    I was just inspecting my brushes when I noticed that all of them are slightly tapered side to side toward the generator. One set is worse than the rest with maybe 3/16" of uneven wear. Its welding fine, but Im not sure if this is common, or a symptom of poor brush rack alignment or something similar. Any thoughts?

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,392
    Post Thanks / Like

    Re: 200d uneven brushes

    Have seen this before. I suspect it starts due to the one or more brush springs being a little offset from center causing the brush to wear sideways.

    This one was still welding too believe it or not.
    Name:  Hardin SA200 001.jpg
Views: 97
Size:  64.2 KB
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  3. #3
    Join Date
    Aug 2010
    Posts
    59
    Post Thanks / Like

    Re: 200d uneven brushes

    Thanks, that makes me feel better. Next set of brushes Im gonna try to figure out a spacer between the brushes to hold them true.

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,392
    Post Thanks / Like

    Re: 200d uneven brushes

    Mmmm I'd be careful there. Could easily create a situation that causes them to hang up. I'd just make sure the springs are straight and centered on each brush.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,081,800.84538 seconds with 12 queries