    Stacking beads

    Did some practice just to keep in shape.
    Quite happy with it. Half of the plate was done flat and the other half horizontal.
    1/8 7018

    Name:  WP_20180715_18_20_19_Pro.jpg
Views: 746
Size:  112.2 KB
    Fronius Transpocket 180
    Kemppi minarc 150
    Esab powercut 400

  2. #2
    Join Date
    Mar 2015
    Posts
    242
    Post Thanks / Like

    Re: Stacking beads

    Look's purtty. Now do some with the same hand traveling opposite direction. After that,might as well try other hand.

  3. #3
    Join Date
    May 2018
    Location
    the Netherlands
    Posts
    262
    Post Thanks / Like

    Re: Stacking beads

    Quote Originally Posted by Jax View Post
    After that,might as well try other hand.
    You're right, i have to practice that more because i'm not good with my non-dominant hand.
    Fronius Transpocket 180
    Kemppi minarc 150
    Esab powercut 400

  4. #4
    Join Date
    Nov 2004
    Location
    Southern Montana
    Posts
    977
    Post Thanks / Like

    Re: Stacking beads

    Just a suggestion... you might try moving your torch ahead a bit more on each puddle before introducing filler. It will make for a wider puddle profile (dimes). This is for appearance, only, and does not, necessarily, improve fusion, or weld strength. It took me awhile to learn the technique, too.

    What is the difference between flat and horizontal?

    Wow! After producing all of those beads you must have been out of breathe, and probably lost a couple of pounds, fulfilling your desire to stay in shape. (A joke.)
    Last edited by Weldordie; 11-12-2018 at 03:43 AM.

  5. #5
    Join Date
    May 2018
    Location
    the Netherlands
    Posts
    262
    Post Thanks / Like

    Re: Stacking beads

    Quote Originally Posted by Weldordie View Post
    Just a suggestion... you might try moving your torch ahead a bit more on each puddle before introducing filler. It will make for a wider puddle profile (dimes). This is for appearance, only, and does not, necessarily, improve fusion, or weld strength. It took me awhile to learn the technique, too.

    What is the difference between flat and horizontal?

    Wow! After producing all of those beads you must have been out of breathe, and probably lost a couple of pounds, fulfilling your desire to stay in shape. (A joke.)
    This was done with stick not TIG. But I'm flattered that you think it might be TIG. Stick like TIG.

    Flat is 1F/1G and horizontal is 2F/2G
    Fronius Transpocket 180
    Kemppi minarc 150
    Esab powercut 400

  6. #6
    Join Date
    Jun 2011
    Location
    Texas
    Posts
    642
    Post Thanks / Like

    Re: Stacking beads

    Quote Originally Posted by Weldordie View Post
    What is the difference between flat and horizontal?
    Flat is lying flat on the table, while you make beads going across it.

    Horizontal is when it's standing up on edge, presenting a vertical surface, and you make the beads going across it.

    By the way, one thing you might do, if you have a band saw, is cleanly cut across it in 2 or 3 places and look for cavities. There shouldn't be any.
    -Ruark
    "Become one with the puddle, grasshopper" - Welding Instructor
    Lincoln 3200HD
    Hobart Stickmate LX235
    TWECO Fabricator 211i

  7. #7
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,918
    Post Thanks / Like

    Re: Stacking beads

    for some real world practice try it overhead then go to restricted access.
    i.u.o.e. # 15
    queens, ny and sunny fla

  8. #8
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    2,419
    Post Thanks / Like

    Re: Stacking beads

    3g, show us some 3g, that's the fun stuff

  9. #9
    Join Date
    Apr 2018
    Location
    TN
    Posts
    307
    Post Thanks / Like

    Re: Stacking beads

    I can tell the top is the horizontal and I'm not supposed to be able to tell. It looks very good, but some small tweaks needed. It's better than my last run at horizontal though..... I rarely ever have to do it so not much practice with it.
    1957 Lincoln Idealarc 300 AC/DC
    2020 ESAB ES 180i MiniArc
    Lincoln Idealarc SP200
    Lincoln 3350 PAPR
    CK CK17FV
    CK CK9FV

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,634,494,111.61516 seconds with 14 queries