    Grinding wheel recommendations?

    Its time to replace my medium (60-80 grit) 8x1 grinding wheel on one of my bench grinders. I mostly grind steel welds with it. I know, a better welder should not have to grind welds, but this is a finished product and has to be blended smooth.

    I want a good balanced wheel that will last, but reasonably priced. I see brands listed for $20-200. I have a Dayton and a Baldor grinders that do a good job so I dont want just a cheap wheel.

    What brands and vendors do you recommend?

    Thank you for your input.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 120

    10FtDrillBit.com

  2. #2
    Join Date
    Jun 2016
    Location
    Back to the jungle
    Posts
    3,994
    Post Thanks / Like

    Re: Grinding wheel recommendations?


  3. #3
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,335
    Post Thanks / Like

    Re: Grinding wheel recommendations?

    The last wheels I bought were from Enco.
    IIRC they were TruMax wheels. They are
    still working after several years of moderate
    use, so Im thinking theyre good.
    Now that Enco is gone I will probably get
    wheels from MSC when a free shipping
    and 15% off when ordering $100 or more
    type deal comes around. Ill just have to
    wait until I need $100 worth of stuff,
    Machine shop I worked in used Norton
    wheels, with few exceptions.

  4. #4
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,622
    Post Thanks / Like

    Re: Grinding wheel recommendations?

    I used bench grinder 36 grit for steel
    For hand grinding 24 grit and drill bit grinding 60 grit

    Dave


    Quote Originally Posted by wb4rt View Post
    Its time to replace my medium (60-80 grit) 8x1 grinding wheel on one of my bench grinders. I mostly grind steel welds with it. I know, a better welder should not have to grind welds, but this is a finished product and has to be blended smooth.

    I want a good balanced wheel that will last, but reasonably priced. I see brands listed for $20-200. I have a Dayton and a Baldor grinders that do a good job so I dont want just a cheap wheel.

    What brands and vendors do you recommend?

    Thank you for your input.

  5. #5
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    1,887
    Post Thanks / Like

    Re: Grinding wheel recommendations?

    The Norton green is rated for 3150 rpms, my Dayton is 3450 rpms. I see other wheels rated above 3450 rpms, but still trying to figure out which one.

    Ideas?
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211
    Miller 375 Plasma Cutter
    Hobart Handler 120

    10FtDrillBit.com

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,065,086.23903 seconds with 11 queries