key ring

    You don't make coat hangers, you weld with them.
    Tiger Sales: AHP Distributor www.tigersalesco.com
    AHP200x; AHP 160ST; MM350P, Spoolmatic 30A; Everlast PowerTig 185; Thermal Dynamics 60i plasma.
    For Sale: Cobra Mig 250 w/ Push-pull gun. Lincoln Wirematic 250

  6. #6
    Join Date
    Jul 2008
    Posts
    3,197
    Post Thanks / Like

    Re: Key ring

    Quote Originally Posted by soutthpaw View Post
    You don't make coat hangers, you weld with them.
    But only on OTR trailers and NASA projects.

  7. #7
    Join Date
    Mar 2008
    Location
    Georgetown, Texas
    Posts
    2,033
    Post Thanks / Like

    Re: Key ring

    Quote Originally Posted by SmoothOperator View Post
    A key ring ........really...... Next guys will want to be showing " coat hangars " they made........
    Now that you mention it, I made this for an interior decorator years ago to display an antique dress on. They wanted one with just a touch of class.
    Attached Images Attached Images  

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,664,147.31406 seconds with 12 queries