Yes sir Pat. I do the same and return about a hour later to check again. I try to get torch work and welding done first . There's always more to do after that anyways. Those sparks can be a problem.
Remote Jobsite work required a fire permit and dedicated fire watch. We were required to stop welding or use of open flame one hour before quitting for the day. Gotta play safe.